ECO-FRIENDLY MORTAR FOR PIPELINE REPAIR AND REINFORCEMENT AND PIPELINE REPAIR AND REINFORCEMENT COMPLEX PIPELINE REPAIR AND REPAIR METHOD USING THE SAME
The present invention relates to eco-friendly mortar for repairing and reinforcing a pipeline, which excludes Portland cement to increase binding force with a reinforcement material and strength while maximizing generation of hexavalent chrome (Cr^6+), which is a harmful material, and a pipeline repairing/reinforcement method using the same. According to the present invention, the eco-friendly mortar for repairing and reinforcing a pipeline comprises: 49-55 wt% of blast furnace slag cement, 0.05-0.2 wt% of twisted PE fiber, 0.2-1.5 wt% of polymer, 0.02-0.1 wt% of a thickener, 0.05-0.2 wt% of a defoamer, and 40-50 wt% of fine aggregate. To increase coupling properties and tensile strength, the twisted PE fiber is added in a shape in which twisted PE short fiber having a length of 3-6 cm and having both end parts bent in a ring shape are uniformly dispersed.
본 발명은 관로 보수·보강용 친환경 모르타르 및 이를 이용한 관로 보수보강 공법에 관한 것으로, 포틀랜드 시멘트를 배제하여 유해물질인 6가 크롬(Cr)의 발생을 극소화하면서 보강재와의 결합력과 강도를 향상시킬 수 있도록 한 것이다. 이러한 본 발명의 관로 보수부강용 친환경 모르타르는, 고로슬래그 시멘트 49~55%중량, PE 합사 0.05~0.2%중량, 폴리머 0.2~1.5%중량, 증점제 0.02~0.1%중량, 기포제 0.05~0.2%중량 및 잔골재 40~50%중량을 포함하되, 상기 PE 합사는 결합성과 인장강도를 높이기 위하여 양단부가 고리 형태로 구부러진 길이 3 내지 6cm의 단섬유 PE 합사로 구비되어 균일하게 분산된 형태로 첨가된 것을 특징으로 한다.
ECO-FRIENDLY MORTAR FOR PIPELINE REPAIR AND REINFORCEMENT AND PIPELINE REPAIR AND REINFORCEMENT COMPLEX PIPELINE REPAIR AND REPAIR METHOD USING THE SAME
The present invention relates to eco-friendly mortar for repairing and reinforcing a pipeline, which excludes Portland cement to increase binding force with a reinforcement material and strength while maximizing generation of hexavalent chrome (Cr^6+), which is a harmful material, and a pipeline repairing/reinforcement method using the same. According to the present invention, the eco-friendly mortar for repairing and reinforcing a pipeline comprises: 49-55 wt% of blast furnace slag cement, 0.05-0.2 wt% of twisted PE fiber, 0.2-1.5 wt% of polymer, 0.02-0.1 wt% of a thickener, 0.05-0.2 wt% of a defoamer, and 40-50 wt% of fine aggregate. To increase coupling properties and tensile strength, the twisted PE fiber is added in a shape in which twisted PE short fiber having a length of 3-6 cm and having both end parts bent in a ring shape are uniformly dispersed.
본 발명은 관로 보수·보강용 친환경 모르타르 및 이를 이용한 관로 보수보강 공법에 관한 것으로, 포틀랜드 시멘트를 배제하여 유해물질인 6가 크롬(Cr)의 발생을 극소화하면서 보강재와의 결합력과 강도를 향상시킬 수 있도록 한 것이다. 이러한 본 발명의 관로 보수부강용 친환경 모르타르는, 고로슬래그 시멘트 49~55%중량, PE 합사 0.05~0.2%중량, 폴리머 0.2~1.5%중량, 증점제 0.02~0.1%중량, 기포제 0.05~0.2%중량 및 잔골재 40~50%중량을 포함하되, 상기 PE 합사는 결합성과 인장강도를 높이기 위하여 양단부가 고리 형태로 구부러진 길이 3 내지 6cm의 단섬유 PE 합사로 구비되어 균일하게 분산된 형태로 첨가된 것을 특징으로 한다.
ECO-FRIENDLY MORTAR FOR PIPELINE REPAIR AND REINFORCEMENT AND PIPELINE REPAIR AND REINFORCEMENT COMPLEX PIPELINE REPAIR AND REPAIR METHOD USING THE SAME
관로 보수·보강용 친환경 모르타르 및 이를 이용한 관로 보수·보강 복합체와 관로 보수,보강공법
KIM JONG BONG (author) / LEE SEUNG IL (author) / KIM SO RA (author)
2020-08-13
Patent
Electronic Resource
Korean
Reinforcement and Repair Pressure Pipeline With CFRP
British Library Conference Proceedings | 2013
|European Patent Office | 2020
|Online Contents | 1998
|Repair-reinforcement mortar of concrete structure and repair-reinforcement method using thereof
European Patent Office | 2020
|