Disclosed is a method for manufacturing a pottery washstand. The method for manufacturing a pottery washstand comprises: a spinning wheel molding step of obtaining a bowl molded body including an annular cross section and a stand molded body by molding basis material soil using a rotating spinning wheel; a drying step of drying the bowl molded body and the stand molded body which have gone through the spinning wheel molding step for 6 to 8 days; a surface cleaning step of wiping off the surfaces of the bowl molded body and the stand molded body which have gone through the drying step; a biscuit firing step of putting the bowl molded body and the stand molded body which have gone through the surface cleaning step into a kiln, and heating the same at a temperature of 850-900°C to obtain a bowl plastic body and a stand plastic body; a glaze coating step of applying adhesive glaze onto the bowl plastic body and the stand plastic body which have obtained through the biscuit firing step; and a secondary firing step of putting the bowl plastic body and the stand plastic body together into the kiln after placing the bowl plastic body on top of the stand plastic body coated with the glaze, and heating the same at a temperature of 1,250-1,350°C to obtain a pottery washstand having the stand plastic body and the bowl plastic body bonded to each other. The pottery washstand of the present invention has high intensity and durability.
도자기 세면대 제조방법이 개시된다. 이 도자기 세면대 제조방법은, 회전하는 물레를 이용해 소지토를 성형하여, 원환형 단면을 포함하는 볼(bowl) 성형체와 스탠드(stand) 성형체를 얻는 물레 성형 단계와; 상기 물레 성형 단계를 거친 볼 성형체와 스탠드 성형체를 6 ~ 8 일간 건조하는 건조 단계와; 상기 건조 단계를 거친 볼 성형체와 스탠드 성형체의 표면을 닦아내는 표면 청소 단계와; 상기 건조 단계와 상기 표면 청소 단계를 거친 볼 성형체와 스탠드 성형체를 가마에 넣고, 850 ~ 900℃ 온도로 가열하여 볼 소성체와 스탠드 소성체를 얻는 초벌구이 단계와; 상기 초벌구이 단계를 거쳐 얻은 볼 소성체와 스탠드 소성체에 접착성 유약을 바르는 유약 도포 단계와; 유약을 바른 스탠드 소성체 상단에 유약을 바른 볼 소성체를 올린 후 상기 스탠드 소성체와 상기 볼 소성체를 함께 가마에 넣고, 1250 ~ 1350℃의 온도로 가열하여, 스탠드 소성체와 볼 소성체가 접착된 도자기 세면대를 제조하는 재벌구이 단계를 포함하는 것을 특징으로 하는 도자기 세면대 제조방법.
Disclosed is a method for manufacturing a pottery washstand. The method for manufacturing a pottery washstand comprises: a spinning wheel molding step of obtaining a bowl molded body including an annular cross section and a stand molded body by molding basis material soil using a rotating spinning wheel; a drying step of drying the bowl molded body and the stand molded body which have gone through the spinning wheel molding step for 6 to 8 days; a surface cleaning step of wiping off the surfaces of the bowl molded body and the stand molded body which have gone through the drying step; a biscuit firing step of putting the bowl molded body and the stand molded body which have gone through the surface cleaning step into a kiln, and heating the same at a temperature of 850-900°C to obtain a bowl plastic body and a stand plastic body; a glaze coating step of applying adhesive glaze onto the bowl plastic body and the stand plastic body which have obtained through the biscuit firing step; and a secondary firing step of putting the bowl plastic body and the stand plastic body together into the kiln after placing the bowl plastic body on top of the stand plastic body coated with the glaze, and heating the same at a temperature of 1,250-1,350°C to obtain a pottery washstand having the stand plastic body and the bowl plastic body bonded to each other. The pottery washstand of the present invention has high intensity and durability.
도자기 세면대 제조방법이 개시된다. 이 도자기 세면대 제조방법은, 회전하는 물레를 이용해 소지토를 성형하여, 원환형 단면을 포함하는 볼(bowl) 성형체와 스탠드(stand) 성형체를 얻는 물레 성형 단계와; 상기 물레 성형 단계를 거친 볼 성형체와 스탠드 성형체를 6 ~ 8 일간 건조하는 건조 단계와; 상기 건조 단계를 거친 볼 성형체와 스탠드 성형체의 표면을 닦아내는 표면 청소 단계와; 상기 건조 단계와 상기 표면 청소 단계를 거친 볼 성형체와 스탠드 성형체를 가마에 넣고, 850 ~ 900℃ 온도로 가열하여 볼 소성체와 스탠드 소성체를 얻는 초벌구이 단계와; 상기 초벌구이 단계를 거쳐 얻은 볼 소성체와 스탠드 소성체에 접착성 유약을 바르는 유약 도포 단계와; 유약을 바른 스탠드 소성체 상단에 유약을 바른 볼 소성체를 올린 후 상기 스탠드 소성체와 상기 볼 소성체를 함께 가마에 넣고, 1250 ~ 1350℃의 온도로 가열하여, 스탠드 소성체와 볼 소성체가 접착된 도자기 세면대를 제조하는 재벌구이 단계를 포함하는 것을 특징으로 하는 도자기 세면대 제조방법.
METHOD FOR MAKING POTTERY WASHSTAND
도자기 세면대 제조방법
JO EUN HAN (author)
2016-01-18
Patent
Electronic Resource
Korean
IPC:
C04B