METHOD FOR PRODUCTION OF LATEX-MODIFIED QUICK-HARDENING CONCRETE
PROBLEM TO BE SOLVED: To provide an easily handleable latex-modified quick-hardening concrete having a proper slump value.SOLUTION: A method for production of a latex-modified quick-hardening concrete comprises: a conveyance process of the non-liquid system constituent material of a latex-modified quick-hardening concrete in which a storage container storing at least cement and a coarse aggregate is conveyed to the site at which the latex-modified quick-hardening concrete is used; a conveyance process of the liquid system constituent material of the latex-modified quick-hardening concrete in which the liquid system constituent material of the latex-modified quick-hardening concrete including at least a rubber latex and water as the constituents is conveyed to the site at which the above concrete is used; a first kneading process in which the cement, coarse aggregate, rubber latex, setting retarder and water in the constituent material of the conveyed latex-modified quick-hardening concrete are supplied into the drum of a mixer arranged to the site at which the above concrete is used, and are kneaded; and a second kneading process in which the quick-hardening cement admixture conveyed in the conveyance process is supplied to the kneaded material after the first kneading process, and is kneaded. The amount of the coarse aggregate is 500 kg/mor more, and that of the rubber latex is 5-30 pts.mass based on 100 pts.mass of cement. The amount of the quick-hardening cement admixture is 10-100 pts.mass based on 100 pts.mass of cement.
【課題】適切なスランプ値を有し、取り扱い易いラテックス改質速硬コンクリートを提供することである。【解決手段】少なくともセメント及び粗骨材が収納されている収納容器が、ラテックス改質速硬コンクリート使用現場に、搬送されるラテックス改質速硬コンクリート非液体系構成材料の搬送工程と、少なくともゴムラテックス及び水を構成要素とするラテックス改質速硬コンクリート液体系構成材料が、ラテックス改質速硬コンクリート使用現場に、搬送されるラテックス改質速硬コンクリート液体系構成材料の搬送工程と、前記搬送工程で搬送されて来たラテックス改質速硬コンクリート構成材料中のセメント、粗骨材、ゴムラテックス、凝結遅延剤、及び水が、ラテックス改質速硬コンクリート使用現場に配されているミキサのドラム内に、供給・混練される第1混練工程と、前記第1混練工程の後、該混練物に前記搬送工程で搬送されて来た速硬性セメント混和材が供給・混練される第2混練工程とを具備してなり、前記粗骨材の量は500kg/m3以上であり、前記ゴムラテックスの量は、前記セメント100質量部に対して、5〜30質量部であり、前記速硬性セメント混和材の量は、前記セメント100質量部に対して、10〜100質量部であるラテックス改質速硬コンクリートの製造方法。【選択図】なし
METHOD FOR PRODUCTION OF LATEX-MODIFIED QUICK-HARDENING CONCRETE
PROBLEM TO BE SOLVED: To provide an easily handleable latex-modified quick-hardening concrete having a proper slump value.SOLUTION: A method for production of a latex-modified quick-hardening concrete comprises: a conveyance process of the non-liquid system constituent material of a latex-modified quick-hardening concrete in which a storage container storing at least cement and a coarse aggregate is conveyed to the site at which the latex-modified quick-hardening concrete is used; a conveyance process of the liquid system constituent material of the latex-modified quick-hardening concrete in which the liquid system constituent material of the latex-modified quick-hardening concrete including at least a rubber latex and water as the constituents is conveyed to the site at which the above concrete is used; a first kneading process in which the cement, coarse aggregate, rubber latex, setting retarder and water in the constituent material of the conveyed latex-modified quick-hardening concrete are supplied into the drum of a mixer arranged to the site at which the above concrete is used, and are kneaded; and a second kneading process in which the quick-hardening cement admixture conveyed in the conveyance process is supplied to the kneaded material after the first kneading process, and is kneaded. The amount of the coarse aggregate is 500 kg/mor more, and that of the rubber latex is 5-30 pts.mass based on 100 pts.mass of cement. The amount of the quick-hardening cement admixture is 10-100 pts.mass based on 100 pts.mass of cement.
【課題】適切なスランプ値を有し、取り扱い易いラテックス改質速硬コンクリートを提供することである。【解決手段】少なくともセメント及び粗骨材が収納されている収納容器が、ラテックス改質速硬コンクリート使用現場に、搬送されるラテックス改質速硬コンクリート非液体系構成材料の搬送工程と、少なくともゴムラテックス及び水を構成要素とするラテックス改質速硬コンクリート液体系構成材料が、ラテックス改質速硬コンクリート使用現場に、搬送されるラテックス改質速硬コンクリート液体系構成材料の搬送工程と、前記搬送工程で搬送されて来たラテックス改質速硬コンクリート構成材料中のセメント、粗骨材、ゴムラテックス、凝結遅延剤、及び水が、ラテックス改質速硬コンクリート使用現場に配されているミキサのドラム内に、供給・混練される第1混練工程と、前記第1混練工程の後、該混練物に前記搬送工程で搬送されて来た速硬性セメント混和材が供給・混練される第2混練工程とを具備してなり、前記粗骨材の量は500kg/m3以上であり、前記ゴムラテックスの量は、前記セメント100質量部に対して、5〜30質量部であり、前記速硬性セメント混和材の量は、前記セメント100質量部に対して、10〜100質量部であるラテックス改質速硬コンクリートの製造方法。【選択図】なし
METHOD FOR PRODUCTION OF LATEX-MODIFIED QUICK-HARDENING CONCRETE
ラテックス改質速硬コンクリートの製造方法
KWAK DOYEON (author) / TAKAHASHI HIROAKI (author)
2016-01-12
Patent
Electronic Resource
Japanese
Quick-hardening latex modified concrete composition and its construction method
European Patent Office | 2025
|LATEX MODIFIED ULTRA RAPID HARDENING CONCRETE COMPOSITION USING THE HYBRID SYNTHETIC RUBBER LATEX
European Patent Office | 2020
|