A platform for research: civil engineering, architecture and urbanism
HIGH-STRENGTH PORTLAND CEMENT SLURRY FOR ULTRA-HIGH TEMPERATURE CEMENTING, PREPARATION METHOD THEREFOR AND APPLICATION THEREOF
A high-strength Portland cement slurry for ultra-high-temperature cementing, a preparation method therefor and an application thereof. In parts by weight, the composition of the cement slurry comprises: 100 parts of Portland cement, 4-6 parts of a high temperature anti-cracking material, 80-105 parts of a high-temperature reinforcing material, 70-78 parts of water, 0.5-1.5 parts of a dispersant, 1-3 parts of a fluid loss reducer, 0.5-2.5 parts of a retarder and 0.2-0.5 parts of a defoamer; the high-temperature reinforcing material is a combination of acid-washed quartz sand, metakaolin and aluminum sulfate, a combination of acid-washed quartz sand, metakaolin, feldspar and sodium sulfate, or a combination of acid-washed quartz sand, metakaolin, feldspar and calcium nitrite. The cement slurry has good settling stability, rapid strength development in low temperatures, high compressive strength of cement stone at a high temperature of 600° C., and stable development of long-term high-temperature compressive strength.
HIGH-STRENGTH PORTLAND CEMENT SLURRY FOR ULTRA-HIGH TEMPERATURE CEMENTING, PREPARATION METHOD THEREFOR AND APPLICATION THEREOF
A high-strength Portland cement slurry for ultra-high-temperature cementing, a preparation method therefor and an application thereof. In parts by weight, the composition of the cement slurry comprises: 100 parts of Portland cement, 4-6 parts of a high temperature anti-cracking material, 80-105 parts of a high-temperature reinforcing material, 70-78 parts of water, 0.5-1.5 parts of a dispersant, 1-3 parts of a fluid loss reducer, 0.5-2.5 parts of a retarder and 0.2-0.5 parts of a defoamer; the high-temperature reinforcing material is a combination of acid-washed quartz sand, metakaolin and aluminum sulfate, a combination of acid-washed quartz sand, metakaolin, feldspar and sodium sulfate, or a combination of acid-washed quartz sand, metakaolin, feldspar and calcium nitrite. The cement slurry has good settling stability, rapid strength development in low temperatures, high compressive strength of cement stone at a high temperature of 600° C., and stable development of long-term high-temperature compressive strength.
HIGH-STRENGTH PORTLAND CEMENT SLURRY FOR ULTRA-HIGH TEMPERATURE CEMENTING, PREPARATION METHOD THEREFOR AND APPLICATION THEREOF
ZHANG HUA (author) / JIN JIANZHOU (author) / YU YONGJIN (author) / QU CONGFENG (author) / QI FENGZHONG (author) / XU MING (author) / LIU SHUOQIONG (author) / WANG ZHAOHUI (author) / GUO YUCHAO (author) / LIU JILIANG (author)
2023-09-07
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2024
|European Patent Office | 2022
|European Patent Office | 2024
|Cementing material composition, cement slurry and preparation method and application thereof
European Patent Office | 2024
|High temperature resistant Portland cement slurry and production method thereof
European Patent Office | 2023
|