A platform for research: civil engineering, architecture and urbanism
CEMENT-BASED SOLIDIFIER AND GROUND IMPROVEMENT METHOD USING THE SAME
To provide cement-based solidifier capable of producing solidified soil that is less likely to leach hexavalent chromium over a long period of time.SOLUTION: A cement-based solidifier that includes cement clinker powder, hemihydrate gypsum powder, dihydrate gypsum powder, anhydrous gypsum powder, and blast furnace slag powder. The solidifier contains SO3 in the following ratios: The ratio of (b) the second total mass, which is the sum of the mass of SO3 derived from the cement clinker powder, hemihydrate gypsum powder, dihydrate gypsum powder and anhydrous gypsum powder, to (a) the first total mass, which is the sum of the mass of cement clinker powder, hemihydrate gypsum powder, dihydrate gypsum powder, anhydrous gypsum powder and blast furnace slag powder, is 4.00% or more to 11.00% or less. The ratio of the mass of SO3 derived from the cement clinker powder to (a) the first total mass is 1.01% or more to 2.30% or less. The ratio of mass of SO3 derived from the hemihydrate gypsum powder to (a) the first total mass is 0.60 to 2.80%. The ratio of the mass of SO3 derived from the dihydrate gypsum powder to (a) the first total mass is 0.70% or more to 2.80% or less.SELECTED DRAWING: None
【課題】長期間にわたって六価クロムを溶出させにくい固化処理土を作製可能なセメント系固化材を提供する。【解決手段】セメント系固化材は、セメントクリンカ粉末、半水石膏粉末、二水石膏粉末、無水石膏粉末及び高炉スラグ粉末を含む。セメントクリンカ粉末、半水石膏粉末、二水石膏粉末、無水石膏粉末及び高炉スラグ粉末の質量の合計である第1の合計質量に対する、セメントクリンカ粉末、半水石膏粉末、二水石膏粉末及び無水石膏粉末にそれぞれ由来するSO3の質量の合計である第2の合計質量の割合が4.00%以上11.00%以下である。第1の合計質量に対する、セメントクリンカ粉末に由来するSO3の質量の割合が1.01%以上2.30%以下である。第1の合計質量に対する、半水石膏粉末に由来するSO3の質量の割合が0.60%以上2.80%以下である。第1の合計質量に対する、二水石膏粉末に由来するSO3の質量の割合が0.70%以上2.80%以下である。【選択図】なし
CEMENT-BASED SOLIDIFIER AND GROUND IMPROVEMENT METHOD USING THE SAME
To provide cement-based solidifier capable of producing solidified soil that is less likely to leach hexavalent chromium over a long period of time.SOLUTION: A cement-based solidifier that includes cement clinker powder, hemihydrate gypsum powder, dihydrate gypsum powder, anhydrous gypsum powder, and blast furnace slag powder. The solidifier contains SO3 in the following ratios: The ratio of (b) the second total mass, which is the sum of the mass of SO3 derived from the cement clinker powder, hemihydrate gypsum powder, dihydrate gypsum powder and anhydrous gypsum powder, to (a) the first total mass, which is the sum of the mass of cement clinker powder, hemihydrate gypsum powder, dihydrate gypsum powder, anhydrous gypsum powder and blast furnace slag powder, is 4.00% or more to 11.00% or less. The ratio of the mass of SO3 derived from the cement clinker powder to (a) the first total mass is 1.01% or more to 2.30% or less. The ratio of mass of SO3 derived from the hemihydrate gypsum powder to (a) the first total mass is 0.60 to 2.80%. The ratio of the mass of SO3 derived from the dihydrate gypsum powder to (a) the first total mass is 0.70% or more to 2.80% or less.SELECTED DRAWING: None
【課題】長期間にわたって六価クロムを溶出させにくい固化処理土を作製可能なセメント系固化材を提供する。【解決手段】セメント系固化材は、セメントクリンカ粉末、半水石膏粉末、二水石膏粉末、無水石膏粉末及び高炉スラグ粉末を含む。セメントクリンカ粉末、半水石膏粉末、二水石膏粉末、無水石膏粉末及び高炉スラグ粉末の質量の合計である第1の合計質量に対する、セメントクリンカ粉末、半水石膏粉末、二水石膏粉末及び無水石膏粉末にそれぞれ由来するSO3の質量の合計である第2の合計質量の割合が4.00%以上11.00%以下である。第1の合計質量に対する、セメントクリンカ粉末に由来するSO3の質量の割合が1.01%以上2.30%以下である。第1の合計質量に対する、半水石膏粉末に由来するSO3の質量の割合が0.60%以上2.80%以下である。第1の合計質量に対する、二水石膏粉末に由来するSO3の質量の割合が0.70%以上2.80%以下である。【選択図】なし
CEMENT-BASED SOLIDIFIER AND GROUND IMPROVEMENT METHOD USING THE SAME
セメント系固化材及びこれを用いた地盤改良方法
DOI KOTA (author) / KONO TAKESHI (author) / KIYOTA MASATO (author)
2022-10-13
Patent
Electronic Resource
Japanese
GROUND SOLIDIFIER COMPOSITION AND METHOD FOR SILIDIFYING SIOL USING THE SAME
European Patent Office | 2017
|A COMPOSITION OF SOIL SOLIDIFIER AND CONSTRUCTION METHOD USING THE SAME
European Patent Office | 2017
|