UTILISATION D'UNE COMPOSITION À BASE DE LIANT HYDRAULIQUE DANS LE CADRE D'UN PROCÉDÉ D'INERTAGE DE SOL POLLUÉ
The invention relates to the use of a composition comprising: 40 to 99% of a sulfoaluminous clinker containing, as a phasic composition, in relation to the total weight of the clinker: 5 to 80% of an optionally iron-doped calcium sulfoaluminate phase of formula C4AxFy$z, where x varies from 2 to 3, y varies from 0 to 0.5 and z varies from 0.8 to 1.2; 0 to 25% of a calcium aluminoferrite phase of a composition of general formula C6Ax'Fy', where x' varies from 0 to 1.5 and y' varies from 0.5 to 3; and 10 to 70% of a C2S belite phase; and 1 to 60% of lime; in a method for inerting polluted soil. The invention also relates to a composition for inerting polluted soil, comprising: 70 to 98% of a sulfoaluminous clinker containing, as a phasic composition, in relation to the total weight of the clinker: 5 to 60 % of an optionally iron-doped calcium sulfoaluminate phase of formula C4AxFy$z, where x varies from 2 to 3, y varies from 0 to 0.5 and z varies from 0.8 to 1.2; 0 to 25% of a calcium aluminoferrite phase of a composition of general formula C6Ax'Fy', where x' varies from 0 to 1.5 and y' varies from 0.5 to 3; and 20 to 70% of a C2S belite phase; and 2 to 30% of lime.
La présente invention a pour objet l'utilisation d'une composition comprenant: de 40% à 99% d'un clinker sulfoalumineux comprenant comme composition phasique, par rapport au poids total du clinker: de 5 à 80 % de phase sulfoaluminate de calcium éventuellement dopée en fer correspondant à la formule C4AxFy$z dans laquelle x varie de 2 à 3; y varie de 0 à 0.5; et et z varie de 0.8 à 1.2; de 0 à 25 % de phase aluminoferrite calcique d'une composition correspondant à la formule générale C 6 A x' F y' x' varie de 0 à 1.5; et y' varie de 0.5 à 3; et de 10 à 70% de phase bélite C 2 S; et de 1% à 60% de chaux; dans un procédé d'inertage de sol pollué. La présente invention a également pour objet unecomposition pour inertage de sol pollué comprenant: de 70% à 98% d'un clinker sulfoalumineux comprenant comme composition phasique, par rapport au poids total du clinker: de 5 à 60 % de phase sulfoaluminate de calcium éventuellement dopée en fer correspondant à la formule C4AxFy$z dans laquelle x varie de 2 à 3; y varie de 0 à 0.5; et et z varie de 0.8 à 1.2; de 0 à 25% de phase aluminoferrite calcique d'une composition correspondant à la formule générale C 6 A x' F y' x' varie de 0 à 1.5; et y' varie de 0.5 à 3; et de 20 à 70% de phase bélite C 2 S; et de 2% à 30% de chaux.
UTILISATION D'UNE COMPOSITION À BASE DE LIANT HYDRAULIQUE DANS LE CADRE D'UN PROCÉDÉ D'INERTAGE DE SOL POLLUÉ
The invention relates to the use of a composition comprising: 40 to 99% of a sulfoaluminous clinker containing, as a phasic composition, in relation to the total weight of the clinker: 5 to 80% of an optionally iron-doped calcium sulfoaluminate phase of formula C4AxFy$z, where x varies from 2 to 3, y varies from 0 to 0.5 and z varies from 0.8 to 1.2; 0 to 25% of a calcium aluminoferrite phase of a composition of general formula C6Ax'Fy', where x' varies from 0 to 1.5 and y' varies from 0.5 to 3; and 10 to 70% of a C2S belite phase; and 1 to 60% of lime; in a method for inerting polluted soil. The invention also relates to a composition for inerting polluted soil, comprising: 70 to 98% of a sulfoaluminous clinker containing, as a phasic composition, in relation to the total weight of the clinker: 5 to 60 % of an optionally iron-doped calcium sulfoaluminate phase of formula C4AxFy$z, where x varies from 2 to 3, y varies from 0 to 0.5 and z varies from 0.8 to 1.2; 0 to 25% of a calcium aluminoferrite phase of a composition of general formula C6Ax'Fy', where x' varies from 0 to 1.5 and y' varies from 0.5 to 3; and 20 to 70% of a C2S belite phase; and 2 to 30% of lime.
La présente invention a pour objet l'utilisation d'une composition comprenant: de 40% à 99% d'un clinker sulfoalumineux comprenant comme composition phasique, par rapport au poids total du clinker: de 5 à 80 % de phase sulfoaluminate de calcium éventuellement dopée en fer correspondant à la formule C4AxFy$z dans laquelle x varie de 2 à 3; y varie de 0 à 0.5; et et z varie de 0.8 à 1.2; de 0 à 25 % de phase aluminoferrite calcique d'une composition correspondant à la formule générale C 6 A x' F y' x' varie de 0 à 1.5; et y' varie de 0.5 à 3; et de 10 à 70% de phase bélite C 2 S; et de 1% à 60% de chaux; dans un procédé d'inertage de sol pollué. La présente invention a également pour objet unecomposition pour inertage de sol pollué comprenant: de 70% à 98% d'un clinker sulfoalumineux comprenant comme composition phasique, par rapport au poids total du clinker: de 5 à 60 % de phase sulfoaluminate de calcium éventuellement dopée en fer correspondant à la formule C4AxFy$z dans laquelle x varie de 2 à 3; y varie de 0 à 0.5; et et z varie de 0.8 à 1.2; de 0 à 25% de phase aluminoferrite calcique d'une composition correspondant à la formule générale C 6 A x' F y' x' varie de 0 à 1.5; et y' varie de 0.5 à 3; et de 20 à 70% de phase bélite C 2 S; et de 2% à 30% de chaux.
UTILISATION D'UNE COMPOSITION À BASE DE LIANT HYDRAULIQUE DANS LE CADRE D'UN PROCÉDÉ D'INERTAGE DE SOL POLLUÉ
USE OF A HYDRAULIC BINDER COMPOSITION IN A METHOD FOR INERTING POLLUTED SOIL
JACOB YVAN-PIERRE (author) / BARNES-DAVIN LAURY (author) / NOWALSKI VIRGINIE (author)
2019-08-29
Patent
Electronic Resource
French
European Patent Office | 2020
|PROCÉDÉ DE TRAITEMENT DE SOL POLLUÉ PAR UN LIANT HYDRAULIQUE À PHASE MAYENITE
European Patent Office | 2020
|PROCEDE DE TRAITEMENT DE SOL POLLUE PAR UN LIANT HYDRAULIQUE A PHASE MAYENITE
European Patent Office | 2020
|PROCEDE DE TRAITEMENT DE SOL POLLUE PAR UN LIANT HYDRAULIQUE A PHASE MAYENITE
European Patent Office | 2018
|PROCÉDÉ DE TRAITEMENT DE SOL POLLUÉ PAR UN LIANT HYDRAULIQUE À PHASE MAYENITE
European Patent Office | 2018
|