DECK COMPOSITE SLAB, AND CONCRETE THICKENING METHOD FOR DECK COMPOSITE SLAB
To provide a deck composite slab which can be provided as a floor slab that requires having a performance of resisting fire for more than 2 hours in performance-based fireproof-design buildings, and its concrete thickening method.SOLUTION: A concrete 304 has a thickness greater than 100 mm on top of a crest part 3a of a deck plate 3. Thereby, a deck composite slab 300 can improve fireproof performance through thickening of thickness of the concrete 304 so as to meet a required performance of resisting fire for more than 2 hours in a performance-based fireproof-design building. As a result, for example, additionally placing the concrete on an existing slab enables minor work to cope with a tenant change to applications with a required time of resisting fire for more than 2 hours.SELECTED DRAWING: Figure 2
【課題】性能規定型の耐火設計建物において、2時間を超える耐火性能が要求される床スラブとして提供可能なデッキ合成スラブ、およびそのコンクリート増厚方法を提供する。【解決手段】コンクリート304は、デッキプレート3の山部3a上における厚さが100mmより大きい。これにより、デッキ合成スラブ300は、コンクリート304の厚みを十分に厚くすることで耐火性能を向上し、性能規定型の耐火設計建物において、2時間を超える耐火性能の要求を満たすことができる。これにより、例えば既存スラブに対するコンクリート増し打ちにより、耐火要求時間が2時間を超える用途へのテナント変更にも軽微な施工によって対応することができる。【選択図】図2
DECK COMPOSITE SLAB, AND CONCRETE THICKENING METHOD FOR DECK COMPOSITE SLAB
To provide a deck composite slab which can be provided as a floor slab that requires having a performance of resisting fire for more than 2 hours in performance-based fireproof-design buildings, and its concrete thickening method.SOLUTION: A concrete 304 has a thickness greater than 100 mm on top of a crest part 3a of a deck plate 3. Thereby, a deck composite slab 300 can improve fireproof performance through thickening of thickness of the concrete 304 so as to meet a required performance of resisting fire for more than 2 hours in a performance-based fireproof-design building. As a result, for example, additionally placing the concrete on an existing slab enables minor work to cope with a tenant change to applications with a required time of resisting fire for more than 2 hours.SELECTED DRAWING: Figure 2
【課題】性能規定型の耐火設計建物において、2時間を超える耐火性能が要求される床スラブとして提供可能なデッキ合成スラブ、およびそのコンクリート増厚方法を提供する。【解決手段】コンクリート304は、デッキプレート3の山部3a上における厚さが100mmより大きい。これにより、デッキ合成スラブ300は、コンクリート304の厚みを十分に厚くすることで耐火性能を向上し、性能規定型の耐火設計建物において、2時間を超える耐火性能の要求を満たすことができる。これにより、例えば既存スラブに対するコンクリート増し打ちにより、耐火要求時間が2時間を超える用途へのテナント変更にも軽微な施工によって対応することができる。【選択図】図2
DECK COMPOSITE SLAB, AND CONCRETE THICKENING METHOD FOR DECK COMPOSITE SLAB
デッキ合成スラブ、及びデッキ合成スラブのコンクリート増厚方法
KORI YASUAKI (author)
2023-08-07
Patent
Electronic Resource
Japanese
DECK PLATE FOR DECK COMPOSITE SLAB AND DECK COMPOSITE SLAB
European Patent Office | 2023
|DECK COMPOSITE SLAB AND METHOD FOR DESIGNING DECK COMPOSITE SLAB
European Patent Office | 2022
|DECK SLAB, DECK SLAB CONSTRUCTION METHOD, AND DECK SLAB DESIGN METHOD
European Patent Office | 2023
|