METHOD FOR MANUFACTURING COMPOSITE COMPONENT OF TIMEPIECE OR OF JEWELRY PART, AND COMPOSITE COMPONENT OBTAINED BY SUCH METHOD
PROBLEM TO BE SOLVED: To manufacture a composite component of a timepiece or of a jewelry part with high hardness.SOLUTION: This invention relates to a method for manufacturing a composite component of a timepiece or of a jewelry part, the composite component including a porous ceramic part and a metallic material filling the pores of the ceramic part, the method including the steps of: providing a porous ceramic preform of the component; providing a metallic material; heating the metallic material to a temperature higher than the melting point of the metallic material; filling the pores of the ceramic preform with the molten metallic material; cooling the metallic material and the ceramic preform to obtain a solidified metallic material in the pores of the ceramic preform; and applying finishing treatments to obtain the composite component, wherein the porous ceramic preform consists essentially of a material selected from the group consisting of SiN, SiOand mixtures thereof, and the metallic material is gold, platinum, palladium metals or alloys of these metals. This invention further relates to a composite component of a timepiece or of a jewelry part comprising a porous ceramic part and a metallic material filling the pores of the ceramic part, wherein the ceramic part consists essentially of a material selected from the group consisting of SiN, SiOand mixtures thereof, and the metallic material is selected from the group consisting of gold, platinum, palladium metals and alloys of these metals.SELECTED DRAWING: None
【課題】計時器又は宝飾物の硬度が高い複合材部品を製造する。【解決手段】本発明は、計時器又は宝飾物の複合材部品を製造する方法に関し、前記複合材部品は、多孔性のセラミックス部分及び前記セラミックス部分の孔に充填される金属性物質を有し、前記複合材部品の多孔性のセラミックスプレフォームを用意するステップと、金属性物質を用意するステップと、前記金属性物質の融点よりも高い温度まで前記金属性物質を加熱するステップと、前記セラミックスプレフォームの孔を溶融した前記金属性物質で充填するステップと、前記セラミックスプレフォームの孔において凝固した金属性物質を得るために、前記金属性物質及び前記セラミックスプレフォームを冷却するステップと、前記複合材部品を得るために、仕上げ処置を行うステップとを有し、前記多孔性のセラミックスプレフォームは、本質的に、Si3N4、SiO2及びこれらのいずれかを含有する混合物からなる群から選択される物質によって構成しており、前記金属性物質は、金、白金、パラジウムの金属及びこれらのいずれかの金属の合金からなる群から選択される。また、本発明は、多孔性のセラミックス部分及び前記セラミックス部分の孔に充填される金属性物質を有する計時器又は宝飾物の複合材部品に関し、前記セラミックス部分は、本質的に、Si3N4、SiO2及びこれらのいずれかを含有する混合物からなる群から選択される物質によって構成しており、前記金属性物質は、金、白金、パラジウムの金属及びこれらのいずれかの金属の合金からなる群から選択される。【選択図】なし
METHOD FOR MANUFACTURING COMPOSITE COMPONENT OF TIMEPIECE OR OF JEWELRY PART, AND COMPOSITE COMPONENT OBTAINED BY SUCH METHOD
PROBLEM TO BE SOLVED: To manufacture a composite component of a timepiece or of a jewelry part with high hardness.SOLUTION: This invention relates to a method for manufacturing a composite component of a timepiece or of a jewelry part, the composite component including a porous ceramic part and a metallic material filling the pores of the ceramic part, the method including the steps of: providing a porous ceramic preform of the component; providing a metallic material; heating the metallic material to a temperature higher than the melting point of the metallic material; filling the pores of the ceramic preform with the molten metallic material; cooling the metallic material and the ceramic preform to obtain a solidified metallic material in the pores of the ceramic preform; and applying finishing treatments to obtain the composite component, wherein the porous ceramic preform consists essentially of a material selected from the group consisting of SiN, SiOand mixtures thereof, and the metallic material is gold, platinum, palladium metals or alloys of these metals. This invention further relates to a composite component of a timepiece or of a jewelry part comprising a porous ceramic part and a metallic material filling the pores of the ceramic part, wherein the ceramic part consists essentially of a material selected from the group consisting of SiN, SiOand mixtures thereof, and the metallic material is selected from the group consisting of gold, platinum, palladium metals and alloys of these metals.SELECTED DRAWING: None
【課題】計時器又は宝飾物の硬度が高い複合材部品を製造する。【解決手段】本発明は、計時器又は宝飾物の複合材部品を製造する方法に関し、前記複合材部品は、多孔性のセラミックス部分及び前記セラミックス部分の孔に充填される金属性物質を有し、前記複合材部品の多孔性のセラミックスプレフォームを用意するステップと、金属性物質を用意するステップと、前記金属性物質の融点よりも高い温度まで前記金属性物質を加熱するステップと、前記セラミックスプレフォームの孔を溶融した前記金属性物質で充填するステップと、前記セラミックスプレフォームの孔において凝固した金属性物質を得るために、前記金属性物質及び前記セラミックスプレフォームを冷却するステップと、前記複合材部品を得るために、仕上げ処置を行うステップとを有し、前記多孔性のセラミックスプレフォームは、本質的に、Si3N4、SiO2及びこれらのいずれかを含有する混合物からなる群から選択される物質によって構成しており、前記金属性物質は、金、白金、パラジウムの金属及びこれらのいずれかの金属の合金からなる群から選択される。また、本発明は、多孔性のセラミックス部分及び前記セラミックス部分の孔に充填される金属性物質を有する計時器又は宝飾物の複合材部品に関し、前記セラミックス部分は、本質的に、Si3N4、SiO2及びこれらのいずれかを含有する混合物からなる群から選択される物質によって構成しており、前記金属性物質は、金、白金、パラジウムの金属及びこれらのいずれかの金属の合金からなる群から選択される。【選択図】なし
METHOD FOR MANUFACTURING COMPOSITE COMPONENT OF TIMEPIECE OR OF JEWELRY PART, AND COMPOSITE COMPONENT OBTAINED BY SUCH METHOD
計時器又は宝飾物の複合材部品を製造する方法及びこの方法によって製造された複合材部品
DUBACH ALBAN (author) / RODRIGUEZ PABLO (author) / POMPE ROBERT (author)
2016-12-15
Patent
Electronic Resource
Japanese
European Patent Office | 2022
|European Patent Office | 2024
|European Patent Office | 2018
|European Patent Office | 2016
|Method for manufacturing a carbon-carbon timepiece component
European Patent Office | 2025
|