METHOD TO MANUFACTURE CONCRETE AND REINFORCED CONCRETE PRODUCTS, SOLID STRUCTURES AND FACILITIES
FIELD: construction.SUBSTANCE: method to manufacture concrete and reinforced concrete products, solid structures and facilities from concrete mix consists in the fact in a mixer for 1.5-3 minutes they mix sand, cement and crushed stone with water and electrolyte. The produced mix is poured into a curb, a cassette or a form, working surfaces of which are electrodes, and the mixture is exposed to electric stabilisation by sending alternating current pulses, the current density of which is in the range of 10-49 A/m, with duration of 3-7 min with a stop before each change of polarity of the pulse for more than 2 min. At the same time in process of mixture pouring into a curb, cassette or a form the mixture is exposed to vibration, then into the poured mix they install an emitter and a receiver of ultrasound at the fixed distance, for instance, 1 m. Ultrasound pulses, which are recorded in the ultrasound receiver, are generated in the emitter via identical equal time intervals, in the period of each pause before each change of polarity of the current pulse. Duration of the specified fixed distance travelling by each ultrasound pulse is determined, and by results of the measurements they calculate the value ? according to the given mathematical expression. At that moment of time, when the value ? takes the value below 1, they disconnect the pulse current and perform secondary vibration of the mix poured into the curb, cassette or form for 1-2 minutes. Afterwards the product is maintained for 5-6 hours until structural strength is achieved.EFFECT: increased efficiency and improved characteristics of manufactured products.1 tbl, 1 dwg
Изобретение относится к области изготовления строительных материалов. Способ изготовления бетонных и железобетонных изделий, монолитных конструкций и сооружений из бетонной смеси заключается в том, что в смесителе в течение 1,5-3 минут смешивают песок, цемент и щебень с водой и электролитом. Заливают полученную смесь в опалубку, кассету или форму, рабочие поверхности которых являются электродами, и подвергают смесь электростабилизации пропусканием знакопеременных импульсов тока, плотность тока которых лежит в диапазоне 10-49 А/м,продолжительностью 3-7 мин с остановкой перед каждой сменой полярности импульса более 2 мин. При этом в процессе заливки смеси в опалубку, кассету или форму смесь подвергают вибрации, затем в залитую смесь устанавливают на фиксированном расстоянии, например 1 м, излучатель и приемник ультразвука. Генерируют в излучателе через одинаковые равные между собой интервалы времени, в период каждой паузы перед каждой сменой полярности импульса тока, импульсы ультразвука, которые регистрируют в приемнике ультразвука. Определяют длительность прохождения каждым импульсом ультразвука указанного фиксированного расстояния и по результатам измерений рассчитывают величину α по приведенному математическому выражению. В тот момент времени, когда величина α примет значение меньше 1, отключают импульсный ток и проводят вторичную вибрацию залитой в опалубку, кассету или форму смеси в течение 1-2 минут. После чего выдерживают изделие в течение 5-6 часов до достижения конструкционной прочности. Техническим результатом является повышение производительности и улучшение характеристик изготавливаемых из
METHOD TO MANUFACTURE CONCRETE AND REINFORCED CONCRETE PRODUCTS, SOLID STRUCTURES AND FACILITIES
FIELD: construction.SUBSTANCE: method to manufacture concrete and reinforced concrete products, solid structures and facilities from concrete mix consists in the fact in a mixer for 1.5-3 minutes they mix sand, cement and crushed stone with water and electrolyte. The produced mix is poured into a curb, a cassette or a form, working surfaces of which are electrodes, and the mixture is exposed to electric stabilisation by sending alternating current pulses, the current density of which is in the range of 10-49 A/m, with duration of 3-7 min with a stop before each change of polarity of the pulse for more than 2 min. At the same time in process of mixture pouring into a curb, cassette or a form the mixture is exposed to vibration, then into the poured mix they install an emitter and a receiver of ultrasound at the fixed distance, for instance, 1 m. Ultrasound pulses, which are recorded in the ultrasound receiver, are generated in the emitter via identical equal time intervals, in the period of each pause before each change of polarity of the current pulse. Duration of the specified fixed distance travelling by each ultrasound pulse is determined, and by results of the measurements they calculate the value ? according to the given mathematical expression. At that moment of time, when the value ? takes the value below 1, they disconnect the pulse current and perform secondary vibration of the mix poured into the curb, cassette or form for 1-2 minutes. Afterwards the product is maintained for 5-6 hours until structural strength is achieved.EFFECT: increased efficiency and improved characteristics of manufactured products.1 tbl, 1 dwg
Изобретение относится к области изготовления строительных материалов. Способ изготовления бетонных и железобетонных изделий, монолитных конструкций и сооружений из бетонной смеси заключается в том, что в смесителе в течение 1,5-3 минут смешивают песок, цемент и щебень с водой и электролитом. Заливают полученную смесь в опалубку, кассету или форму, рабочие поверхности которых являются электродами, и подвергают смесь электростабилизации пропусканием знакопеременных импульсов тока, плотность тока которых лежит в диапазоне 10-49 А/м,продолжительностью 3-7 мин с остановкой перед каждой сменой полярности импульса более 2 мин. При этом в процессе заливки смеси в опалубку, кассету или форму смесь подвергают вибрации, затем в залитую смесь устанавливают на фиксированном расстоянии, например 1 м, излучатель и приемник ультразвука. Генерируют в излучателе через одинаковые равные между собой интервалы времени, в период каждой паузы перед каждой сменой полярности импульса тока, импульсы ультразвука, которые регистрируют в приемнике ультразвука. Определяют длительность прохождения каждым импульсом ультразвука указанного фиксированного расстояния и по результатам измерений рассчитывают величину α по приведенному математическому выражению. В тот момент времени, когда величина α примет значение меньше 1, отключают импульсный ток и проводят вторичную вибрацию залитой в опалубку, кассету или форму смеси в течение 1-2 минут. После чего выдерживают изделие в течение 5-6 часов до достижения конструкционной прочности. Техническим результатом является повышение производительности и улучшение характеристик изготавливаемых из
METHOD TO MANUFACTURE CONCRETE AND REINFORCED CONCRETE PRODUCTS, SOLID STRUCTURES AND FACILITIES
СПОСОБ ИЗГОТОВЛЕНИЯ БЕТОННЫХ И ЖЕЛЕЗОБЕТОННЫХ ИЗДЕЛИЙ, МОНОЛИТНЫХ КОНСТРУКЦИЙ И СООРУЖЕНИЙ
SMIRNOV GENNADIJ VASIL EVICH (author) / SMIRNOV DMITRIJ GENNAD EVICH (author)
2015-06-10
Patent
Electronic Resource
Russian
Crushed concrete as concrete aggregate in the manufacture of reinforced concrete structures
DOAJ | 2018
|Manufacture of reinforced concrete pipes
Engineering Index Backfile | 1941
|REINFORCEMENT FOR REINFORCED CONCRETE STRUCTURES AND METHOD OF ITS MANUFACTURE
European Patent Office | 2024
|