Composite of cobalt-based perovskite material with negative thermal expansion material, and preparation method of same, and solid oxide fuel cell comprising same
The present invention relates to a composite of a cobalt-based perovskite material with a negative thermal expansion material, and a preparation method of the same, and a solid oxide fuel cell (SOFC) comprising the same, and belongs to the technical field of fuel cells. In the present invention, a negative thermal expansion material is introduced into a cobalt-based perovskite oxide to successfully prepare an SOFC cathode material with excellent electrochemical performance and low thermal expansivity. The composite electrode achieves prominent mechanical tolerance in SOFC, which can moderate a volume change during the whole calcination process and enable a smooth transition to a high-temperature stage. The composite electrode has a thermal expansion coefficient (TEC) only of 12.9×10−6 K−1, which is perfectly matched with that of an SDC electrolyte. In addition, the composite shows excellent oxygen reduction reaction (ORR) activity, high TEC, and extremely-excellent anti-CO2 poisoning performance.
Composite of cobalt-based perovskite material with negative thermal expansion material, and preparation method of same, and solid oxide fuel cell comprising same
The present invention relates to a composite of a cobalt-based perovskite material with a negative thermal expansion material, and a preparation method of the same, and a solid oxide fuel cell (SOFC) comprising the same, and belongs to the technical field of fuel cells. In the present invention, a negative thermal expansion material is introduced into a cobalt-based perovskite oxide to successfully prepare an SOFC cathode material with excellent electrochemical performance and low thermal expansivity. The composite electrode achieves prominent mechanical tolerance in SOFC, which can moderate a volume change during the whole calcination process and enable a smooth transition to a high-temperature stage. The composite electrode has a thermal expansion coefficient (TEC) only of 12.9×10−6 K−1, which is perfectly matched with that of an SDC electrolyte. In addition, the composite shows excellent oxygen reduction reaction (ORR) activity, high TEC, and extremely-excellent anti-CO2 poisoning performance.
Composite of cobalt-based perovskite material with negative thermal expansion material, and preparation method of same, and solid oxide fuel cell comprising same
ZHOU WEI (author) / ZHANG YUAN (author) / ZHOU CHUAN (author) / YANG GUANGMING (author) / SHAO ZONGPING (author)
2024-07-09
Patent
Electronic Resource
English
European Patent Office | 2022
|Negative thermal expansion material and composite material comprising same
European Patent Office | 2019
|NEGATIVE THERMAL EXPANSION MATERIAL, METHOD FOR PRODUCING SAME, AND COMPOSITE MATERIAL
European Patent Office | 2025
|NEGATIVE THERMAL EXPANSION MATERIAL, METHOD FOR PRODUCING SAME, AND COMPOSITE MATERIAL
European Patent Office | 2025
|NEGATIVE THERMAL EXPANSION MATERIAL, METHOD FOR MANUFACTURING SAME, AND COMPOSITE MATERIAL
European Patent Office | 2025
|