Celadon tile and method of manufacturing the same
Disclosed are a celadon tile and a manufacturing method thereof. The disclosed celadon tile manufacturing method comprises: a molding step of forming a shape of tiles; a step of drying the molded tile; a step of biscuit-firing the dried tile; a step of glazing (coating glazes) the biscuit-fired tile; and a step of re-firing the tile having glazes coated thereon. In the glazing step, a glaze is used, containing SiO_2, Al_2O_3, Fe_2O_3, CaO, MgO, TiO_2, Na_2O, and K_2O as ingredients. The content of each ingredient of the glaze is as follows: 59.0-61.5% of SiO_2; 18.9-20.0% of Al_2O_3; 2.50-2.90% of Fe_2O_3; 10.80-11.50% of CaO; 1.50-1.90% of MgO; 0.55-0.80% of TiO_2; 1.00-1.50% of Na2_O; and 1.20-1.70% of K_2O. Such manufacturing method may further comprise a step of carving a pattern on the molded tile between the molding step and the drying step. The celadon tile of the present invention can be beneficial to user′s health by having high emittance of far infrared rays and good electromagnetic wave blocking effects.
청자 타일 및 그 제조방법에 관해 개시되어 있다. 개시된 청자 타일 제조방법은 타일의 형태를 만드는 성형 과정과, 상기 성형된 타일을 건조하는 과정과, 상기 건조된 타일을 초벌구이하는 과정과, 상기 초벌구이된 타일에 시유하는 과정(유약을 바르는 과정)과, 상기 유약이 칠해진 타일을 재벌구이하는 과정을 포함하고, 상기 시유하는 과정에서 SiO, AlO, FeO, CaO, MgO, TiO, NaO, KO를 성분으로 포함하는 유약을 사용하고, 상기 유약의 각 성분의 함량은 SiO가 59.0%~61.5%, AlO가 18.9%~20.0%, FeO가 2.50%~2.90%, CaO가 10.80%~11.50%, MgO가 1.50%~1.90%, TiO가 0.55%~0.80%, NaO가 1.00%~1.50%, KO가 1.20%~1.70% 정도일 수 있다. 이러한 제조방법에서, 상기 성형 과정과 상기 건조 과정 사이에 상기 성형된 타일에 문양을 새기는 조각하는 과정을 더 포함할 수 있다.
Celadon tile and method of manufacturing the same
Disclosed are a celadon tile and a manufacturing method thereof. The disclosed celadon tile manufacturing method comprises: a molding step of forming a shape of tiles; a step of drying the molded tile; a step of biscuit-firing the dried tile; a step of glazing (coating glazes) the biscuit-fired tile; and a step of re-firing the tile having glazes coated thereon. In the glazing step, a glaze is used, containing SiO_2, Al_2O_3, Fe_2O_3, CaO, MgO, TiO_2, Na_2O, and K_2O as ingredients. The content of each ingredient of the glaze is as follows: 59.0-61.5% of SiO_2; 18.9-20.0% of Al_2O_3; 2.50-2.90% of Fe_2O_3; 10.80-11.50% of CaO; 1.50-1.90% of MgO; 0.55-0.80% of TiO_2; 1.00-1.50% of Na2_O; and 1.20-1.70% of K_2O. Such manufacturing method may further comprise a step of carving a pattern on the molded tile between the molding step and the drying step. The celadon tile of the present invention can be beneficial to user′s health by having high emittance of far infrared rays and good electromagnetic wave blocking effects.
청자 타일 및 그 제조방법에 관해 개시되어 있다. 개시된 청자 타일 제조방법은 타일의 형태를 만드는 성형 과정과, 상기 성형된 타일을 건조하는 과정과, 상기 건조된 타일을 초벌구이하는 과정과, 상기 초벌구이된 타일에 시유하는 과정(유약을 바르는 과정)과, 상기 유약이 칠해진 타일을 재벌구이하는 과정을 포함하고, 상기 시유하는 과정에서 SiO, AlO, FeO, CaO, MgO, TiO, NaO, KO를 성분으로 포함하는 유약을 사용하고, 상기 유약의 각 성분의 함량은 SiO가 59.0%~61.5%, AlO가 18.9%~20.0%, FeO가 2.50%~2.90%, CaO가 10.80%~11.50%, MgO가 1.50%~1.90%, TiO가 0.55%~0.80%, NaO가 1.00%~1.50%, KO가 1.20%~1.70% 정도일 수 있다. 이러한 제조방법에서, 상기 성형 과정과 상기 건조 과정 사이에 상기 성형된 타일에 문양을 새기는 조각하는 과정을 더 포함할 수 있다.
Celadon tile and method of manufacturing the same
청자 타일 및 그 제조방법
LEE YONG HEE (author) / LEE SEUNG HOON (author)
2019-09-25
Patent
Electronic Resource
Korean
IPC:
C04B
Kalk
,
LIME
/
B28B
Formgeben von Ton oder anderen keramischen Stoffzusammensetzungen, Schlacke oder von Mischungen, die zementartiges Material enthalten, z.B. Putzmörtel
,
SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG OR MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER
/
C03C
Chemische Zusammensetzungen für Gläser, Glasuren oder Emails
,
CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUS ENAMELS
/
E04C
STRUCTURAL ELEMENTS
,
Bauelemente
European Patent Office | 2024
|Celadon manufacturing process and celadon manufacturing tool
European Patent Office | 2020
|CELADON GLAZE COMPOSITION AND MANUFACTURING METHOD OF THE SAME
European Patent Office | 2018
TRANSLUCENT CELADON COMPOSITION AND MANUFACTURING METHOD OF THE SAME
European Patent Office | 2019
|