High softening point reformed asphalt composition and waterproofing coating using the same
The present invention relates to a high softening point reformed asphalt waterproofing compound and a waterproofing method using the same capable of forming a waterproofing sheet by inputting a softening point increasing additive to basic reformed asphalt with a softening point of 85°C or more; being constructed at 200°C or less; and having low-temperature bending properties for elongation at -30°C or more. The present invention comprises: 40-80 wt% of the basic reformed asphalt melted at 150-200°C; and the softening point increasing additive which is manufactured by mixing 10-50 wt% of waste tire powder, 5-20 wt% of blast furnace slag fine powder, 1-5 wt% of gilsonite powder, and 2-10 wt% of an adhesion improving agent. The basic reformed asphalt includes: 40-60 wt% of asphalt; 5-20 wt% of natural asphalt; 5-15 wt% of polymer plastic; 5-20 wt% of an SBS polymer; 2-10 wt% of a specific fiber filler; 0.1-0.5 wt% of an UV stabilizer; and 0.1-0.5 wt% of an antioxidant. The present invention impregnates or constructs the high softening point reformed asphalt waterproofing compound with a glass fiber mesh or a glass paper on a waterproofing surface; forms a waterproofing coating sheet by impregnating the high softening point reformed asphalt waterproofing compound with the glass fiber mesh or the glass paper and spraying silica; and then constructs a waterproofing layer by adhering to and compressing the waterproofing coating sheet on the waterproofing surface with the high softening point reformed asphalt waterproofing compound.
본 발명은 고연화점 개질아스팔트 방수 컴파운드와 이를 이용한 방수공법에 관한 것으로, 그 목적은 연화점 85℃ 이상의 기본 개질아스팔트에 연화점 상승첨가재를 투입하여 방수시트로 형성할 수 있으면서도 200℃ 이하에서 시공이 가능하며, -30℃ 이상의 저온에서도 신축에 대하여 저온굴곡성을 구비한 고연화점 개질아스팔트 방수 컴파운드와 이를 이용한 방수공법을 제공하는 것이다.본 발명은 150℃∼200℃로 용융된 기본 개질아스팔트 40∼80wt%에, 연화점 상승첨가재로 폐타이어분말 10∼50wt%, 고로슬래그미분말 5∼20wt%, 길소나이트분말 1∼5wt%, 접착개선제 2∼10wt%가 혼합되되, 상기 기본 개질아스팔트는 아스팔트 40∼60wt%, 천연 아스팔트 5∼20wt%, 고분자플라스틱 5∼15wt%, SBS고분자 5∼20wt%, 특수섬유질 충진제 2∼10wt%, UV안정제 0.1∼0.5wt%, 산화방지제 0.1∼0.5wt%를 포함한다.본 발명은 방수표면에 고연화점 개질아스팔트 방수 컴파운드를 유리섬유메쉬 또는 글라스페이퍼 함침시켜 시공하거나, 고연화점 개질아스팔트 방수 컴파운드를 유리섬유메쉬 또는 글라스페이퍼에 함침시키고 규사를 살포하여 방수도막시트를 형성한 후, 상기 방수도막시트를 고연화점 개질아스팔트 방수 컴파운드에 의해 방수표면에 접착 및 압착하여 방수층을 시공하도록 되어 있다.
High softening point reformed asphalt composition and waterproofing coating using the same
The present invention relates to a high softening point reformed asphalt waterproofing compound and a waterproofing method using the same capable of forming a waterproofing sheet by inputting a softening point increasing additive to basic reformed asphalt with a softening point of 85°C or more; being constructed at 200°C or less; and having low-temperature bending properties for elongation at -30°C or more. The present invention comprises: 40-80 wt% of the basic reformed asphalt melted at 150-200°C; and the softening point increasing additive which is manufactured by mixing 10-50 wt% of waste tire powder, 5-20 wt% of blast furnace slag fine powder, 1-5 wt% of gilsonite powder, and 2-10 wt% of an adhesion improving agent. The basic reformed asphalt includes: 40-60 wt% of asphalt; 5-20 wt% of natural asphalt; 5-15 wt% of polymer plastic; 5-20 wt% of an SBS polymer; 2-10 wt% of a specific fiber filler; 0.1-0.5 wt% of an UV stabilizer; and 0.1-0.5 wt% of an antioxidant. The present invention impregnates or constructs the high softening point reformed asphalt waterproofing compound with a glass fiber mesh or a glass paper on a waterproofing surface; forms a waterproofing coating sheet by impregnating the high softening point reformed asphalt waterproofing compound with the glass fiber mesh or the glass paper and spraying silica; and then constructs a waterproofing layer by adhering to and compressing the waterproofing coating sheet on the waterproofing surface with the high softening point reformed asphalt waterproofing compound.
본 발명은 고연화점 개질아스팔트 방수 컴파운드와 이를 이용한 방수공법에 관한 것으로, 그 목적은 연화점 85℃ 이상의 기본 개질아스팔트에 연화점 상승첨가재를 투입하여 방수시트로 형성할 수 있으면서도 200℃ 이하에서 시공이 가능하며, -30℃ 이상의 저온에서도 신축에 대하여 저온굴곡성을 구비한 고연화점 개질아스팔트 방수 컴파운드와 이를 이용한 방수공법을 제공하는 것이다.본 발명은 150℃∼200℃로 용융된 기본 개질아스팔트 40∼80wt%에, 연화점 상승첨가재로 폐타이어분말 10∼50wt%, 고로슬래그미분말 5∼20wt%, 길소나이트분말 1∼5wt%, 접착개선제 2∼10wt%가 혼합되되, 상기 기본 개질아스팔트는 아스팔트 40∼60wt%, 천연 아스팔트 5∼20wt%, 고분자플라스틱 5∼15wt%, SBS고분자 5∼20wt%, 특수섬유질 충진제 2∼10wt%, UV안정제 0.1∼0.5wt%, 산화방지제 0.1∼0.5wt%를 포함한다.본 발명은 방수표면에 고연화점 개질아스팔트 방수 컴파운드를 유리섬유메쉬 또는 글라스페이퍼 함침시켜 시공하거나, 고연화점 개질아스팔트 방수 컴파운드를 유리섬유메쉬 또는 글라스페이퍼에 함침시키고 규사를 살포하여 방수도막시트를 형성한 후, 상기 방수도막시트를 고연화점 개질아스팔트 방수 컴파운드에 의해 방수표면에 접착 및 압착하여 방수층을 시공하도록 되어 있다.
High softening point reformed asphalt composition and waterproofing coating using the same
고연화점 개질아스팔트 방수 컴파운드와 이를 이용한 방수공법
KWON BONG JU (author)
2018-05-18
Patent
Electronic Resource
Korean
European Patent Office | 2020
|Asphalt coating waterproofing method with improved waterproofing properties
European Patent Office | 2024
|European Patent Office | 2024
|