ADDITIVE METHOD FOR OBTAINING DIMENSION PRODUCTS FROM CONDUCTIVE CERAMICS BY SPARK PLASMA SINTERING
FIELD: material processing.SUBSTANCE: method relates to the technique of hot pressing with simultaneous sintering of powders and to the thermomechanical class of welding using thermal energy and pressure. An additive method for producing dimensional products from conductive materials by spark plasma sintering involves prebaking of the connected parts, placing the powder of the base material between the connected parts, while only the first connected part is presintered, and the second and subsequent parts are obtained by filling the powder of the original ceramics into a mold in which one of the punches is already sintered, followed by joint electric spark plasma sintering. Sintering is carried out in a vacuum or in a protective argon atmosphere at high temperatures released in the powder. Finished products (carbides, borides: SiC, TiC, TaC, ZrB2, HfB2, metals: W, Mo, Ta, Nb and their alloys, including high-entropy) are obtained by combining several successively baked parts and powder layers into one whole.EFFECT: expansion of the range of solutions in large size equipment production.5 cl, 6 dwg
Способ относится к технике горячего прессования с одновременным спеканием порошков и к термомеханическому классу сварки с использованием тепловой энергии и давления. Аддитивный способ получения габаритных изделий из токопроводящих материалов методом искрового плазменного спекания включает предварительный обжиг соединяемых деталей, размещение между соединяемыми деталями порошка материала основы, при этом только первую соединяемую деталь подвергают предварительному спеканию, а вторую и последующие детали получают путем засыпки порошка исходной керамики в форму, в которой одним из пуансонов служит уже спеченная деталь, с последующим проведением совместного электроискрового плазменного спекания. Спекание проводят в вакууме или в защитной атмосфере аргона при высоких температурах, выделяемых в порошке. Готовые изделия (карбиды, бориды - SiC, TiC, ТаС, ZrB2, HfB2, металлы - W, Mo, Та, Nb и их сплавы, в том числе высокоэнтропийные) получают путем объединения нескольких последовательно припекаемых деталей и порошковых слоев в одно целое. 4 з.п. ф-лы, 6 ил.
ADDITIVE METHOD FOR OBTAINING DIMENSION PRODUCTS FROM CONDUCTIVE CERAMICS BY SPARK PLASMA SINTERING
FIELD: material processing.SUBSTANCE: method relates to the technique of hot pressing with simultaneous sintering of powders and to the thermomechanical class of welding using thermal energy and pressure. An additive method for producing dimensional products from conductive materials by spark plasma sintering involves prebaking of the connected parts, placing the powder of the base material between the connected parts, while only the first connected part is presintered, and the second and subsequent parts are obtained by filling the powder of the original ceramics into a mold in which one of the punches is already sintered, followed by joint electric spark plasma sintering. Sintering is carried out in a vacuum or in a protective argon atmosphere at high temperatures released in the powder. Finished products (carbides, borides: SiC, TiC, TaC, ZrB2, HfB2, metals: W, Mo, Ta, Nb and their alloys, including high-entropy) are obtained by combining several successively baked parts and powder layers into one whole.EFFECT: expansion of the range of solutions in large size equipment production.5 cl, 6 dwg
Способ относится к технике горячего прессования с одновременным спеканием порошков и к термомеханическому классу сварки с использованием тепловой энергии и давления. Аддитивный способ получения габаритных изделий из токопроводящих материалов методом искрового плазменного спекания включает предварительный обжиг соединяемых деталей, размещение между соединяемыми деталями порошка материала основы, при этом только первую соединяемую деталь подвергают предварительному спеканию, а вторую и последующие детали получают путем засыпки порошка исходной керамики в форму, в которой одним из пуансонов служит уже спеченная деталь, с последующим проведением совместного электроискрового плазменного спекания. Спекание проводят в вакууме или в защитной атмосфере аргона при высоких температурах, выделяемых в порошке. Готовые изделия (карбиды, бориды - SiC, TiC, ТаС, ZrB2, HfB2, металлы - W, Mo, Та, Nb и их сплавы, в том числе высокоэнтропийные) получают путем объединения нескольких последовательно припекаемых деталей и порошковых слоев в одно целое. 4 з.п. ф-лы, 6 ил.
ADDITIVE METHOD FOR OBTAINING DIMENSION PRODUCTS FROM CONDUCTIVE CERAMICS BY SPARK PLASMA SINTERING
АДДИТИВНЫЙ СПОСОБ ПОЛУЧЕНИЯ ГАБАРИТНЫХ ИЗДЕЛИЙ ИЗ ТОКОПРОВОДЯЩЕЙ КЕРАМИКИ МЕТОДОМ ИСКРОВОГО ПЛАЗМЕННОГО СПЕКАНИЯ
ANISIMOV ALEKSANDR GEORGIEVICH (author) / MALI VYACHESLAV IOSIFOVICH (author) / ESIKOV MAKSIM ALEKSANDROVICH (author) / KRIZHANOVSKIJ VYACHESLAV VASILEVICH (author)
2021-12-13
Patent
Electronic Resource
Russian
Study of rare-earth oxide sintering additive systems for Spark Plasma Sintering AlN ceramics
British Library Online Contents | 2010
|Sparking advanced ceramics: Spark plasma sintering
British Library Online Contents | 2010
Spark Plasma Sintering of Nano-Crystalline Ceramics
British Library Online Contents | 2004
|SPACER FOR SPARK PLASMA SINTERING, SPARK PLASMA SINTERING DEVICE, AND SPARK PLASMA SINTERING METHOD
European Patent Office | 2018
|Preparation of SiC Ceramics by Spark Plasma Sintering
British Library Online Contents | 2002
|