A platform for research: civil engineering, architecture and urbanism
METHOD FOR MANUFACTURING GROUT INJECTION MATERIAL GROUT INJECTION MATERIAL PRODUCED THEREBY AND CONSTRUCTION METHOD
The present invention relates to a method for producing a grout-injection material, a grout-injection material produced thereby, and a grouting construction method using the same, is for controlling the consolidation time and increasing the compressive strength by the improvement in composition of a ground improvement material disclosed in the existing patent registration No. 0681272, thereby suppressing flooding and maximizing the ground reinforcement efficiency. To achieve said feature, a method which is for producing a grout-injection material (AGP-S) and in which a first material (AGP-A material) and a second material (AGP-B material) is mixed, according to the present invention is characterized in that the production is made through mixing the first material and the second material in a certain ratio with each other, the first material (AGP-A material) having a mixed composition of calcium oxide (CaO), aluminum oxide (Al_2O_3), silicon dioxide (SiO_2), magnesium oxide (MgO), sulfur trioxide (SO_3), sodium aluminate (NaAlO_2), and iron trioxide (Fe_2O_3), and the second material (AGP-B material) having a mixed composition of calcium oxide (CaO), sulfur trioxide (SO_3), silicon dioxide (SiO_2), aluminum oxide (Al_2O_3), magnesium oxide (MgO), and iron trioxide (Fe_2O_3).
본 발명은 그라우트 주입재 제조방법 및 이에 의해 제조된 그라우트 주입재 및 이를 이용한 그라우팅 시공방법에 관한 것으로서, 기존 특허등록 제0681272호에 개시된 지반개량재의 성분 개선을 통한 고결시간의 조절과 압축강도가 증가되어질 수 있도록 하여 침수를 억제함과 함께 지반 보강효율이 극대화되도록 하기 위한 것이다. 이를 실현하기 위한 본 발명은, 제1재(AGP-A재)와 제2재(AGP-B재)를 혼합하여 그라우트 주입재(AGP-S)를 제조하는 방법에 있어서, 상기 제1재(AGP-A재)는 산화칼슘(CaO), 산화알루미늄(AlO), 이산화규소(SiO), 산화마그네슘(MgO), 삼산화황(SO), 소듐알루미네이트(NaAlO), 삼산화철(FeO)의 혼합 조성을 이루고; 상기 제2재(AGP-B재)는 산화칼슘(CaO), 삼산화황(SO), 이산화규소(SiO), 산화알루미늄(AlO), 산화마그네슘(MgO), 삼산화철(FeO)의 혼합 조성을 이루는 상태에서 상호간에 일정 비율로 혼합을 통해 제조가 이루어지는 것을 특징으로 한다.
METHOD FOR MANUFACTURING GROUT INJECTION MATERIAL GROUT INJECTION MATERIAL PRODUCED THEREBY AND CONSTRUCTION METHOD
The present invention relates to a method for producing a grout-injection material, a grout-injection material produced thereby, and a grouting construction method using the same, is for controlling the consolidation time and increasing the compressive strength by the improvement in composition of a ground improvement material disclosed in the existing patent registration No. 0681272, thereby suppressing flooding and maximizing the ground reinforcement efficiency. To achieve said feature, a method which is for producing a grout-injection material (AGP-S) and in which a first material (AGP-A material) and a second material (AGP-B material) is mixed, according to the present invention is characterized in that the production is made through mixing the first material and the second material in a certain ratio with each other, the first material (AGP-A material) having a mixed composition of calcium oxide (CaO), aluminum oxide (Al_2O_3), silicon dioxide (SiO_2), magnesium oxide (MgO), sulfur trioxide (SO_3), sodium aluminate (NaAlO_2), and iron trioxide (Fe_2O_3), and the second material (AGP-B material) having a mixed composition of calcium oxide (CaO), sulfur trioxide (SO_3), silicon dioxide (SiO_2), aluminum oxide (Al_2O_3), magnesium oxide (MgO), and iron trioxide (Fe_2O_3).
본 발명은 그라우트 주입재 제조방법 및 이에 의해 제조된 그라우트 주입재 및 이를 이용한 그라우팅 시공방법에 관한 것으로서, 기존 특허등록 제0681272호에 개시된 지반개량재의 성분 개선을 통한 고결시간의 조절과 압축강도가 증가되어질 수 있도록 하여 침수를 억제함과 함께 지반 보강효율이 극대화되도록 하기 위한 것이다. 이를 실현하기 위한 본 발명은, 제1재(AGP-A재)와 제2재(AGP-B재)를 혼합하여 그라우트 주입재(AGP-S)를 제조하는 방법에 있어서, 상기 제1재(AGP-A재)는 산화칼슘(CaO), 산화알루미늄(AlO), 이산화규소(SiO), 산화마그네슘(MgO), 삼산화황(SO), 소듐알루미네이트(NaAlO), 삼산화철(FeO)의 혼합 조성을 이루고; 상기 제2재(AGP-B재)는 산화칼슘(CaO), 삼산화황(SO), 이산화규소(SiO), 산화알루미늄(AlO), 산화마그네슘(MgO), 삼산화철(FeO)의 혼합 조성을 이루는 상태에서 상호간에 일정 비율로 혼합을 통해 제조가 이루어지는 것을 특징으로 한다.
METHOD FOR MANUFACTURING GROUT INJECTION MATERIAL GROUT INJECTION MATERIAL PRODUCED THEREBY AND CONSTRUCTION METHOD
그라우트 주입재 제조방법, 이에 의해 제조된 그라우트 주입재 및 이를 이용한 그라우팅 시공방법
CHOI DOO YOUNG (author)
2020-08-24
Patent
Electronic Resource
Korean
European Patent Office | 2024
|GROUT MATERIAL INJECTION METHOD, STRUCTURE REINFORCEMENT METHOD AND GROUT MATERIAL INJECTION DEVICE
European Patent Office | 2024
|GROUT MATERIAL INJECTION MANAGEMENT DEVICE, GROUT MATERIAL INJECTION MANAGEMENT METHOD, AND PROGRAM
European Patent Office | 2023
|INJECTION METHOD OF GROUT MATERIAL, AND INJECTION SUPPORT DEVICE OF GROUT MATERIAL
European Patent Office | 2024
|