The present invention relates to a crack reduction type repairing material composition which contains 3-85 wt% of rapid hardening functional binders, 10-80 wt% of fine aggregates and 5-40 wt% of water, and specifically, to a crack reduction type repairing material composition for concrete structure maintenance, wherein the rapid hardening functional binder comprises: 20-92 wt% of early strength type Portland cement; 1-30 wt% of amorphous calcium aluminate; 1-20 wt% of kaolinite; 1-20 wt% of boehmite; 1-10 wt% of fine ceramics; 1-10 wt% of gypsum; 1-10 wt% of zinc chloride; 0.5-10 wt% of polyvinyl acetate; 0.5-10 wt% of methyl methacrylate-methacrylic acid copolymer; 0.5-10 wt% of polyvinyl-methylether copolymer; and 0.5-10 wt% of polyphenylene-ether copolymer. In addition, the present invention relates to a maintenance method of concrete structures using the same. According to the present invention, the maintenance method has excellent site applicability, workability, resistance to chloride ion permeation, durability, attaching properties, resistance to weather and waterproofness, thereby increasing performance periods of concrete structures, reducing maintenance costs and improving constructability.
본 발명은 속경형 기능성 결합재 3∼85 중량%, 잔골재 10∼80 중량% 및 물 5∼40 중량%를 포함하는 균열저감형 보수재 조성물로서, 상기 속경형 기능성 결합재가 조강포틀랜드 시멘트20∼92 중량%, 비정질 칼슘알루미네이트 1∼30 중량%, 카올리나이트 1∼20 중량%, 뵘사이트 1∼20 중량%, 파인 세라믹 1∼10 중량%, 석고 1∼10 중량%, 염화아연 1∼10 중량%, 폴리초산비닐 0.5∼10 중량%, 메틸메타크릴레이트-메타아크릴산 공중합체 0.5∼10 중량%, 폴리비닐-메틸에테르 공중합체 0.5∼10 중량%, 및 폴리페닐렌-에테르 공중합체 0.5∼10 중량%를 포함하는 콘크리트 구조물 보수용 균열저감형 보수재 조성물 및 이를 이용한 콘크리트 구조물의 유지 보수 방법에 관한 것이다. 본 발명에 의한 유지보수 방법은 현장 적용성, 작업성, 염소이온 침투 저항성, 내구성, 부착성, 내후성 및 방수성이 우수하여 콘크리트 구조물의 공용기간 증가, 유지보수비용 절감 및 시공성 향상을 구현할 수 있다.
The present invention relates to a crack reduction type repairing material composition which contains 3-85 wt% of rapid hardening functional binders, 10-80 wt% of fine aggregates and 5-40 wt% of water, and specifically, to a crack reduction type repairing material composition for concrete structure maintenance, wherein the rapid hardening functional binder comprises: 20-92 wt% of early strength type Portland cement; 1-30 wt% of amorphous calcium aluminate; 1-20 wt% of kaolinite; 1-20 wt% of boehmite; 1-10 wt% of fine ceramics; 1-10 wt% of gypsum; 1-10 wt% of zinc chloride; 0.5-10 wt% of polyvinyl acetate; 0.5-10 wt% of methyl methacrylate-methacrylic acid copolymer; 0.5-10 wt% of polyvinyl-methylether copolymer; and 0.5-10 wt% of polyphenylene-ether copolymer. In addition, the present invention relates to a maintenance method of concrete structures using the same. According to the present invention, the maintenance method has excellent site applicability, workability, resistance to chloride ion permeation, durability, attaching properties, resistance to weather and waterproofness, thereby increasing performance periods of concrete structures, reducing maintenance costs and improving constructability.
본 발명은 속경형 기능성 결합재 3∼85 중량%, 잔골재 10∼80 중량% 및 물 5∼40 중량%를 포함하는 균열저감형 보수재 조성물로서, 상기 속경형 기능성 결합재가 조강포틀랜드 시멘트20∼92 중량%, 비정질 칼슘알루미네이트 1∼30 중량%, 카올리나이트 1∼20 중량%, 뵘사이트 1∼20 중량%, 파인 세라믹 1∼10 중량%, 석고 1∼10 중량%, 염화아연 1∼10 중량%, 폴리초산비닐 0.5∼10 중량%, 메틸메타크릴레이트-메타아크릴산 공중합체 0.5∼10 중량%, 폴리비닐-메틸에테르 공중합체 0.5∼10 중량%, 및 폴리페닐렌-에테르 공중합체 0.5∼10 중량%를 포함하는 콘크리트 구조물 보수용 균열저감형 보수재 조성물 및 이를 이용한 콘크리트 구조물의 유지 보수 방법에 관한 것이다. 본 발명에 의한 유지보수 방법은 현장 적용성, 작업성, 염소이온 침투 저항성, 내구성, 부착성, 내후성 및 방수성이 우수하여 콘크리트 구조물의 공용기간 증가, 유지보수비용 절감 및 시공성 향상을 구현할 수 있다.
Method For Protecting Concrete Structure
콘크리트 구조물의 유지 보수 방법
KANG IN KIL (author)
2019-09-17
Patent
Electronic Resource
Korean
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2018
|European Patent Office | 2016
|European Patent Office | 2018
|European Patent Office | 2019
|