Method for Manufacturing of environmently friendly Saltpan floor board and construction method therefor
The present invention relates to a method for manufacturing eco-friendly tiles for a bottom of a saltpan and a construction method thereof, and more specifically, to a method for manufacturing eco-friendly tiles for a bottom of a saltpan which rapidly and conveniently manufactures tiles at a room temperature, not a high temperature with a firing process, compared with general ceramic tiles, and a construction method thereof. The method for manufacturing eco-friendly tiles for a bottom of a saltpan of the present invention comprises the steps of: mixing (S1) 50-70 wt% of prompt cement with 35-50 wt% of adhesive binders for coating layers of tiles; mixing (S2) a material, comprising 24-40 wt% of prompt cement, 15-25 wt% of silica, 45-50 wt% of aggregates, with adhesive binders having 100 wt% of prompt cement; injecting (S3) the materials of the (S1) step into a mold of which a bottom is made of separable materials, and putting fiber reinforcing materials; supplying (S4) a uniformly mixed the aggregates (S2) into the mold and forming and processing the same; and aging (S5) the formed and processed tiles at a room temperature. In addition, the present invention rapidly and conveniently builds a bottom of a saltpan, and fills pores between tiles, unlike a construction method of general tiles for a saltpan, such that foreign substances do not enter the saltpan and, accordingly, clean bay salt having a high natural mineral content can be manufactured.
본 발명은 친환경 염전 바닥용 타일의 제조방법 및 시공방법에 관한 것으로 보다 상세하게 서술하면 친환경 염전 바닥용 타일을 제조함에 있어 일반 도기타일이나 자기타일과 달리 고온에서 소성가공하지 않고 상온에서 신속하고 편리하게 제조 가능한 친환경 염전바닥용 타일의 제조방법 및 그 시공방법에 관한 것이다. 본 발명의 친환경 염전 바닥용 타일의 제조방법은 타일의 코팅층 용으로 프롬시멘트 50~70중량%와 접착바인더 35~50중량%를 혼합하는 단계(S1), 프롬시멘트 24~40중량%, 규사 15~25%중량%, 골재 45~50중량%의 재료를 프롬시멘트의 100중량%의 접착바인더와 함께 배합하는 단계(S2), 바닥이 이형물질로 이루어진 형틀에 상기 (S1) 단계 물질을 주입 한 뒤 섬유보강재를 넣는 단계(S3) 고르게 혼합된 상기 (S2)골재를 형틀에 공급하여 성형 가공하는 단계(S4)와, 성형 가공된 타일을 상온에서 숙성하는 단계(S5)로 이루어진 것1을 특징으로 한다. 또한 본 발명은 신속하고 편리하게 염전바닥을 조성하며 일반염전바닥용 타일의 시공방법과 달리 타일과 타일 사이의 공극을 메꾸어줌으로서 염전에 이물질이 유입되지 않아 천연 미네랄 함유량이 높은 청결한 천일염을 제조할 수 있는 친환경 염전 바닥용 타일의 시공방법에 관한 것이다.
Method for Manufacturing of environmently friendly Saltpan floor board and construction method therefor
The present invention relates to a method for manufacturing eco-friendly tiles for a bottom of a saltpan and a construction method thereof, and more specifically, to a method for manufacturing eco-friendly tiles for a bottom of a saltpan which rapidly and conveniently manufactures tiles at a room temperature, not a high temperature with a firing process, compared with general ceramic tiles, and a construction method thereof. The method for manufacturing eco-friendly tiles for a bottom of a saltpan of the present invention comprises the steps of: mixing (S1) 50-70 wt% of prompt cement with 35-50 wt% of adhesive binders for coating layers of tiles; mixing (S2) a material, comprising 24-40 wt% of prompt cement, 15-25 wt% of silica, 45-50 wt% of aggregates, with adhesive binders having 100 wt% of prompt cement; injecting (S3) the materials of the (S1) step into a mold of which a bottom is made of separable materials, and putting fiber reinforcing materials; supplying (S4) a uniformly mixed the aggregates (S2) into the mold and forming and processing the same; and aging (S5) the formed and processed tiles at a room temperature. In addition, the present invention rapidly and conveniently builds a bottom of a saltpan, and fills pores between tiles, unlike a construction method of general tiles for a saltpan, such that foreign substances do not enter the saltpan and, accordingly, clean bay salt having a high natural mineral content can be manufactured.
본 발명은 친환경 염전 바닥용 타일의 제조방법 및 시공방법에 관한 것으로 보다 상세하게 서술하면 친환경 염전 바닥용 타일을 제조함에 있어 일반 도기타일이나 자기타일과 달리 고온에서 소성가공하지 않고 상온에서 신속하고 편리하게 제조 가능한 친환경 염전바닥용 타일의 제조방법 및 그 시공방법에 관한 것이다. 본 발명의 친환경 염전 바닥용 타일의 제조방법은 타일의 코팅층 용으로 프롬시멘트 50~70중량%와 접착바인더 35~50중량%를 혼합하는 단계(S1), 프롬시멘트 24~40중량%, 규사 15~25%중량%, 골재 45~50중량%의 재료를 프롬시멘트의 100중량%의 접착바인더와 함께 배합하는 단계(S2), 바닥이 이형물질로 이루어진 형틀에 상기 (S1) 단계 물질을 주입 한 뒤 섬유보강재를 넣는 단계(S3) 고르게 혼합된 상기 (S2)골재를 형틀에 공급하여 성형 가공하는 단계(S4)와, 성형 가공된 타일을 상온에서 숙성하는 단계(S5)로 이루어진 것1을 특징으로 한다. 또한 본 발명은 신속하고 편리하게 염전바닥을 조성하며 일반염전바닥용 타일의 시공방법과 달리 타일과 타일 사이의 공극을 메꾸어줌으로서 염전에 이물질이 유입되지 않아 천연 미네랄 함유량이 높은 청결한 천일염을 제조할 수 있는 친환경 염전 바닥용 타일의 시공방법에 관한 것이다.
Method for Manufacturing of environmently friendly Saltpan floor board and construction method therefor
친환경 염전바닥용 타일 제조방법 및 시공방법
LEE SOON MAN (author) / LEE SEONG HWA (author) / BAE YEONG JIN (author)
2018-03-08
Patent
Electronic Resource
Korean
IPC:
B28B
Formgeben von Ton oder anderen keramischen Stoffzusammensetzungen, Schlacke oder von Mischungen, die zementartiges Material enthalten, z.B. Putzmörtel
,
SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG OR MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER
/
E04F
FINISHING WORK ON BUILDINGS, e.g. STAIRS, FLOORS
,
Ausbau von Bauwerken, z.B. Treppen, Fußböden