A platform for research: civil engineering, architecture and urbanism
METHOD FOR FIXING CARBON DIOXIDE
To provide a method capable of fixing more carbon dioxide in a cement composition.SOLUTION: A method for fixing carbon dioxide includes: a carbon dioxide gas solidification step for ejecting liquefied carbon dioxide gas from liquefied carbon dioxide gas storage means for storing carbon dioxide gas which is pressurized and liquefied, in such an ejection condition that the pressure of it drops at a pressure drop rate which is high enough to produce dry ice and thereby obtaining dry ice in a powdery state; a dry ice compaction step for compressing and storing the powdery dry ice in a compaction container and obtaining block-shaped dry ice having the same shape as an internal space of the compaction container and having a bulk density of 0.30-1.00 g/cm3; and a dry ice utilization step for taking out the block shaped dry ice from the compaction container and then obtaining a cement composition which is constituted by fixing carbon dioxide originating from the block-shaped dry ice by mixing at least cement, water and the block shaped dry ice or its crushed matter.SELECTED DRAWING: None
【課題】より多くの二酸化炭素をセメント組成物に固定化することができる方法を提供する。【解決手段】加圧して液化した炭酸ガスが収容された液化炭酸ガス収容手段から、上記液化した炭酸ガスを、ドライアイスを生成させるのに十分な大きさの圧力低下速度で圧力を低下させる条件下で噴出させて、粉末状のドライアイスを得る炭酸ガス固体化工程と、粉末状のドライアイスを、成形用容器内に圧縮して収容し、かさ密度が0.30~1.00g/cm3であり、成形用容器の内部空間と同じ形状を有するブロック状のドライアイスを得るドライアイス成形工程と、成形用容器から、ブロック状のドライアイスを取り出し、次いで、少なくとも、ブロック状のドライアイスまたはその破砕物と、セメントと、水を混合して、ブロック状のドライアイスに由来する二酸化炭素が固定されてなるセメント組成物を得るドライアイス利用工程とを含む二酸化炭素の固定化方法。【選択図】なし
METHOD FOR FIXING CARBON DIOXIDE
To provide a method capable of fixing more carbon dioxide in a cement composition.SOLUTION: A method for fixing carbon dioxide includes: a carbon dioxide gas solidification step for ejecting liquefied carbon dioxide gas from liquefied carbon dioxide gas storage means for storing carbon dioxide gas which is pressurized and liquefied, in such an ejection condition that the pressure of it drops at a pressure drop rate which is high enough to produce dry ice and thereby obtaining dry ice in a powdery state; a dry ice compaction step for compressing and storing the powdery dry ice in a compaction container and obtaining block-shaped dry ice having the same shape as an internal space of the compaction container and having a bulk density of 0.30-1.00 g/cm3; and a dry ice utilization step for taking out the block shaped dry ice from the compaction container and then obtaining a cement composition which is constituted by fixing carbon dioxide originating from the block-shaped dry ice by mixing at least cement, water and the block shaped dry ice or its crushed matter.SELECTED DRAWING: None
【課題】より多くの二酸化炭素をセメント組成物に固定化することができる方法を提供する。【解決手段】加圧して液化した炭酸ガスが収容された液化炭酸ガス収容手段から、上記液化した炭酸ガスを、ドライアイスを生成させるのに十分な大きさの圧力低下速度で圧力を低下させる条件下で噴出させて、粉末状のドライアイスを得る炭酸ガス固体化工程と、粉末状のドライアイスを、成形用容器内に圧縮して収容し、かさ密度が0.30~1.00g/cm3であり、成形用容器の内部空間と同じ形状を有するブロック状のドライアイスを得るドライアイス成形工程と、成形用容器から、ブロック状のドライアイスを取り出し、次いで、少なくとも、ブロック状のドライアイスまたはその破砕物と、セメントと、水を混合して、ブロック状のドライアイスに由来する二酸化炭素が固定されてなるセメント組成物を得るドライアイス利用工程とを含む二酸化炭素の固定化方法。【選択図】なし
METHOD FOR FIXING CARBON DIOXIDE
二酸化炭素の固定化方法
ABU TOSHIYA (author) / SASAKI KOICHI (author) / HAYAKAWA TAKAYUKI (author)
2022-09-07
Patent
Electronic Resource
Japanese
European Patent Office | 2025
|