СПЕЧЕННЫЙ ЦИРКОНОВЫЙ МАТЕРИАЛ ДЛЯ МАТРИЦЫ ПРЕСС-ФОРМЫ
A refractory object may include a zircon body that may include at least about 0.1 wt. % and not greater than about 5.5 wt. % of an Al2O3 containing component for a total weight of the zircon body. The zircon body may further include at least about 25 wt. % and not greater than about 35 wt. % of a SiO2 component for a total weight of the zircon body.
СПЕЧЕННЫЙ ЦИРКОНОВЫЙ МАТЕРИАЛ ДЛЯ МАТРИЦЫ ПРЕСС-ФОРМЫ
A refractory object may include a zircon body that may include at least about 0.1 wt. % and not greater than about 5.5 wt. % of an Al2O3 containing component for a total weight of the zircon body. The zircon body may further include at least about 25 wt. % and not greater than about 35 wt. % of a SiO2 component for a total weight of the zircon body.
СПЕЧЕННЫЙ ЦИРКОНОВЫЙ МАТЕРИАЛ ДЛЯ МАТРИЦЫ ПРЕСС-ФОРМЫ