A platform for research: civil engineering, architecture and urbanism
SLIP RESISTANT ARTICLE AND THE METHOD FOR PREPARING THE SAME
The present invention provides a slip resistant article comprising a substrate and a slip resistant coating applied on the surface of the substrate. The substrate is a ceramic tile substrate. The slip resistant coating is further prepared from a slip resistant solution, and the slip resistant solution comprises the reaction product of the following reaction components: 1-83.5 wt.% of a first silane, based on the total weight of the slip resistant solution as 100 wt.%, the general formula of the first silane being R1 aSi (OR) 4-a-bR2 b, wherein the value of a is 0 to 3; when the value of a is 0, the value of b is 0; when the value of a is 1, the value of b is 0 to 2; when the value of a is 2, the value of b is 0 to 1; when a value of a is 3, the value of b is 0; R represents alkyl group having 1 to 4 carbon atoms; R1 represents hydrocarbyl group with epoxy functional group; and R2 represents alkyl group having 1 to 2 carbon atoms; and 16.5-99 wt.% of a first solvent, based on the total weight of the slip resistant solution as 100 wt.%, the first solvent being water and/or alcohol.
La présente invention concerne un article antidérapant comprenant un substrat et un revêtement antidérapant appliqué à la surface du substrat. Le substrat est un substrat de carreau de céramique. Le revêtement antidérapant est en outre préparé à partir d'une solution antidérapante, et la solution antidérapante comprend le produit de réaction des constituants de réaction suivants : de 1 à 83,5 % en poids d'un premier silane, sur la base du poids total de la solution antidérapante de 100 % en poids, la formule générale du premier silane étant R1 aSi (OU) 4-a-bR2 b, où la valeur de a est de 0 à 3 ; lorsque la valeur de a est 0, la valeur de b est 0 ; lorsque la valeur de a est 1, la valeur de b est de 0 à 2 ; lorsque la valeur de a est 2, la valeur de b est de 0 à 1 ; lorsque la valeur de a est 3, la valeur de b est 0 ; R représente un groupe alkyle ayant 1 à 4 atomes de carbone ; R1 représente un groupe hydrocarbyle à groupe fonctionnel époxy ; et R2 représente un groupe alkyle ayant de 1 à 2 atomes de carbone ; et de 16,5 à 99 % en poids d'un premier solvant, sur la base du poids total de la solution antidérapante de 100 % en poids, le premier solvant étant de l'eau et/ou un alcool.
SLIP RESISTANT ARTICLE AND THE METHOD FOR PREPARING THE SAME
The present invention provides a slip resistant article comprising a substrate and a slip resistant coating applied on the surface of the substrate. The substrate is a ceramic tile substrate. The slip resistant coating is further prepared from a slip resistant solution, and the slip resistant solution comprises the reaction product of the following reaction components: 1-83.5 wt.% of a first silane, based on the total weight of the slip resistant solution as 100 wt.%, the general formula of the first silane being R1 aSi (OR) 4-a-bR2 b, wherein the value of a is 0 to 3; when the value of a is 0, the value of b is 0; when the value of a is 1, the value of b is 0 to 2; when the value of a is 2, the value of b is 0 to 1; when a value of a is 3, the value of b is 0; R represents alkyl group having 1 to 4 carbon atoms; R1 represents hydrocarbyl group with epoxy functional group; and R2 represents alkyl group having 1 to 2 carbon atoms; and 16.5-99 wt.% of a first solvent, based on the total weight of the slip resistant solution as 100 wt.%, the first solvent being water and/or alcohol.
La présente invention concerne un article antidérapant comprenant un substrat et un revêtement antidérapant appliqué à la surface du substrat. Le substrat est un substrat de carreau de céramique. Le revêtement antidérapant est en outre préparé à partir d'une solution antidérapante, et la solution antidérapante comprend le produit de réaction des constituants de réaction suivants : de 1 à 83,5 % en poids d'un premier silane, sur la base du poids total de la solution antidérapante de 100 % en poids, la formule générale du premier silane étant R1 aSi (OU) 4-a-bR2 b, où la valeur de a est de 0 à 3 ; lorsque la valeur de a est 0, la valeur de b est 0 ; lorsque la valeur de a est 1, la valeur de b est de 0 à 2 ; lorsque la valeur de a est 2, la valeur de b est de 0 à 1 ; lorsque la valeur de a est 3, la valeur de b est 0 ; R représente un groupe alkyle ayant 1 à 4 atomes de carbone ; R1 représente un groupe hydrocarbyle à groupe fonctionnel époxy ; et R2 représente un groupe alkyle ayant de 1 à 2 atomes de carbone ; et de 16,5 à 99 % en poids d'un premier solvant, sur la base du poids total de la solution antidérapante de 100 % en poids, le premier solvant étant de l'eau et/ou un alcool.
SLIP RESISTANT ARTICLE AND THE METHOD FOR PREPARING THE SAME
ARTICLE ANTIDÉRAPANT ET SON PROCÉDÉ DE PRÉPARATION
YIN LONG (author) / YU XIN (author) / YU ZHIGANG (author) / YANG LIN (author) / LI WENYAN (author) / JING NAIYONG (author)
2015-09-24
Patent
Electronic Resource
English
WATER RESISTANT CEMENTITIOUS ARTICLE AND METHOD FOR PREPARING SAME
European Patent Office | 2015
|Method for preparing a water resistant cementitious article
European Patent Office | 2021
|