A platform for research: civil engineering, architecture and urbanism
HYDROPHOBIC ADMIXTURE AND PROCESSES FOR MAKING SAME
A hydrophobic admixture may include titanium dioxide at about 1-16.5 weight % (wt %) of the hydrophobic admixture. The hydrophobic admixture can include a carbon allotrope at about 1-38.5 wt % of the hydrophobic admixture. The hydrophobic admixture may include calcium salt at about 25-82.5 wt % of the hydrophobic admixture. The hydrophobic admixture may include calcium stearate at about 15-27.5 wt % of the hydrophobic admixture. The hydrophobic admixture may include magnesium carbonate at about 0-11 wt % of the hydrophobic admixture.
HYDROPHOBIC ADMIXTURE AND PROCESSES FOR MAKING SAME
A hydrophobic admixture may include titanium dioxide at about 1-16.5 weight % (wt %) of the hydrophobic admixture. The hydrophobic admixture can include a carbon allotrope at about 1-38.5 wt % of the hydrophobic admixture. The hydrophobic admixture may include calcium salt at about 25-82.5 wt % of the hydrophobic admixture. The hydrophobic admixture may include calcium stearate at about 15-27.5 wt % of the hydrophobic admixture. The hydrophobic admixture may include magnesium carbonate at about 0-11 wt % of the hydrophobic admixture.
HYDROPHOBIC ADMIXTURE AND PROCESSES FOR MAKING SAME
DUMITRAS ALAN (author) / SOTO MATIAS (author) / VALE RECHARLIS SOUZA DO (author)
2024-01-04
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Admixture, flowable material, hardened material, and method of making the same
European Patent Office | 2019
|Admixture, Flowable Material, Hardened Material, and Method of Making the Same
European Patent Office | 2017
|ADMIXTURE, FLOWABLE MATERIAL, HARDENED MATERIAL, AND METHOD OF MAKING THE SAME
European Patent Office | 2017
|ALKALI-SILICA MITIGATION ADMIXTURE, METHODS OF MAKING AND KITS COMPRISING THE SAME
European Patent Office | 2021
|