DIELECTRIC THIN FILM
PROBLEM TO BE SOLVED: To provide a dielectric thin film which can change a dielectric constant (relative dielectric constant) by ultraviolet irradiation.SOLUTION: A dielectric thin film comprises a polymer-coated zinc oxide fine particle that comprises a zinc oxide fine particle, and a polymer coating layer formed on the surface of the zinc oxide fine particle and having an average thickness of 5-500 nm.SELECTED DRAWING: None
【課題】紫外線照射によって誘電率(比誘電率)を変化させることが可能な誘電体薄膜を提供すること。【解決手段】酸化亜鉛微粒子と該酸化亜鉛微粒子の表面に形成されている平均厚さが5〜500nmの高分子被覆層とからなる高分子被覆酸化亜鉛微粒子を含有することを特徴とする誘電体薄膜。【選択図】なし
DIELECTRIC THIN FILM
PROBLEM TO BE SOLVED: To provide a dielectric thin film which can change a dielectric constant (relative dielectric constant) by ultraviolet irradiation.SOLUTION: A dielectric thin film comprises a polymer-coated zinc oxide fine particle that comprises a zinc oxide fine particle, and a polymer coating layer formed on the surface of the zinc oxide fine particle and having an average thickness of 5-500 nm.SELECTED DRAWING: None
【課題】紫外線照射によって誘電率(比誘電率)を変化させることが可能な誘電体薄膜を提供すること。【解決手段】酸化亜鉛微粒子と該酸化亜鉛微粒子の表面に形成されている平均厚さが5〜500nmの高分子被覆層とからなる高分子被覆酸化亜鉛微粒子を含有することを特徴とする誘電体薄膜。【選択図】なし
DIELECTRIC THIN FILM
誘電体薄膜
HAYASHIDA KENICHI (author) / TANAKA HIROMITSU (author)
2017-08-24
Patent
Electronic Resource
Japanese
European Patent Office | 2019
European Patent Office | 2017
|European Patent Office | 2017
|