To provide a coated component (100), along with methods of its formation.SOLUTION: A coated component (100) may include a ceramic matrix composite substrate (102) comprising silicon carbide and having a surface (103), a bond coat (104) on the surface (103) of the substrate (102), and an environmental barrier coating (108) on the bond coat (104). The bond coat (104) includes a plurality of discrete particles (110) dispersed within a matrix phase (112), with the matrix phase (112) formed from mullite and defining 60-98% by volume of the bond coat (104). The plurality of discrete particles (110) include an oxygen getter and has 50% of its volume or greater formed from particles having an average size of 10 μm to 100 μm.SELECTED DRAWING: Figure 1
【課題】コーティングされた構成部品(100)をその形成方法とともに提供すること。【解決手段】コーティングされた構成部品(100)は、炭化ケイ素を含み、表面(103)を有するセラミックマトリックス複合材基材(102)と、基材(102)の表面(103)上のボンドコート(104)と、ボンドコート(104)上の環境バリアコーティング(108)とを含むことができる。ボンドコート(104)は、マトリックス相(112)内に分散された複数の離散粒子(110)を含み、マトリックス相(112)はムライトから形成され、ボンドコート(104)の60体積%~98体積%を画定する。複数の離散粒子(110)は酸素ゲッターを含み、その体積の50%以上が、10μm~100μmの平均サイズを有する粒子から形成される。【選択図】図1
To provide a coated component (100), along with methods of its formation.SOLUTION: A coated component (100) may include a ceramic matrix composite substrate (102) comprising silicon carbide and having a surface (103), a bond coat (104) on the surface (103) of the substrate (102), and an environmental barrier coating (108) on the bond coat (104). The bond coat (104) includes a plurality of discrete particles (110) dispersed within a matrix phase (112), with the matrix phase (112) formed from mullite and defining 60-98% by volume of the bond coat (104). The plurality of discrete particles (110) include an oxygen getter and has 50% of its volume or greater formed from particles having an average size of 10 μm to 100 μm.SELECTED DRAWING: Figure 1
【課題】コーティングされた構成部品(100)をその形成方法とともに提供すること。【解決手段】コーティングされた構成部品(100)は、炭化ケイ素を含み、表面(103)を有するセラミックマトリックス複合材基材(102)と、基材(102)の表面(103)上のボンドコート(104)と、ボンドコート(104)上の環境バリアコーティング(108)とを含むことができる。ボンドコート(104)は、マトリックス相(112)内に分散された複数の離散粒子(110)を含み、マトリックス相(112)はムライトから形成され、ボンドコート(104)の60体積%~98体積%を画定する。複数の離散粒子(110)は酸素ゲッターを含み、その体積の50%以上が、10μm~100μmの平均サイズを有する粒子から形成される。【選択図】図1