The invention relates to a fritted ball comprising the following crystallised phases, in weight percentages on the basis of the crystallised phases and in relation to a total of 100%: 25% ≤ zirconium, or « Z1 », ≤ 94%; 4% ≤ stabilised zirconium + stabilised hafnia, or « Z2 », ≤ 61 %; monoclinic zirconium + monoclinic hafnia, or « Z3 » ≤ 50%; corindon ≤ 57%; crystallised phases other than Z1, Z2, Z3 and corindon ≤ 10%; and the following chemical composition, in weight percentages on the basis of the oxides and in relation to a total of 100%: 33% ≤ ZrO2 + HfO2, or « Z4 » ≤ 83,4%; HfO2 ≤ 2%; 10,6% < Si2 < 34,7%; Al2O3 ≤ 50%; 0% ≤ Y2O3, or « Z5 »; 0% < CeO2, or « Z6 »; 0,3% ≤ Ce02 + Y2O3 ≤ 19%, provided that (1) CeO2 + 3,76*Y2O3 ≥ 0,128*Z, and (2) CeO2 + 1,3*Y2O3 ≤ 0,318*Z, with Z=Z4+Z5+Z6-(0,67*Z1*(Z4+Z5+Z6)/(0,67*Z1+Z2+Z3)); MgO ≤ 5%; CaO ≤ 2%; as well as oxides other than ZrO2, HfO2, SiO2, Al2O3, MgO, CaO, CeO2 and Y2O3 ≤ 5,0%.
Bille frittée présentant : - les phases cristallisées suivantes, en pourcentages en masse sur la base des phases cristallisées et pour un total de 100% : - 25% ≤ zircon, ou « Z1 », ≤ 94%; - 4% ≤ zircone stabilisée + hafnie stabilisée, ou « Z2 », ≤ 61 %; - zircone monoclinique + hafnie monoclinique, ou « Z3 » ≤ 50%; - corindon ≤ 57%; - phases cristallisées autres que Z1, Z2, Z3 et corindon ≤ 10%; la composition chimique suivante, en pourcentages en masse sur la base des oxydes et pour un total de 100% : 33% ≤ ZrO2 + HfO2, ou « Z4 » ≤ 83,4%; HfO2 ≤ 2%; 10,6% < Si2 < 34,7%; Al2O3 ≤ 50%; 0% ≤ Y2O3, ou « Z5 »; 0% < CeO2, ou « Z6 »; 0,3% ≤ Ce02 + Y2O3 ≤ 19%, pourvu que (1) CeO2 + 3,76*Y2O3 ≥ 0,128*Z, et (2) CeO2 + 1,3*Y2O3 ≤ 0,318*Z, avec Z=Z4+Z5+Z6-(0,67*Z1*(Z4+Z5+Z6)/(0,67*Z1+Z2+Z3)); MgO ≤ 5%; CaO ≤ 2%; oxydes autres que ZrO2, HfO2, SiO2, Al2O3, MgO, CaO, CeO2 et Y2O3 ≤ 5,0%.
The invention relates to a fritted ball comprising the following crystallised phases, in weight percentages on the basis of the crystallised phases and in relation to a total of 100%: 25% ≤ zirconium, or « Z1 », ≤ 94%; 4% ≤ stabilised zirconium + stabilised hafnia, or « Z2 », ≤ 61 %; monoclinic zirconium + monoclinic hafnia, or « Z3 » ≤ 50%; corindon ≤ 57%; crystallised phases other than Z1, Z2, Z3 and corindon ≤ 10%; and the following chemical composition, in weight percentages on the basis of the oxides and in relation to a total of 100%: 33% ≤ ZrO2 + HfO2, or « Z4 » ≤ 83,4%; HfO2 ≤ 2%; 10,6% < Si2 < 34,7%; Al2O3 ≤ 50%; 0% ≤ Y2O3, or « Z5 »; 0% < CeO2, or « Z6 »; 0,3% ≤ Ce02 + Y2O3 ≤ 19%, provided that (1) CeO2 + 3,76*Y2O3 ≥ 0,128*Z, and (2) CeO2 + 1,3*Y2O3 ≤ 0,318*Z, with Z=Z4+Z5+Z6-(0,67*Z1*(Z4+Z5+Z6)/(0,67*Z1+Z2+Z3)); MgO ≤ 5%; CaO ≤ 2%; as well as oxides other than ZrO2, HfO2, SiO2, Al2O3, MgO, CaO, CeO2 and Y2O3 ≤ 5,0%.
Bille frittée présentant : - les phases cristallisées suivantes, en pourcentages en masse sur la base des phases cristallisées et pour un total de 100% : - 25% ≤ zircon, ou « Z1 », ≤ 94%; - 4% ≤ zircone stabilisée + hafnie stabilisée, ou « Z2 », ≤ 61 %; - zircone monoclinique + hafnie monoclinique, ou « Z3 » ≤ 50%; - corindon ≤ 57%; - phases cristallisées autres que Z1, Z2, Z3 et corindon ≤ 10%; la composition chimique suivante, en pourcentages en masse sur la base des oxydes et pour un total de 100% : 33% ≤ ZrO2 + HfO2, ou « Z4 » ≤ 83,4%; HfO2 ≤ 2%; 10,6% < Si2 < 34,7%; Al2O3 ≤ 50%; 0% ≤ Y2O3, ou « Z5 »; 0% < CeO2, ou « Z6 »; 0,3% ≤ Ce02 + Y2O3 ≤ 19%, pourvu que (1) CeO2 + 3,76*Y2O3 ≥ 0,128*Z, et (2) CeO2 + 1,3*Y2O3 ≤ 0,318*Z, avec Z=Z4+Z5+Z6-(0,67*Z1*(Z4+Z5+Z6)/(0,67*Z1+Z2+Z3)); MgO ≤ 5%; CaO ≤ 2%; oxydes autres que ZrO2, HfO2, SiO2, Al2O3, MgO, CaO, CeO2 et Y2O3 ≤ 5,0%.
BILLES FRITTEES DE ZIRCON
FRITTED ZIRCONIUM BALLS
NONNET EMMANUEL (author)
2019-01-24
Patent
Electronic Resource
French