FLOWABLE MATERIAL USING BOILER ASH
The present invention relates to a flowable composition including boiler ash. The flowable composition includes: 10-15 wt% of captured carbon dioxide; 30-40 wt% of boiler ash; 40-50 wt% of slag; 4-7 wt% of an activating agent; and 1-3 wt% of a quick-setting agent, wherein the boiler ash uses coal and limestone as combustion media and is generated from a circulated fluidized bed boiler carrying out complete combustion of coal and limestone by circulating heat continuously. The composition according to the present invention uses no cement causing environmental pollution. The composition uses captured carbon dioxide and slag as binders. In addition, since the composition uses slag as a binder, it can solve the problems of a rapid drop in strength and early strength development, occurring in the conventional solidifying material and a ground modifier using cement as a binder.
보일러 애시가 혼합된 본 발명의 유동성 조성물은 이산화탄소 포집물 10 ~ 15 중량%; 보일러 애시 30 ~ 40 중량%; 슬래그 40 ~ 50 중량%; 활성화제 4 ~ 7 중량%; 급결제 1 ~ 3 중량%;를 포함하되, 상기 보일러 애시는 연소매체로 석탄과 석회석을 사용하되, 지속적으로 열을 순환시켜 석탄과 석회석을 완전 연소시키는 순환 유동층 보일러에서 생성된 것이다. 본 발명의 조성물은 환경오염을 유발하는 시멘트를 전혀 사용하지 않는 특징이 있다. 본 발명은 조성물의 바인더로 이산화탄소 포집물과 슬래그를 사용한다. 아울러, 슬래그를 바인더로 사용하기 때문에 시멘트를 바인더로 사용하는 기존 고화재 및 지반 개량재의 급격한 강도저하의 문제, 초기 강도발현의 문제를 해결할 수 있다.
FLOWABLE MATERIAL USING BOILER ASH
The present invention relates to a flowable composition including boiler ash. The flowable composition includes: 10-15 wt% of captured carbon dioxide; 30-40 wt% of boiler ash; 40-50 wt% of slag; 4-7 wt% of an activating agent; and 1-3 wt% of a quick-setting agent, wherein the boiler ash uses coal and limestone as combustion media and is generated from a circulated fluidized bed boiler carrying out complete combustion of coal and limestone by circulating heat continuously. The composition according to the present invention uses no cement causing environmental pollution. The composition uses captured carbon dioxide and slag as binders. In addition, since the composition uses slag as a binder, it can solve the problems of a rapid drop in strength and early strength development, occurring in the conventional solidifying material and a ground modifier using cement as a binder.
보일러 애시가 혼합된 본 발명의 유동성 조성물은 이산화탄소 포집물 10 ~ 15 중량%; 보일러 애시 30 ~ 40 중량%; 슬래그 40 ~ 50 중량%; 활성화제 4 ~ 7 중량%; 급결제 1 ~ 3 중량%;를 포함하되, 상기 보일러 애시는 연소매체로 석탄과 석회석을 사용하되, 지속적으로 열을 순환시켜 석탄과 석회석을 완전 연소시키는 순환 유동층 보일러에서 생성된 것이다. 본 발명의 조성물은 환경오염을 유발하는 시멘트를 전혀 사용하지 않는 특징이 있다. 본 발명은 조성물의 바인더로 이산화탄소 포집물과 슬래그를 사용한다. 아울러, 슬래그를 바인더로 사용하기 때문에 시멘트를 바인더로 사용하는 기존 고화재 및 지반 개량재의 급격한 강도저하의 문제, 초기 강도발현의 문제를 해결할 수 있다.
FLOWABLE MATERIAL USING BOILER ASH
보일러 애시가 혼합된 유동성 조성물
JEONG DU SU (author) / PARK CHANG WOO (author) / CHO AH RAM (author)
2020-10-07
Patent
Electronic Resource
Korean
Flowable Fill Using Flue Gas Desulfurization Material
British Library Conference Proceedings | 2004
|Flowable fill using flue gas desulfurization material
Tema Archive | 2004
|