METHOD OF PRODUCTION OF NANODISPERSE ADDITIVE FOR CONCRETE
FIELD: biotechnologies.SUBSTANCE: method of production of nanodisperse additive for concrete is offered. Cyanobacteria of the sort Pseudanabaena sp. 0411 or Leptolyngbya laminosa 0412 are cultivated in a nutrient medium at the temperature 23-25°C. The nutrient medium is Z-8 medium with adding of sodium silicate solution neutralized by 2 M HCl. Ratio of solution of silicate of sodium and Z-8 5:1 medium. Cultivation is carried out in the bioreactor at continuous lighting and mixing during 10 days with the subsequent removal of nutrient medium residue. Then the culture is poured by 30% hydrogen peroxide solution and heated up to 70°C. The produced biosilicated nanotubes are washed out by distilled water with subsequent treatment in a mechanical activator in the water medium of anion surface-active substance of naphthalene formaldehyde type at the ultrasound frequency 35 kHz and concentration of solid phase 5% up to the particle size 85-250 nanometres.EFFECT: increase of mobility of concrete mix, curing acceleration, increase of strength and density of concrete, decrease of water absorption.3 tbl, 1 ex
Изобретение относится к области биотехнологии. Предложен способ получения нанодисперсной добавки для бетона. Цианобактерии вида Pseudanabaena sp. 0411 или Leptolyngbya laminosa 0412 культивируют на питательной среде при температуре 23-25°C. В качестве питательной среды используют среду Z-8 с добавлением раствора силиката натрия, нейтрализованного 2 М HCl. Соотношение раствора силиката натрия и среды Z-8 5:1. Культивирование осуществляют в биореакторе при постоянном освещении и перемешивании в течение 10 суток с последующим удалением остатков питательной среды. Затем культуру заливают 30% раствором пероксида водорода и нагревают до 70°C. Полученные биосилифицированные нанотрубки промывают дистиллированной водой с последующей обработкой в механоактиваторе в водной среде анионного поверхностно-активного вещества нафталинформальдегидного типа при частоте ультразвука 35 кГц и концентрации твердой фазы 5% до размера частиц 85-250 нм. Преимуществом способа является увеличение подвижности бетонной смеси, ускорение твердения, повышение прочности и плотности бетона, снижение водопоглощения. 3 табл., 1 пр.
METHOD OF PRODUCTION OF NANODISPERSE ADDITIVE FOR CONCRETE
FIELD: biotechnologies.SUBSTANCE: method of production of nanodisperse additive for concrete is offered. Cyanobacteria of the sort Pseudanabaena sp. 0411 or Leptolyngbya laminosa 0412 are cultivated in a nutrient medium at the temperature 23-25°C. The nutrient medium is Z-8 medium with adding of sodium silicate solution neutralized by 2 M HCl. Ratio of solution of silicate of sodium and Z-8 5:1 medium. Cultivation is carried out in the bioreactor at continuous lighting and mixing during 10 days with the subsequent removal of nutrient medium residue. Then the culture is poured by 30% hydrogen peroxide solution and heated up to 70°C. The produced biosilicated nanotubes are washed out by distilled water with subsequent treatment in a mechanical activator in the water medium of anion surface-active substance of naphthalene formaldehyde type at the ultrasound frequency 35 kHz and concentration of solid phase 5% up to the particle size 85-250 nanometres.EFFECT: increase of mobility of concrete mix, curing acceleration, increase of strength and density of concrete, decrease of water absorption.3 tbl, 1 ex
Изобретение относится к области биотехнологии. Предложен способ получения нанодисперсной добавки для бетона. Цианобактерии вида Pseudanabaena sp. 0411 или Leptolyngbya laminosa 0412 культивируют на питательной среде при температуре 23-25°C. В качестве питательной среды используют среду Z-8 с добавлением раствора силиката натрия, нейтрализованного 2 М HCl. Соотношение раствора силиката натрия и среды Z-8 5:1. Культивирование осуществляют в биореакторе при постоянном освещении и перемешивании в течение 10 суток с последующим удалением остатков питательной среды. Затем культуру заливают 30% раствором пероксида водорода и нагревают до 70°C. Полученные биосилифицированные нанотрубки промывают дистиллированной водой с последующей обработкой в механоактиваторе в водной среде анионного поверхностно-активного вещества нафталинформальдегидного типа при частоте ультразвука 35 кГц и концентрации твердой фазы 5% до размера частиц 85-250 нм. Преимуществом способа является увеличение подвижности бетонной смеси, ускорение твердения, повышение прочности и плотности бетона, снижение водопоглощения. 3 табл., 1 пр.
METHOD OF PRODUCTION OF NANODISPERSE ADDITIVE FOR CONCRETE
СПОСОБ ПОЛУЧЕНИЯ НАНОДИСПЕРСНОЙ ДОБАВКИ ДЛЯ БЕТОНА
LUKUTTSOVA NATAL JA PETROVNA (author) / USTINOV ALEKSANDR GENNAD EVICH (author)
2015-07-20
Patent
Electronic Resource
Russian
Fibre concrete havinga nanodisperse silica additive Фибробетон с добавкой нанодисперсного кремнезема
DOAJ | 2013
|MANUFACTURING METHOD OF COMPLEX NANODISPERSE ADDITIVE FOR HIGH-STRENGTH CONCRETE
European Patent Office | 2015
|Fine Grain Portland Cement Concrete with Complex Nanodisperse Admixture for Structure Rehabilitating
British Library Conference Proceedings | 2015
|Fine Grain Portland Cement Concrete with Complex Nanodisperse Admixture for Structure Rehabilitating
Trans Tech Publications | 2015
|