A platform for research: civil engineering, architecture and urbanism
SINTERED BODY AND PRODUCTION METHOD THEREOF
PROBLEM TO BE SOLVED: To provide a sintered body which has the desired thermal conductivity and mechanical strength while the performance of the AlN whisker part can be sufficiently utilized, and to provide a production method thereof.SOLUTION: A ZrOsintered body for sensor A10 includes: an AlN whisker 100 which has a fibrous AlN single crystal and an oxygen atom containing layer covering the AlN 100 single crystal; and a ZrOparticle 200 covering the AlN whisker 100; in which the oxygen atom containing layer is produced by at least AlN single crystal incorporating the oxygen atoms, the film thickness of the oxygen containing layer is 7 to 500 nm. A production method of a ZrOsintered body for sensor A10 includes a step of mixing the AlN whisker 100 with ZrO2 particle 200, and sintering the mixture.SELECTED DRAWING: Figure 1
【課題】AlNウィスカーの性能を活かしつつ所望の熱伝導性および機械的強度を備える焼結体とその製造方法の提供。【解決手段】繊維状のAlN単結晶とAlN単結晶を覆う酸素原子含有層とを有するAlNウィスカー100と、AlNウィスカー100を覆うZrO2粒子200とを有し、酸素原子含有層は、AlN単結晶が少なくとも酸素原子を取り込むことにより生成された層であり、酸素原子含有層の膜厚は、7〜500nmであるZrO2センサーA10焼結体。AlNウイスカー100とZrO2粒子200を混合し、混合物を焼結するZrO2センサーA10焼結体の製造方法。【選択図】図1
SINTERED BODY AND PRODUCTION METHOD THEREOF
PROBLEM TO BE SOLVED: To provide a sintered body which has the desired thermal conductivity and mechanical strength while the performance of the AlN whisker part can be sufficiently utilized, and to provide a production method thereof.SOLUTION: A ZrOsintered body for sensor A10 includes: an AlN whisker 100 which has a fibrous AlN single crystal and an oxygen atom containing layer covering the AlN 100 single crystal; and a ZrOparticle 200 covering the AlN whisker 100; in which the oxygen atom containing layer is produced by at least AlN single crystal incorporating the oxygen atoms, the film thickness of the oxygen containing layer is 7 to 500 nm. A production method of a ZrOsintered body for sensor A10 includes a step of mixing the AlN whisker 100 with ZrO2 particle 200, and sintering the mixture.SELECTED DRAWING: Figure 1
【課題】AlNウィスカーの性能を活かしつつ所望の熱伝導性および機械的強度を備える焼結体とその製造方法の提供。【解決手段】繊維状のAlN単結晶とAlN単結晶を覆う酸素原子含有層とを有するAlNウィスカー100と、AlNウィスカー100を覆うZrO2粒子200とを有し、酸素原子含有層は、AlN単結晶が少なくとも酸素原子を取り込むことにより生成された層であり、酸素原子含有層の膜厚は、7〜500nmであるZrO2センサーA10焼結体。AlNウイスカー100とZrO2粒子200を混合し、混合物を焼結するZrO2センサーA10焼結体の製造方法。【選択図】図1
SINTERED BODY AND PRODUCTION METHOD THEREOF
焼結体とその製造方法
TAKEUCHI YUKIHISA (author) / UJIHARA TORU (author) / SHIOJIRI DAISHI (author) / MATSUMOTO MASAKI (author) / SAITO HIROSHI (author) / HAYASHI IKUO (author)
2018-10-04
Patent
Electronic Resource
Japanese
SINTERED BODY, TOOL USING SINTERED BODY, AND SINTERED BODY PRODUCTION METHOD
European Patent Office | 2016
|FERRITE SINTERED BODY, FERRITE SINTERED MAGNET, AND PRODUCTION METHOD THEREOF
European Patent Office | 2020
|SINTERED BODY TOOL USING SINTERED BODY AND SINTERED BODY PRODUCTION METHOD
European Patent Office | 2017
|