A platform for research: civil engineering, architecture and urbanism
PROBLEM TO BE SOLVED: To provide a fluid flow-rectification member of a structure in which, by adjusting the density of a ceramic fiber, the weight increase is suppressed and the surface strength is sufficient.SOLUTION: A ceramic fiber layer 22 is constructed of a strand 21 which is a bundle of a plurality of unit ceramic fibers 40; the unit ceramic fiber 40 has a smaller cross-sectional area as approaching an outermost side ceramic fiber layer 222; because of this, since the strand 215 is formed of a unit ceramic fiber 41 having a smaller cross-sectional area as approaching the outermost side ceramic fiber layer 222, the outermost side strand 215 can be formed with high density to ensure the strength; thereby, as the outermost side ceramic fiber layer 222 which is in close proximity to the fluid and is most likely to be broken, is formed of a unit ceramic fiber 41 having a small cross-sectional area, even when the strand 215 deforms, the unit ceramic fiber 41 is less likely to be bent, and a fluid flow-rectification member 10A which is, as a whole, less likely to be broken, can be provided; and also, the excessive weight increase can be suppressed.SELECTED DRAWING: Figure 4
【課題】セラミック繊維の密度を調整することにより、重量増を抑えて表面の強度が十分な構造の流体用整流部材を提供する。【解決手段】セラミック繊維層22は、複数の単位セラミック繊維40を束ねたストランド21で構成されている。単位セラミック繊維40は、最外側セラミック繊維層222に近いほどその断面積が小さい。このため、最外側セラミック繊維層222に近いほどストランド215を断面積が小さい単位セラミック繊維41で形成するので、最外側のストランド215を高密度で形成して強度を確保することができる。これにより、流体に近接して最も破損しやすい最外側セラミック繊維層222を断面積が小さい単位セラミック繊維41で形成するので、ストランド215が変形しても単位セラミック繊維41が折れにくく、全体として破損しにくい流体用整流部材10Aを提供できる。また、過度の重量化を抑制できる。【選択図】図4
PROBLEM TO BE SOLVED: To provide a fluid flow-rectification member of a structure in which, by adjusting the density of a ceramic fiber, the weight increase is suppressed and the surface strength is sufficient.SOLUTION: A ceramic fiber layer 22 is constructed of a strand 21 which is a bundle of a plurality of unit ceramic fibers 40; the unit ceramic fiber 40 has a smaller cross-sectional area as approaching an outermost side ceramic fiber layer 222; because of this, since the strand 215 is formed of a unit ceramic fiber 41 having a smaller cross-sectional area as approaching the outermost side ceramic fiber layer 222, the outermost side strand 215 can be formed with high density to ensure the strength; thereby, as the outermost side ceramic fiber layer 222 which is in close proximity to the fluid and is most likely to be broken, is formed of a unit ceramic fiber 41 having a small cross-sectional area, even when the strand 215 deforms, the unit ceramic fiber 41 is less likely to be bent, and a fluid flow-rectification member 10A which is, as a whole, less likely to be broken, can be provided; and also, the excessive weight increase can be suppressed.SELECTED DRAWING: Figure 4
【課題】セラミック繊維の密度を調整することにより、重量増を抑えて表面の強度が十分な構造の流体用整流部材を提供する。【解決手段】セラミック繊維層22は、複数の単位セラミック繊維40を束ねたストランド21で構成されている。単位セラミック繊維40は、最外側セラミック繊維層222に近いほどその断面積が小さい。このため、最外側セラミック繊維層222に近いほどストランド215を断面積が小さい単位セラミック繊維41で形成するので、最外側のストランド215を高密度で形成して強度を確保することができる。これにより、流体に近接して最も破損しやすい最外側セラミック繊維層222を断面積が小さい単位セラミック繊維41で形成するので、ストランド215が変形しても単位セラミック繊維41が折れにくく、全体として破損しにくい流体用整流部材10Aを提供できる。また、過度の重量化を抑制できる。【選択図】図4
FLUID FLOW-RECTIFICATION MEMBER
流体用整流部材