COMPOSITION FOR REPAIRING AND REINFORCING CONCRETE STRUCTURE AND METHOD FOR REPAIRING AND REINFORCING CONCRETE STRUCTURE THEREWITH
The present invention relates to a composition for repairing and finishing a cross section of a concrete structure, which comprises 10 to 65 wt % of a functional improvement binder, 10 to 85 wt % of a fine aggregate, and 5 to 30 wt % of water, and to a method for repairing and finishing a concrete structure using the same. The functional improvement binder includes, with respect to 100 wt % of the functional improvement binder in total, 15 to 85 wt % of rapid hardening Portland cement, 5 to 45 wt % of calcium or magnesium sulfoaluminate, 3 to 40 wt % of tricalcium aluminate cement, 3 to 40 wt % of calcium chloroaluminate, 1 to 30 wt % of furnace slag, 0.5 to 20 wt % of gelite powder, 0.5 to 15 wt % of gypsum, 0.5 to 15 wt % of tricalcium silicate, 0.5 to 10 wt % of kaolin, 0.5 to 10 wt % of aluminosilicate, 0.1 to 10 wt % of graphene powder, 0.1 to 10 wt % of ethylene-vinyl acetate-vinyl alcohol copolymer, 0.1 to 10 wt % of methylacrylate-butylacrylate-butadiene copolymer, 0.1 to 10 wt % of polyfluorovinyl copolymer, and 0.1 to 10 wt % of polychloro-trifluoroethylene copolymer. Accordingly, when repairing the concrete structure using the composition of the present invention, the bending toughness, abrasion resistance, salt resistance, neutralization resistance, freeze-thaw resistance, and surface hardness of the concrete structure can be improved by using the functional improvement binder.
본 발명은 기능 개선 결합재 10∼65중량%, 잔골재 10∼85중량% 및 물 5∼30중량%를 포함하는 콘크리트 구조물 단면 보수 마감용 조성물 및 이를 이용한 콘크리트 구조물 보수 마감 공법으로서, 상기 기능 개선 결합재는, 기능 개선 결합재의 총 100 중량% 기준으로, 조강 포틀랜드 시멘트 15∼85중량%, 칼슘 또는 마그네슘설포알루미네이트 5∼45중량%, 트리칼슘알루미네이트시멘트 3∼40중량%, 칼슘클로로알루미네이트 3∼40중량%, 고로 슬래그 1∼30중량%, 겔라이트 분말 0.5∼20중량%, 석고 0.5∼15중량%, 규산삼석회 0.5∼15중량%, 카올린 0.5∼10중량%, 알루미노 규산염 0.5∼10중량%, 그래핀분말 0.1∼10중량%, 에틸렌-초산비닐-비닐알코올 공중합체 0.1∼10중량%, 메틸아크릴레이트-부틸아크릴레이트-부타디엔 공중합체 0.1∼10중량%, 폴리플루오로화비닐 공중합체 0.1∼10중량%, 및 폴리클로로-트리플루오로에틸렌 공중합체 0.1∼10중량%를 포함한다. 본 발명의 조성물을 사용하여 콘크리트 구조물을 보수하면, 기능 개선 결합재를 사용함으로써 콘크리트 구조물에 대한 휨인성, 내마모성, 내염해성, 중성화 저항성, 동결융해 저항성 및 표면경도를 개선할 수 있다.
COMPOSITION FOR REPAIRING AND REINFORCING CONCRETE STRUCTURE AND METHOD FOR REPAIRING AND REINFORCING CONCRETE STRUCTURE THEREWITH
The present invention relates to a composition for repairing and finishing a cross section of a concrete structure, which comprises 10 to 65 wt % of a functional improvement binder, 10 to 85 wt % of a fine aggregate, and 5 to 30 wt % of water, and to a method for repairing and finishing a concrete structure using the same. The functional improvement binder includes, with respect to 100 wt % of the functional improvement binder in total, 15 to 85 wt % of rapid hardening Portland cement, 5 to 45 wt % of calcium or magnesium sulfoaluminate, 3 to 40 wt % of tricalcium aluminate cement, 3 to 40 wt % of calcium chloroaluminate, 1 to 30 wt % of furnace slag, 0.5 to 20 wt % of gelite powder, 0.5 to 15 wt % of gypsum, 0.5 to 15 wt % of tricalcium silicate, 0.5 to 10 wt % of kaolin, 0.5 to 10 wt % of aluminosilicate, 0.1 to 10 wt % of graphene powder, 0.1 to 10 wt % of ethylene-vinyl acetate-vinyl alcohol copolymer, 0.1 to 10 wt % of methylacrylate-butylacrylate-butadiene copolymer, 0.1 to 10 wt % of polyfluorovinyl copolymer, and 0.1 to 10 wt % of polychloro-trifluoroethylene copolymer. Accordingly, when repairing the concrete structure using the composition of the present invention, the bending toughness, abrasion resistance, salt resistance, neutralization resistance, freeze-thaw resistance, and surface hardness of the concrete structure can be improved by using the functional improvement binder.
본 발명은 기능 개선 결합재 10∼65중량%, 잔골재 10∼85중량% 및 물 5∼30중량%를 포함하는 콘크리트 구조물 단면 보수 마감용 조성물 및 이를 이용한 콘크리트 구조물 보수 마감 공법으로서, 상기 기능 개선 결합재는, 기능 개선 결합재의 총 100 중량% 기준으로, 조강 포틀랜드 시멘트 15∼85중량%, 칼슘 또는 마그네슘설포알루미네이트 5∼45중량%, 트리칼슘알루미네이트시멘트 3∼40중량%, 칼슘클로로알루미네이트 3∼40중량%, 고로 슬래그 1∼30중량%, 겔라이트 분말 0.5∼20중량%, 석고 0.5∼15중량%, 규산삼석회 0.5∼15중량%, 카올린 0.5∼10중량%, 알루미노 규산염 0.5∼10중량%, 그래핀분말 0.1∼10중량%, 에틸렌-초산비닐-비닐알코올 공중합체 0.1∼10중량%, 메틸아크릴레이트-부틸아크릴레이트-부타디엔 공중합체 0.1∼10중량%, 폴리플루오로화비닐 공중합체 0.1∼10중량%, 및 폴리클로로-트리플루오로에틸렌 공중합체 0.1∼10중량%를 포함한다. 본 발명의 조성물을 사용하여 콘크리트 구조물을 보수하면, 기능 개선 결합재를 사용함으로써 콘크리트 구조물에 대한 휨인성, 내마모성, 내염해성, 중성화 저항성, 동결융해 저항성 및 표면경도를 개선할 수 있다.
COMPOSITION FOR REPAIRING AND REINFORCING CONCRETE STRUCTURE AND METHOD FOR REPAIRING AND REINFORCING CONCRETE STRUCTURE THEREWITH
콘크리트 구조물 단면 보수 마감용 조성물 및 이를 이용한 콘크리트 구조물 보수 마감 공법
KIM HOUNG JIN (author)
2019-04-02
Patent
Electronic Resource
Korean
European Patent Office | 2019
|European Patent Office | 2017
|European Patent Office | 2018
|European Patent Office | 2018
|European Patent Office | 2018
|