A platform for research: civil engineering, architecture and urbanism
HARDENED CEMENT FREEZING-DAMAGE SUPPRESSING AGENT
To provide a hardened-cement freezing-damage suppressing agent that has an excellent freezing-damage suppressing-action without using salt, a cement composition, and a hardened cement.SOLUTION: Provided are: a freezing-damage suppressing agent for hardened cement containing at least one antifreeze polysaccharide selected from the group consisting of galactose, mannose, xylose and rhamnose; a cement composition containing cement, antifreeze polysaccharide, and water; and a hardened cement containing antifreeze polysaccharide. It is desirable that the antifreeze polysaccharide is xylomannan. Further preferably, provided is a freezing-damage suppressing agent in which the component ratio of mannose and xylose constituting xylomannan is 1.5 to 2.5 mol of mannose with respect to 1 mol of xylose, and the molecular weight of xylomannan is 280,000 to 340,000.SELECTED DRAWING: None
【課題】塩を使用しなくとも優れた凍害抑制作用を有するセメント硬化体の凍害抑制剤、セメント組成物、及びセメント硬化体。【解決手段】ガラクトース、マンノース、キシロース及びラムノースからなる群から選択される少なくとも一種の不凍多糖を含むセメント硬化体の凍害抑制剤、セメント、不凍多糖、及び水を含むセメント組成物、並びに不凍多糖を含むセメント硬化体。好ましくは、不凍多糖がキシロマンナンであることが望ましい。更に好ましくは、キシロマンナンを構成するマンノースとキシロースの構成比が、キシロース1モルに対してマンノース1.5〜2.5モルであり、キシロマンナンの分子量が、280000〜340000である凍害抑制剤。【選択図】なし
HARDENED CEMENT FREEZING-DAMAGE SUPPRESSING AGENT
To provide a hardened-cement freezing-damage suppressing agent that has an excellent freezing-damage suppressing-action without using salt, a cement composition, and a hardened cement.SOLUTION: Provided are: a freezing-damage suppressing agent for hardened cement containing at least one antifreeze polysaccharide selected from the group consisting of galactose, mannose, xylose and rhamnose; a cement composition containing cement, antifreeze polysaccharide, and water; and a hardened cement containing antifreeze polysaccharide. It is desirable that the antifreeze polysaccharide is xylomannan. Further preferably, provided is a freezing-damage suppressing agent in which the component ratio of mannose and xylose constituting xylomannan is 1.5 to 2.5 mol of mannose with respect to 1 mol of xylose, and the molecular weight of xylomannan is 280,000 to 340,000.SELECTED DRAWING: None
【課題】塩を使用しなくとも優れた凍害抑制作用を有するセメント硬化体の凍害抑制剤、セメント組成物、及びセメント硬化体。【解決手段】ガラクトース、マンノース、キシロース及びラムノースからなる群から選択される少なくとも一種の不凍多糖を含むセメント硬化体の凍害抑制剤、セメント、不凍多糖、及び水を含むセメント組成物、並びに不凍多糖を含むセメント硬化体。好ましくは、不凍多糖がキシロマンナンであることが望ましい。更に好ましくは、キシロマンナンを構成するマンノースとキシロースの構成比が、キシロース1モルに対してマンノース1.5〜2.5モルであり、キシロマンナンの分子量が、280000〜340000である凍害抑制剤。【選択図】なし
HARDENED CEMENT FREEZING-DAMAGE SUPPRESSING AGENT
セメント硬化体の凍害抑制剤
TSURUTA HIROAKI (author) / KAWAHARA HIDEHISA (author)
2019-09-19
Patent
Electronic Resource
Japanese
Cement freezing-thawing resistance of hardened cement paste with synthetic zeolite
British Library Online Contents | 2014
|Cement freezing–thawing resistance of hardened cement paste with synthetic zeolite
Online Contents | 2014
|METHOD FOR SUPPRESSING ALKALI AGGREGATE REACTION IN CEMENT HARDENED BODY
European Patent Office | 2021
|Damage Process in Hardened Cement Paste
Online Contents | 1996
|