A platform for research: civil engineering, architecture and urbanism
CONCRETE CRACK REDUCING METHOD
To provide a concrete crack reducing method that is highly effective in reducing crack in concrete.SOLUTION: The present invention is a concrete crack reducing method in which a shrinkage reducing agent is applied to the surface of concrete during the period after surface-finishing of concrete and until before starting curing, and, preferably, a shrinkage reducing agent is applied by 30 to 200 g per concrete surface 1 m2.SELECTED DRAWING: Figure 2
【課題】本発明は、コンクリートのひび割れを低減する効果が高いコンクリートのひび割れ低減方法を提供する。【解決手段】本発明は、コンクリートの表面仕上げを行なった後、養生を開始するまでの間に、収縮低減剤をコンクリートの表面に施工するコンクリートのひび割れ低減方法であり、好ましくは、コンクリートの表面1m2あたり、収縮低減剤を30~200g施工するコンクリートのひび割れ低減方法である。【選択図】図2
CONCRETE CRACK REDUCING METHOD
To provide a concrete crack reducing method that is highly effective in reducing crack in concrete.SOLUTION: The present invention is a concrete crack reducing method in which a shrinkage reducing agent is applied to the surface of concrete during the period after surface-finishing of concrete and until before starting curing, and, preferably, a shrinkage reducing agent is applied by 30 to 200 g per concrete surface 1 m2.SELECTED DRAWING: Figure 2
【課題】本発明は、コンクリートのひび割れを低減する効果が高いコンクリートのひび割れ低減方法を提供する。【解決手段】本発明は、コンクリートの表面仕上げを行なった後、養生を開始するまでの間に、収縮低減剤をコンクリートの表面に施工するコンクリートのひび割れ低減方法であり、好ましくは、コンクリートの表面1m2あたり、収縮低減剤を30~200g施工するコンクリートのひび割れ低減方法である。【選択図】図2
CONCRETE CRACK REDUCING METHOD
コンクリートのひび割れ低減方法
SHIMAKAGE RYOJI (author) / KISHIRA RYO (author) / MARUTA HIROSHI (author) / FUJII HIROSHI (author)
2022-02-10
Patent
Electronic Resource
Japanese
IPC:
C04B
Kalk
,
LIME
/
B28B
Formgeben von Ton oder anderen keramischen Stoffzusammensetzungen, Schlacke oder von Mischungen, die zementartiges Material enthalten, z.B. Putzmörtel
,
SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG OR MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER
/
B28C
Tonaufbereitung
,
PREPARING CLAY
European Patent Office | 2017
|