PRODUCTION METHOD OF LAMINATE GLASS, LIQUID CRYSTAL FILM, LAMINATE GLASS
To provide a production method of a laminate glass, which can reduce a liquid crystal pool due to an uneven distribution of a liquid crystal in a laminate glass in which a liquid crystal film is sandwiched, a liquid crystal film, and a laminate glass.SOLUTION: A production method of a laminate glass for producing the laminate glass joined by sandwiching a lighting control film 10 provided with a liquid crystal layer 14 by a first glass sheet 33A and a second glass sheet 33B includes a joining step S20 of joining in one body by heating, or, by heating and pressurizing a laminate 30 obtained by sandwiching a first intermediate film forming sheet 31A and a lighting control film 10 and a second intermediate film forming sheet 31B with the first glass sheet 33A and the second glass sheet 33B, and a homogenizing step S30 of homogenizing a layer thickness of the liquid crystal layer 14 by heating the laminate 30 after the joining step S20.SELECTED DRAWING: Figure 4
【課題】液晶フィルムを挟み込んだ合わせガラスにおいて、液晶の偏在による液晶溜り等を低減できる合わせガラス製造方法、液晶フィルム、合わせガラスを提供することである。【解決手段】第1のガラス板33A及び第2のガラス板33Bで液晶層14を備える調光フィルム10を挟んで接合した合わせガラスを製造する合わせガラス製造方法は、第1のガラス板33Aと第2のガラス板33Bとで第1の中間膜形成シート31Aと調光フィルム10と第2の中間膜形成シート31Bとを挟んだ積層体30を、加熱して、又は、加熱及び加圧して一体に接合する接合工程S20と、接合工程S20の後、積層体30を加熱して液晶層14の層厚を均一にする均し工程S30とを備える。【選択図】図4
PRODUCTION METHOD OF LAMINATE GLASS, LIQUID CRYSTAL FILM, LAMINATE GLASS
To provide a production method of a laminate glass, which can reduce a liquid crystal pool due to an uneven distribution of a liquid crystal in a laminate glass in which a liquid crystal film is sandwiched, a liquid crystal film, and a laminate glass.SOLUTION: A production method of a laminate glass for producing the laminate glass joined by sandwiching a lighting control film 10 provided with a liquid crystal layer 14 by a first glass sheet 33A and a second glass sheet 33B includes a joining step S20 of joining in one body by heating, or, by heating and pressurizing a laminate 30 obtained by sandwiching a first intermediate film forming sheet 31A and a lighting control film 10 and a second intermediate film forming sheet 31B with the first glass sheet 33A and the second glass sheet 33B, and a homogenizing step S30 of homogenizing a layer thickness of the liquid crystal layer 14 by heating the laminate 30 after the joining step S20.SELECTED DRAWING: Figure 4
【課題】液晶フィルムを挟み込んだ合わせガラスにおいて、液晶の偏在による液晶溜り等を低減できる合わせガラス製造方法、液晶フィルム、合わせガラスを提供することである。【解決手段】第1のガラス板33A及び第2のガラス板33Bで液晶層14を備える調光フィルム10を挟んで接合した合わせガラスを製造する合わせガラス製造方法は、第1のガラス板33Aと第2のガラス板33Bとで第1の中間膜形成シート31Aと調光フィルム10と第2の中間膜形成シート31Bとを挟んだ積層体30を、加熱して、又は、加熱及び加圧して一体に接合する接合工程S20と、接合工程S20の後、積層体30を加熱して液晶層14の層厚を均一にする均し工程S30とを備える。【選択図】図4
PRODUCTION METHOD OF LAMINATE GLASS, LIQUID CRYSTAL FILM, LAMINATE GLASS
合わせガラス製造方法、液晶フィルム、合わせガラス
YAMAKI MAKOTO (author) / IKEZAWA TAKAO (author) / WATARU HIROKI (author) / DOKO TAKEYUKI (author) / HAGIWARA YUSUKE (author)
2019-09-19
Patent
Electronic Resource
Japanese
IPC:
C03C
Chemische Zusammensetzungen für Gläser, Glasuren oder Emails
,
CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUS ENAMELS
/
E06B
Feste oder bewegliche Abschlüsse für Öffnungen in Bauwerken, Fahrzeugen, Zäunen oder ähnlichen Einfriedungen allgemein, z.B. Türen, Fenster, Läden, Tore
,
FIXED OR MOVABLE CLOSURES FOR OPENINGS IN BUILDINGS, VEHICLES, FENCES, OR LIKE ENCLOSURES, IN GENERAL, e.g. DOORS, WINDOWS, BLINDS, GATES
INTERLAYER FOR GLASS LAMINATE, GLASS LAMINATE AND METHOD FOR ATTACHING GLASS LAMINATE
European Patent Office | 2017
|GLASS LAMINATE MANUFACTURING DEVICE, AND GLASS LAMINATE MANUFACTURING METHOD
European Patent Office | 2019
|LAMINATE GLASS, MANUFACTURING METHOD OF LAMINATE GLASS, DIMMER, DIMMING CELL AND LAMINATE FOR DIMMER
European Patent Office | 2020
|