A platform for research: civil engineering, architecture and urbanism
PROPYLENE ETHYLENE COPOLYMER
A propylene ethylene copolymer having:i) a xylene soluble fraction at 25° C. ranging from 30 wt % to 48 wt %;ii) an intrinsic viscosity of the xylene soluble fraction, ranging from 2.8 to 4.3 dl/g;iii) a melt flow rate, measured according to ISO 1133 at 230° C. with a load of 2.16 kg, ranging from 0.2 g/10 min to 10 g/10 min;iv) an ethylene derived units content ranging from 10.3 wt % to 15.4 wt %;v) the ethylene derived units content on the xylene insoluble fraction, ranging from 6.1 wt % to 9.0 wt %;vi) the ethylene derived units content on the xylene soluble fraction, ranging from 18.2. wt % to 30.2 wt %;vii) the 13C-NMR sequences PEP measured on the xylene insoluble fraction, ranging from 4.1 mol % to 6.5 mol %; and(viii) the 13C-NMR sequences PEP measured on the xylene soluble fraction, ranging from 10.5 mol % to 14.2 mol %.
PROPYLENE ETHYLENE COPOLYMER
A propylene ethylene copolymer having:i) a xylene soluble fraction at 25° C. ranging from 30 wt % to 48 wt %;ii) an intrinsic viscosity of the xylene soluble fraction, ranging from 2.8 to 4.3 dl/g;iii) a melt flow rate, measured according to ISO 1133 at 230° C. with a load of 2.16 kg, ranging from 0.2 g/10 min to 10 g/10 min;iv) an ethylene derived units content ranging from 10.3 wt % to 15.4 wt %;v) the ethylene derived units content on the xylene insoluble fraction, ranging from 6.1 wt % to 9.0 wt %;vi) the ethylene derived units content on the xylene soluble fraction, ranging from 18.2. wt % to 30.2 wt %;vii) the 13C-NMR sequences PEP measured on the xylene insoluble fraction, ranging from 4.1 mol % to 6.5 mol %; and(viii) the 13C-NMR sequences PEP measured on the xylene soluble fraction, ranging from 10.5 mol % to 14.2 mol %.
PROPYLENE ETHYLENE COPOLYMER
TARTARI DAVIDE (author) / MOSCARDI GILBERTO (author) / GALVAN MONICA (author)
2024-10-24
Patent
Electronic Resource
English
IPC:
C08F
MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
,
Makromolekulare Verbindungen, erhalten durch Reaktionen, an denen nur ungesättigte Kohlenstoff-Kohlenstoff-Bindungen beteiligt sind
/
C08J
Verarbeitung
,
WORKING-UP
/
E02D
FOUNDATIONS
,
Gründungen
/
E04D
ROOF COVERINGS
,
Dacheindeckungen
Methacryloyl carbamate functionalized ethylene-propylene copolymer
British Library Online Contents | 2001
|Degradation of ethylene-propylene copolymer in the presence of phenolic antioxidants
British Library Online Contents | 1995
|Strain rate sensitive behavior of wollastonite-reinforced ethylene-propylene copolymer composites
British Library Online Contents | 2004
|Propylene-Ethylene Copolymer Nanocomposites: Epoxy Resin Grafted Nanosilica as a Reinforcing Filler
British Library Online Contents | 2005
|