A platform for research: civil engineering, architecture and urbanism
Grout material using carbon-based expansive admixture and construction method using the same
The present invention relates to a grout material injected into a gap of a structure, and specifically, to a grout material and a grouting construction method using the same, wherein a blending material includes 35-50 wt% of cement, 2 to 10 wt% of a binder, 40-60 wt% of silica sand, 0.05-0.2 wt% of an antifoaming agent, 0.01-0.5 wt% of a thickener, 0.3-1.5 wt% of a high-performance plasticizer, and 1-10 wt% of an expansive additive.
본 발명은, 구조물의 간극에 주입되는 그라우트재에 있어서, 배합재료는, 시멘트 35~50 중량%; 결합재 2~10 중량%; 규사 40~60 중량%; 소포제 0.05~0.2 중량%; 증점제 0.01~0.5 중량%; 고성능유동화제 0.3~1.5 중량%; 팽창재 1~10 중량%를 포함하는 그라우트재 및 이를 이용한 그라우팅 시공방법에 관한 것이다.
Grout material using carbon-based expansive admixture and construction method using the same
The present invention relates to a grout material injected into a gap of a structure, and specifically, to a grout material and a grouting construction method using the same, wherein a blending material includes 35-50 wt% of cement, 2 to 10 wt% of a binder, 40-60 wt% of silica sand, 0.05-0.2 wt% of an antifoaming agent, 0.01-0.5 wt% of a thickener, 0.3-1.5 wt% of a high-performance plasticizer, and 1-10 wt% of an expansive additive.
본 발명은, 구조물의 간극에 주입되는 그라우트재에 있어서, 배합재료는, 시멘트 35~50 중량%; 결합재 2~10 중량%; 규사 40~60 중량%; 소포제 0.05~0.2 중량%; 증점제 0.01~0.5 중량%; 고성능유동화제 0.3~1.5 중량%; 팽창재 1~10 중량%를 포함하는 그라우트재 및 이를 이용한 그라우팅 시공방법에 관한 것이다.
Grout material using carbon-based expansive admixture and construction method using the same
탄소계 팽창재를 이용한 그라우트재 및 이를 이용한 시공방법
LEE JEONG BAE (author)
2021-07-19
Patent
Electronic Resource
Korean
Basic Properties of Expansive Admixture with Anti-Freezing Admixture in a Grout
British Library Conference Proceedings | 1995
|GROUT COMPOSITE FOR PRESTRESSED CONCRETE PSC BRIDGE HAVING DUAL-EXPANSION EXPANSIVE ADMIXTURE
European Patent Office | 2019