CORROSION PROOF METHOD FOR CONCRETE STRUCTURE
To provide a corrosion proof method for a concrete structure capable of restraining deterioration due to any one of salt injury, neutralization, and ASR, by infiltrating an inhibitor even in the interior of a concrete structure.SOLUTION: A corrosion proof method for a concrete structure electrochemically infiltrates solution (lithium nitrite solution L1, lithium hydroxide solution L2) including an inhibitor for restraining corrosion of a steel material (a reinforcing-bar S) inside a concrete structure (a concrete slab C) and implements corrosion proof. In the method, the solution including the inhibitor is brought into contact with both sides of the concrete structure and a first circuitry C1 is provided to flow a direct current so as to penetrate the concrete structure by applying voltage from electrodes E1 and E2 each disposed outside the concrete structure, and thereby electrochemically infiltrating the inhibitor to implement corrosion proof.SELECTED DRAWING: Figure 1
【課題】コンクリート構造物の内部にもインヒビターを浸透させて、塩害、中性化、ASRのいずれによる劣化も抑制することができるコンクリート構造物の防食工法を提供する。【解決手段】コンクリート構造物(コンクリートスラブC)中の鋼材(鉄筋S)の腐食を抑制するインヒビターを含有する溶液(亜硝酸リチウム溶液L1,水酸化リチウム溶液L2)を電気化学的に浸透させて防食するコンクリート構造物の防食工法において、前記インヒビターを含有する溶液を前記コンクリート構造物の両側に接触させるとともに、前記コンクリート構造物の外部に設置された電極E1,E2から電圧を印加して前記コンクリート構造物を貫通するように直流電流を流す第1の回路C1を設け、前記インヒビターを電気化学的に浸透させて防食する。【選択図】図1
CORROSION PROOF METHOD FOR CONCRETE STRUCTURE
To provide a corrosion proof method for a concrete structure capable of restraining deterioration due to any one of salt injury, neutralization, and ASR, by infiltrating an inhibitor even in the interior of a concrete structure.SOLUTION: A corrosion proof method for a concrete structure electrochemically infiltrates solution (lithium nitrite solution L1, lithium hydroxide solution L2) including an inhibitor for restraining corrosion of a steel material (a reinforcing-bar S) inside a concrete structure (a concrete slab C) and implements corrosion proof. In the method, the solution including the inhibitor is brought into contact with both sides of the concrete structure and a first circuitry C1 is provided to flow a direct current so as to penetrate the concrete structure by applying voltage from electrodes E1 and E2 each disposed outside the concrete structure, and thereby electrochemically infiltrating the inhibitor to implement corrosion proof.SELECTED DRAWING: Figure 1
【課題】コンクリート構造物の内部にもインヒビターを浸透させて、塩害、中性化、ASRのいずれによる劣化も抑制することができるコンクリート構造物の防食工法を提供する。【解決手段】コンクリート構造物(コンクリートスラブC)中の鋼材(鉄筋S)の腐食を抑制するインヒビターを含有する溶液(亜硝酸リチウム溶液L1,水酸化リチウム溶液L2)を電気化学的に浸透させて防食するコンクリート構造物の防食工法において、前記インヒビターを含有する溶液を前記コンクリート構造物の両側に接触させるとともに、前記コンクリート構造物の外部に設置された電極E1,E2から電圧を印加して前記コンクリート構造物を貫通するように直流電流を流す第1の回路C1を設け、前記インヒビターを電気化学的に浸透させて防食する。【選択図】図1
CORROSION PROOF METHOD FOR CONCRETE STRUCTURE
コンクリート構造物の防食工法
MURANISHI SHINYA (author) / HASE TOSHIHIKO (author) / HORIKOSHI NAOKI (author) / KOBAYASHI TOSHIAKI (author) / SHOJI AKIO (author)
2020-04-30
Patent
Electronic Resource
Japanese
CONCRETE PROOF FOR CORROSION INHIBITORS
British Library Online Contents | 2009
|European Patent Office | 2020
|ANTICORROSIVE AGENT FOR REINFORCED CONCRETE, AND METHOD OF CORROSION PROOF TREATMENT
European Patent Office | 2016
|