POWDER MIXTURE AND METHOD FOR PRODUCING GEOPOLYMER SOLIDIFIED BODY USING THE SAME
To provide a powder mixture capable of easily generating a geopolymer solidified body at a site and capable of producing a geopolymer solidified body having high strength, and to provide a geopolymer solidified body using the same.SOLUTION: Since a geopolymer solidified body is generated by adding water or water and an aggregate to a powder mixture obtained by mixing an active filler and alkali powder and mixing them, the geopolymer solidified body can be generated by bringing the powder mixture prepared in advance to a site and mixing it with water or water and an aggregate at the site. In addition, since any of sodium metasilicate, sodium metasilicate and sodium hydroxide, or sodium metasilicate and potassium hydroxide is used as the alkali powder in the powder mixture, a geopolymer concrete having high strength can be generated.SELECTED DRAWING: Figure 1
【課題】現場でのジオポリマー固化体の生成を容易に行うことができるとともに、強度の高いジオポリマー固化体を製造することのできる粉体混合物及びこれを用いるジオポリマー固化体を提供する。【解決手段】活性フィラーとアルカリ粉体とを混合してなる粉体混合物に水または水及び骨材を加えて混合することによりジオポリマー固化体を生成するようにしたので、予め用意した粉体混合物を現場に搬入し、現場で水または水及び骨材と混合することによりジオポリマー固化体を生成することができる。また、粉体混合物のアルカリ粉体に、メタケイ酸ナトリウム、メタケイ酸ナトリウム及び水酸化ナトリウム、メタケイ酸ナトリウム及び水酸化カリウムの何れかの粉体を用いるようにしたので、強度の高いジオポリマーコンクリートを生成することができる。【選択図】図1
POWDER MIXTURE AND METHOD FOR PRODUCING GEOPOLYMER SOLIDIFIED BODY USING THE SAME
To provide a powder mixture capable of easily generating a geopolymer solidified body at a site and capable of producing a geopolymer solidified body having high strength, and to provide a geopolymer solidified body using the same.SOLUTION: Since a geopolymer solidified body is generated by adding water or water and an aggregate to a powder mixture obtained by mixing an active filler and alkali powder and mixing them, the geopolymer solidified body can be generated by bringing the powder mixture prepared in advance to a site and mixing it with water or water and an aggregate at the site. In addition, since any of sodium metasilicate, sodium metasilicate and sodium hydroxide, or sodium metasilicate and potassium hydroxide is used as the alkali powder in the powder mixture, a geopolymer concrete having high strength can be generated.SELECTED DRAWING: Figure 1
【課題】現場でのジオポリマー固化体の生成を容易に行うことができるとともに、強度の高いジオポリマー固化体を製造することのできる粉体混合物及びこれを用いるジオポリマー固化体を提供する。【解決手段】活性フィラーとアルカリ粉体とを混合してなる粉体混合物に水または水及び骨材を加えて混合することによりジオポリマー固化体を生成するようにしたので、予め用意した粉体混合物を現場に搬入し、現場で水または水及び骨材と混合することによりジオポリマー固化体を生成することができる。また、粉体混合物のアルカリ粉体に、メタケイ酸ナトリウム、メタケイ酸ナトリウム及び水酸化ナトリウム、メタケイ酸ナトリウム及び水酸化カリウムの何れかの粉体を用いるようにしたので、強度の高いジオポリマーコンクリートを生成することができる。【選択図】図1
POWDER MIXTURE AND METHOD FOR PRODUCING GEOPOLYMER SOLIDIFIED BODY USING THE SAME
粉体混合物及びこれを用いるジオポリマー固化体の製造方法
KISAKU TOMOAKI (author) / TAKAHASHI KOICHI (author) / KOMORI TERUO (author) / YAMAMURA YUKI (author) / SAINO JUN (author) / SAITO YUKIKO (author) / NIE JING (author) / IGAWA SHUNYA (author) / MARUYAMA HAYATO (author) / ISOBE MIKI (author)
2024-03-13
Patent
Electronic Resource
Japanese
POWDER MIXTURE AND METHOD FOR PRODUCING GEOPOLYMER SOLIDIFIED MATERIAL USING SAME
European Patent Office | 2024
|GEOPOLYMER SOLIDIFIED BODY AND METHOD FOR PRODUCING THE SAME
European Patent Office | 2017
|Preparation method of glass-doped geopolymer solidified radionuclide solidified body
European Patent Office | 2022
|European Patent Office | 2022
|