REINFORCING PVA FIBER CONCRETE COMPOSITE AND MANUFACTUARING METHOD THEREOF
The present invention relates to a poly vinyl alcohol (PVA) fiber reinforced concrete composition and a preparation method thereof, which comprises: 9-20 wt% of cement; 5-10 wt% of water; 30-35 wt% of fine aggregate; 20-45 wt% of coarse aggregate; 6-25 wt% of recycled coarse aggregate; 4-7 wt% of fine powder of blast furnace slag, wherein 0.1-1.5 parts by volume of a PVA fiber is further comprised, based on 100 parts by volume. According to the present invention, weight is reduced, tensile stress and cracking occurring in contraction caused by the drying or freezing of concrete are inhibited, strength and toughness are increased, and resistance to impact, abrasion and fatigue, and durability are enhanced to improve stability and durability of a structure.
본 발명은 시멘트 9~20 중량%; 물 5~10 중량%; 잔골재 30~35 중량%; 굵은골재 20~45 중량%; 순환 굵은골재 6~25 중량%; 고로슬래그 미분말 4~7 중량%;를 포함하며, 전체 체적부가 100일 경우, PVA(Poly Vinyl Alcohol)섬유 0.1~0.5 체적부;를 더 포함하는 것을 특징으로 하는 PVA섬유 보강 콘크리트 조성물 및 이를 이용한 PVA 섬유 보강 콘크리트의 제조방법을 제시함으로써, 무게를 경량화함과 더불어, 콘크리트의 건조 또는 동결에 의해 수축 시 발생되는 인장응력 및 균열을 억제하며, 강성을 증가시키고, 인성의 증가와 충격, 마모, 피로에 대한 저항성과 내구성을 증대시켜 구조물의 안정성 및 내구성을 향상시키도록 한다.
REINFORCING PVA FIBER CONCRETE COMPOSITE AND MANUFACTUARING METHOD THEREOF
The present invention relates to a poly vinyl alcohol (PVA) fiber reinforced concrete composition and a preparation method thereof, which comprises: 9-20 wt% of cement; 5-10 wt% of water; 30-35 wt% of fine aggregate; 20-45 wt% of coarse aggregate; 6-25 wt% of recycled coarse aggregate; 4-7 wt% of fine powder of blast furnace slag, wherein 0.1-1.5 parts by volume of a PVA fiber is further comprised, based on 100 parts by volume. According to the present invention, weight is reduced, tensile stress and cracking occurring in contraction caused by the drying or freezing of concrete are inhibited, strength and toughness are increased, and resistance to impact, abrasion and fatigue, and durability are enhanced to improve stability and durability of a structure.
본 발명은 시멘트 9~20 중량%; 물 5~10 중량%; 잔골재 30~35 중량%; 굵은골재 20~45 중량%; 순환 굵은골재 6~25 중량%; 고로슬래그 미분말 4~7 중량%;를 포함하며, 전체 체적부가 100일 경우, PVA(Poly Vinyl Alcohol)섬유 0.1~0.5 체적부;를 더 포함하는 것을 특징으로 하는 PVA섬유 보강 콘크리트 조성물 및 이를 이용한 PVA 섬유 보강 콘크리트의 제조방법을 제시함으로써, 무게를 경량화함과 더불어, 콘크리트의 건조 또는 동결에 의해 수축 시 발생되는 인장응력 및 균열을 억제하며, 강성을 증가시키고, 인성의 증가와 충격, 마모, 피로에 대한 저항성과 내구성을 증대시켜 구조물의 안정성 및 내구성을 향상시키도록 한다.
REINFORCING PVA FIBER CONCRETE COMPOSITE AND MANUFACTUARING METHOD THEREOF
PVA섬유 보강 콘크리트 조성물 및 이를 이용한 PVA 섬유 보강 콘크리트의 제조방법
HA GEE JOO (author) / HA YOUNG JOO (author) / YI DONG RYUL (author) / HA JAE HOON (author) / KANG HYUN WOOK (author)
2015-12-22
Patent
Electronic Resource
Korean
IPC:
C04B
Kalk
,
LIME
REINFORCING METAL FIBER CONCRETE COMPOSITE AND MANUFACTUARING METHOD THEREOF
European Patent Office | 2015
|European Patent Office | 2016
European Patent Office | 2015
|PVA PVA REINFORCING PVA FIBER CONCRETE COMPOSITE AND MANUFACTUARING METHOD THEREOF
European Patent Office | 2016