A platform for research: civil engineering, architecture and urbanism
Method for testing crack recovery performance of concrete
The present invention provides a concrete crack recovery performance test method, comprising the steps of: applying a cylinder-shaped concrete test piece by using epoxy as a whole; dividing the applied concrete test piece into two halves; disposing the bisected concrete test piece between an aqueous 5%-NaCl solution and an aqueous 0.3 N-NaOH solution; measuring chlorine ions passing through the bisected concrete test piece by applying DC voltage of 40 V to 80 V to the aqueous 5%-NaCl solution and the aqueous 0.3 N-NaOH solution for 4 to 8 hours; providing non-hydrated C_2S or non-hydrated C_3S and moisture to the cracked surface of the bisected concrete test piece so as to heal cracks; disposing the crack-healed concrete test piece between an aqueous 5%-NaCl solution and an aqueous 0.3 N-NaOH solution; and measuring chlorine ions passing through the crack-healed concrete test piece by applying DC voltage of 40 V to 80 V to the aqueous 5%-NaCl solution and the aqueous 0.3 N-NaOH solution for 4 to 8 hours.
본 발명은 실린더 형상의 콘크리트 시험체를 전체적으로 에폭시를 이용하여 도포하는 단계, 상기 도포된 콘크리트 시험체를 2등분하는 단계, 상기 2등분된 콘크리트 시험체를 5% NaCl 수용액과 0.3N NaOH 수용액 사이에 배치하는 단계, 상기 5% NaCl 수용액과 상기 0.3N NaOH 수용액에 40V ~ 80V 직류 전압을 4 ~ 8 시간 동안 인가하여, 상기 2등분된 콘크리트 시험체를 통과하는 염소 이온을 측정하는 단계, 상기 2등분된 콘크리트 시험체의 균열면에 미수화 CS 또는 미수화 CS와 수분을 제공하여 균열을 치유하는 단계, 상기 균열이 치유된 콘크리트 시험체를 5% NaCl 수용액과 0.3N NaOH 수용액 사이에 배치하는 단계 및 상기 5% NaCl 수용액과 상기 0.3N NaOH 수용액에 40V ~ 80V 직류 전압을 4 ~ 8 시간 동안 인가하여, 상기 균열이 치유된 콘크리트 시험체를 통과하는 염소 이온을 측정하는 단계를 포함하는 콘크리트 균열 회복 성능 시험 방법을 제공한다.
Method for testing crack recovery performance of concrete
The present invention provides a concrete crack recovery performance test method, comprising the steps of: applying a cylinder-shaped concrete test piece by using epoxy as a whole; dividing the applied concrete test piece into two halves; disposing the bisected concrete test piece between an aqueous 5%-NaCl solution and an aqueous 0.3 N-NaOH solution; measuring chlorine ions passing through the bisected concrete test piece by applying DC voltage of 40 V to 80 V to the aqueous 5%-NaCl solution and the aqueous 0.3 N-NaOH solution for 4 to 8 hours; providing non-hydrated C_2S or non-hydrated C_3S and moisture to the cracked surface of the bisected concrete test piece so as to heal cracks; disposing the crack-healed concrete test piece between an aqueous 5%-NaCl solution and an aqueous 0.3 N-NaOH solution; and measuring chlorine ions passing through the crack-healed concrete test piece by applying DC voltage of 40 V to 80 V to the aqueous 5%-NaCl solution and the aqueous 0.3 N-NaOH solution for 4 to 8 hours.
본 발명은 실린더 형상의 콘크리트 시험체를 전체적으로 에폭시를 이용하여 도포하는 단계, 상기 도포된 콘크리트 시험체를 2등분하는 단계, 상기 2등분된 콘크리트 시험체를 5% NaCl 수용액과 0.3N NaOH 수용액 사이에 배치하는 단계, 상기 5% NaCl 수용액과 상기 0.3N NaOH 수용액에 40V ~ 80V 직류 전압을 4 ~ 8 시간 동안 인가하여, 상기 2등분된 콘크리트 시험체를 통과하는 염소 이온을 측정하는 단계, 상기 2등분된 콘크리트 시험체의 균열면에 미수화 CS 또는 미수화 CS와 수분을 제공하여 균열을 치유하는 단계, 상기 균열이 치유된 콘크리트 시험체를 5% NaCl 수용액과 0.3N NaOH 수용액 사이에 배치하는 단계 및 상기 5% NaCl 수용액과 상기 0.3N NaOH 수용액에 40V ~ 80V 직류 전압을 4 ~ 8 시간 동안 인가하여, 상기 균열이 치유된 콘크리트 시험체를 통과하는 염소 이온을 측정하는 단계를 포함하는 콘크리트 균열 회복 성능 시험 방법을 제공한다.
Method for testing crack recovery performance of concrete
콘크리트 균열 회복 성능 시험 방법
LEE SANG CHUL (author)
2018-06-07
Patent
Electronic Resource
Korean
Testing of Fiberoptic Crack-Detector in Concrete
NTIS | 1989
|Concrete crack repairing device and concrete crack repairing method
European Patent Office | 2024
|Concrete crack repairing device and concrete crack repairing method
European Patent Office | 2020
|Concrete crack repairing device and concrete crack repairing method thereof
European Patent Office | 2021
|