A platform for research: civil engineering, architecture and urbanism
SEMICONDUCTOR CERAMIC COMPOSITION AND METHOD FOR PRODUCING THE SAME
PROBLEM TO BE SOLVED: To provide a semiconductor ceramic composition which is a barium titanate-based semiconductor ceramic composition and can achieve the same performance as that of conventional ceramic compositions using rare earth elements without adding any rare earth elements.SOLUTION: Provided is a semiconductor ceramic composition which comprises a main component represented by a composition formula (1-x)(BaMe)TiO-xBi(Mg, Nb)O, wherein the a satisfies 0.4950≤a≤0.9500, the Me is either one kind of Sr or Ca or two or more kinds selected from the group consisting of Sr, Ca and Pb, the x satisfies 0.0060≤x≤0.0140 when the Me is Sr or two or more kinds selected from the group consisting of Sr, Ca and Pb, and the x satisfies 0.0080≤x≤0.0160 when the Me is Ca.SELECTED DRAWING: None
【課題】チタン酸バリウム系の半導体磁器組成物であって、希土類元素を添加しなくても、希土類元素を用いた従来の磁器組成物と同等の性能を実現できる半導体磁器組成物を提供する。【解決手段】主成分が、組成式(1-x)(BaaMe1-a)TiO3-xBi(Mg,Nb)O3で表される半導体磁器組成物であって、前記aは0.4950≦a≦0.9500であり、前記Meは、SrまたはCaのいずれか1種であるか、または、Sr,CaおよびPbからなる群から選ばれる2種以上であり、前記MeがSrであるか、または、Sr,CaおよびPbからなる群から選ばれる2種以上であるときは、前記xが0.0060≦x≦0.0140であり、前記MeがCaであるときは、前記xが0.0080≦x≦0.0160であることを特徴とする半導体磁器組成物。【選択図】なし
SEMICONDUCTOR CERAMIC COMPOSITION AND METHOD FOR PRODUCING THE SAME
PROBLEM TO BE SOLVED: To provide a semiconductor ceramic composition which is a barium titanate-based semiconductor ceramic composition and can achieve the same performance as that of conventional ceramic compositions using rare earth elements without adding any rare earth elements.SOLUTION: Provided is a semiconductor ceramic composition which comprises a main component represented by a composition formula (1-x)(BaMe)TiO-xBi(Mg, Nb)O, wherein the a satisfies 0.4950≤a≤0.9500, the Me is either one kind of Sr or Ca or two or more kinds selected from the group consisting of Sr, Ca and Pb, the x satisfies 0.0060≤x≤0.0140 when the Me is Sr or two or more kinds selected from the group consisting of Sr, Ca and Pb, and the x satisfies 0.0080≤x≤0.0160 when the Me is Ca.SELECTED DRAWING: None
【課題】チタン酸バリウム系の半導体磁器組成物であって、希土類元素を添加しなくても、希土類元素を用いた従来の磁器組成物と同等の性能を実現できる半導体磁器組成物を提供する。【解決手段】主成分が、組成式(1-x)(BaaMe1-a)TiO3-xBi(Mg,Nb)O3で表される半導体磁器組成物であって、前記aは0.4950≦a≦0.9500であり、前記Meは、SrまたはCaのいずれか1種であるか、または、Sr,CaおよびPbからなる群から選ばれる2種以上であり、前記MeがSrであるか、または、Sr,CaおよびPbからなる群から選ばれる2種以上であるときは、前記xが0.0060≦x≦0.0140であり、前記MeがCaであるときは、前記xが0.0080≦x≦0.0160であることを特徴とする半導体磁器組成物。【選択図】なし
SEMICONDUCTOR CERAMIC COMPOSITION AND METHOD FOR PRODUCING THE SAME
半導体磁器組成物およびその製造方法
KAMISHIRO MASAHIRO (author)
2017-10-05
Patent
Electronic Resource
Japanese
IPC:
C04B
Kalk
,
LIME
SEMICONDUCTOR CERAMIC COMPOSITION, METHOD FOR PRODUCING SAME, AND PTC ELEMENT
European Patent Office | 2015
|SEMICONDUCTOR CERAMIC COMPOSITION AND PROCESS FOR PRODUCING THE SAME
European Patent Office | 2016
|Semiconductor ceramic composition, method for producing the same, and PTC element
European Patent Office | 2015
|SEMICONDUCTOR CERAMIC COMPOSITION, METHOD FOR PRODUCING SAME, PTC ELEMENT AND HEAT GENERATING MODULE
European Patent Office | 2016
|