MANUFACTURING METHOD OF SILICATE POLYMER MOLDED BODY AND SILICATE POLYMER MOLDED BODY
PROBLEM TO BE SOLVED: To provide a manufacturing method of a silicate polymer molded body capable of reducing environmental load, and a silicate polymer molded body.SOLUTION: The manufacturing method of a silicate polymer molded body includes a step of preparing an aggregate containing ceramic-based siding waste (step S1), a step of generating a mixture by mixing the aggregate, aluminosilicate and an alkali silica solution (step S2) and a step of molding the mixture (step S3). The silicate polymer molded body is manufactured by mixing the aggregate containing ceramic-based siding waste, the aluminosilicate and the alkali silica solution and molding the mixture. They are mixed at any mass ratio of aggregate:aluminosilicate:alkali silica solution=(3.0 to 3.8):(1.0 to 0.3):1.0, (1.8 to 2.8):(1.2 to 0.2):1.0, (1.0 to 2.2):(1.3 to 0.2):1.0 and (0.3 to 0.5):(1.3 to 1.0):1.0.
【課題】環境負荷を低減するシリケートポリマー成形体の製造方法及びシリケートポリマー成形体を提供する。【解決手段】本発明のシリケートポリマー成形体の製造方法は、窯業系サイディング廃材を含む骨材を準備する工程(ステップS1)と、骨材と、アルミノ珪酸塩と、アルカリシリカ溶液とを混合して、混合物を生成する工程(ステップS2)と、混合物を成形する工程(ステップS3)とを備える。本発明のシリケートポリマー成形体は、窯業系サイディング廃材を含む骨材と、アルミノ珪酸塩と、アルカリシリカ溶液とが混合され、混合物が成形されてなる。骨材:アルミノ珪酸塩:アルカリシリカ溶液=(3.0〜3.8):(1.0〜0.3):1.0、(1.8〜2.8):(1.2〜0.2):1.0、(1.0〜2.2):(1.3〜0.2):1.0及び(0.3〜0.5):(1.3〜1.0):1.0のいずれかの質量割合の比で混合される。【選択図】図1
MANUFACTURING METHOD OF SILICATE POLYMER MOLDED BODY AND SILICATE POLYMER MOLDED BODY
PROBLEM TO BE SOLVED: To provide a manufacturing method of a silicate polymer molded body capable of reducing environmental load, and a silicate polymer molded body.SOLUTION: The manufacturing method of a silicate polymer molded body includes a step of preparing an aggregate containing ceramic-based siding waste (step S1), a step of generating a mixture by mixing the aggregate, aluminosilicate and an alkali silica solution (step S2) and a step of molding the mixture (step S3). The silicate polymer molded body is manufactured by mixing the aggregate containing ceramic-based siding waste, the aluminosilicate and the alkali silica solution and molding the mixture. They are mixed at any mass ratio of aggregate:aluminosilicate:alkali silica solution=(3.0 to 3.8):(1.0 to 0.3):1.0, (1.8 to 2.8):(1.2 to 0.2):1.0, (1.0 to 2.2):(1.3 to 0.2):1.0 and (0.3 to 0.5):(1.3 to 1.0):1.0.
【課題】環境負荷を低減するシリケートポリマー成形体の製造方法及びシリケートポリマー成形体を提供する。【解決手段】本発明のシリケートポリマー成形体の製造方法は、窯業系サイディング廃材を含む骨材を準備する工程(ステップS1)と、骨材と、アルミノ珪酸塩と、アルカリシリカ溶液とを混合して、混合物を生成する工程(ステップS2)と、混合物を成形する工程(ステップS3)とを備える。本発明のシリケートポリマー成形体は、窯業系サイディング廃材を含む骨材と、アルミノ珪酸塩と、アルカリシリカ溶液とが混合され、混合物が成形されてなる。骨材:アルミノ珪酸塩:アルカリシリカ溶液=(3.0〜3.8):(1.0〜0.3):1.0、(1.8〜2.8):(1.2〜0.2):1.0、(1.0〜2.2):(1.3〜0.2):1.0及び(0.3〜0.5):(1.3〜1.0):1.0のいずれかの質量割合の比で混合される。【選択図】図1
MANUFACTURING METHOD OF SILICATE POLYMER MOLDED BODY AND SILICATE POLYMER MOLDED BODY
シリケートポリマー成形体の製造方法及びシリケートポリマー成形体
KUBOTA TAKAYUKI (author) / ISHIKAWA MASAHIKO (author)
2015-11-12
Patent
Electronic Resource
Japanese
IPC:
C04B
Kalk
,
LIME
SILICATE POLYMER MOLDED BODY AND MANUFACTURING METHOD OF SILICATE POLYMER MOLDED BODY
European Patent Office | 2018
|MANUFACTURING METHOD OF SILICATE POLYMER MOLDED BODY AND SILICATE POLYMER MOLDED BODY
European Patent Office | 2016
|European Patent Office | 2024
|