A platform for research: civil engineering, architecture and urbanism
METHOD OF PREPARING CONCRETE MIXTURE
FIELD: construction.SUBSTANCE: invention relates to construction, namely to methods of preparing concrete mixture and mortar, concrete and structures, and can be used in production of articles and structures in prefabricated house building and monolithic construction. Method involves pretreatment of portland cement together with metakaolin and superplasticizer based on polycarboxylate ester by vortex layer of anisotropic ferromagnetic bodies in nonmagnetic reservoir located in apparatus with external electromagnetic field. At the same time portland cement together with metakaolin and superplasticizer by means of translational movement of the piston is supplied along the inner cavity of the nonmagnetic continuous pipe into the zone of rotating anisotropic ferromagnetic bodies with diameter of 0.8–1.5 mm and length of 5–10 mm, motion of which is provided by the apparatus with external electromagnetic field. At that energy saturation and length of working zone make at least 100 kW/mand 0.6 m, activation time – 4–8 minutes. Ratio of said components is, wt. %: portland cement – 75.0–85.0, superplasticizer – 0.75–0.85, metakaolin – the rest. Further, the activated binder is mixed with coarse and fine aggregate, watered and additionally mixed in a concrete mixer for at least 5 minutes.EFFECT: high mobility of the concrete mixture, high early and high-grade strength of concrete articles for compression, high frost resistance.1 cl, 1 ex, 1 tbl
Изобретение относится к области строительства, а именно к способам приготовления бетонной смеси и строительных растворов, бетонов и конструкций, и может быть использовано в технологии производства изделий и конструкций в сборном домостроении и в монолитном строительстве. Способ включает предварительную обработку портландцемента совместно с метакаолином и суперпластификатором на основе эфира поликарбоксилата вихревым слоем анизотропных ферромагнитных тел в немагнитной емкости, расположенной в аппарате с наружным электромагнитным полем. При этом портландцемент совместно с метакаолином и суперпластификатором посредством поступательного движения поршня подают по внутренней полости немагнитной непрерывной трубы в зону вращающихся анизотропных ферромагнитных тел диаметром 0,8-1,5 мм и длиной 5-10 мм, движение которых обеспечивает аппарат с наружным электромагнитным полем. При этом энергонасыщенность и длина рабочей зоны составляют не менее 100 кВт/ми 0,6 м, время активации - 4-8 мин. Соотношение указанных компонентов составляет, мас.%: портландцемент - 75,0-85,0, суперпластификатор - 0,75-0,85, метакаолин – остальное. Далее активированное вяжущее перемешивают с крупным и мелким заполнителем, затворяют водой и дополнительно перемешивают в бетоносмесителе в течение не менее 5 мин. Техническим результатом является повышение подвижности бетонной смеси, повышение ранней и марочной прочности бетонных изделий на сжатие, повышение морозостойкости. 1 пр., 1 табл.
METHOD OF PREPARING CONCRETE MIXTURE
FIELD: construction.SUBSTANCE: invention relates to construction, namely to methods of preparing concrete mixture and mortar, concrete and structures, and can be used in production of articles and structures in prefabricated house building and monolithic construction. Method involves pretreatment of portland cement together with metakaolin and superplasticizer based on polycarboxylate ester by vortex layer of anisotropic ferromagnetic bodies in nonmagnetic reservoir located in apparatus with external electromagnetic field. At the same time portland cement together with metakaolin and superplasticizer by means of translational movement of the piston is supplied along the inner cavity of the nonmagnetic continuous pipe into the zone of rotating anisotropic ferromagnetic bodies with diameter of 0.8–1.5 mm and length of 5–10 mm, motion of which is provided by the apparatus with external electromagnetic field. At that energy saturation and length of working zone make at least 100 kW/mand 0.6 m, activation time – 4–8 minutes. Ratio of said components is, wt. %: portland cement – 75.0–85.0, superplasticizer – 0.75–0.85, metakaolin – the rest. Further, the activated binder is mixed with coarse and fine aggregate, watered and additionally mixed in a concrete mixer for at least 5 minutes.EFFECT: high mobility of the concrete mixture, high early and high-grade strength of concrete articles for compression, high frost resistance.1 cl, 1 ex, 1 tbl
Изобретение относится к области строительства, а именно к способам приготовления бетонной смеси и строительных растворов, бетонов и конструкций, и может быть использовано в технологии производства изделий и конструкций в сборном домостроении и в монолитном строительстве. Способ включает предварительную обработку портландцемента совместно с метакаолином и суперпластификатором на основе эфира поликарбоксилата вихревым слоем анизотропных ферромагнитных тел в немагнитной емкости, расположенной в аппарате с наружным электромагнитным полем. При этом портландцемент совместно с метакаолином и суперпластификатором посредством поступательного движения поршня подают по внутренней полости немагнитной непрерывной трубы в зону вращающихся анизотропных ферромагнитных тел диаметром 0,8-1,5 мм и длиной 5-10 мм, движение которых обеспечивает аппарат с наружным электромагнитным полем. При этом энергонасыщенность и длина рабочей зоны составляют не менее 100 кВт/ми 0,6 м, время активации - 4-8 мин. Соотношение указанных компонентов составляет, мас.%: портландцемент - 75,0-85,0, суперпластификатор - 0,75-0,85, метакаолин – остальное. Далее активированное вяжущее перемешивают с крупным и мелким заполнителем, затворяют водой и дополнительно перемешивают в бетоносмесителе в течение не менее 5 мин. Техническим результатом является повышение подвижности бетонной смеси, повышение ранней и марочной прочности бетонных изделий на сжатие, повышение морозостойкости. 1 пр., 1 табл.
METHOD OF PREPARING CONCRETE MIXTURE
СПОСОБ ПРИГОТОВЛЕНИЯ БЕТОННОЙ СМЕСИ
IBRAGIMOV RUSLAN ABDIRASHITOVICH (author) / KOROLEV EVGENIJ VALEREVICH (author) / KHUZIAKHMETOV RIFKAT KHABIBRAKHMANOVICH (author) / DEBERDEEV TIMUR RUSTAMOVICH (author)
2019-05-22
Patent
Electronic Resource
Russian
IPC:
C04B
Kalk
,
LIME