A platform for research: civil engineering, architecture and urbanism
POWDER AND SOLID COMPOSITION
A powder that satisfies requirement 1 and requirement 2. Requirement 1: At at least one temperature T1 in the range of -200℃–1,200℃, |dA(T)/dT| is at least 10 ppm/℃, A being (the a-axis (short-axis) lattice constant of the crystals of the powder)/(the c-axis (long-axis) lattice constant of the crystals of the powder), the lattice constants being obtained by x-ray diffraction measurement of the powder. Requirement 2: The particle diameter D50 at which cumulative frequency is 50%, the particle diameter D10 at which cumulative frequency is 10%, and the particle diameter D90 at which cumulative frequency is 90% on a volume-based cumulative particle diameter distribution curve obtained by laser diffraction/scattering satisfy conditions (I) and (II). (I) D10/D50 is 0.05–0.45. (II) D90 is 0.5–70 μm.
L'invention concerne une poudre qui satisfait l'exigence 1 et l'exigence 2. Exigence 1 : À au moins une température T1 dans la plage de -200°C à 1 200°C, |dA(T)/dT| est d'au moins 10 ppm/°C, A étant (constante de réseau de l'axe a (axe court) des cristaux de la poudre)/(constante de réseau de l'axe c (axe long) des cristaux de la poudre), les constantes de réseau étant obtenues par mesure de diffraction des rayons X de la poudre. Exigence 2 : Le diamètre de particule D50 auquel la fréquence cumulative est de 50 %, le diamètre de particule D10 auquel la fréquence cumulative est de 10 %, et le diamètre de particule D90 auquel la fréquence cumulative est de 90 % sur une courbe de distribution de diamètre de particule cumulatif basée sur le volume obtenue par diffraction/diffusion laser satisfont des conditions (I) et (II). (I) D10/D50 est de 0,05 à 0,45. (II) D90 est de 0,5 à 70 μm.
粉体は、要件1及び要件2を満たす。 要件1:-200℃~1200℃における少なくとも一つの温度T1で|dA(T)/dT|が10ppm/℃以上を満たす。 Aは(粉体中の結晶のa軸(短軸)の格子定数)/(粉体中の結晶のc軸(長軸)の格子定数)であり、各格子定数は前記粉体のX線回折測定から得られる。 要件2:レーザー回折散乱法により得られる体積基準累積粒子径分布曲線における、累積頻度が50%となる粒子径D50、累積頻度が10%となる粒子径D10、及び累積頻度が90%となる粒子径D90が、条件(I)及び(II)を満たす。 (I)D10/D50が0.05以上0.45以下である。 (II)D90が0.5μm以上70μm以下である。
POWDER AND SOLID COMPOSITION
A powder that satisfies requirement 1 and requirement 2. Requirement 1: At at least one temperature T1 in the range of -200℃–1,200℃, |dA(T)/dT| is at least 10 ppm/℃, A being (the a-axis (short-axis) lattice constant of the crystals of the powder)/(the c-axis (long-axis) lattice constant of the crystals of the powder), the lattice constants being obtained by x-ray diffraction measurement of the powder. Requirement 2: The particle diameter D50 at which cumulative frequency is 50%, the particle diameter D10 at which cumulative frequency is 10%, and the particle diameter D90 at which cumulative frequency is 90% on a volume-based cumulative particle diameter distribution curve obtained by laser diffraction/scattering satisfy conditions (I) and (II). (I) D10/D50 is 0.05–0.45. (II) D90 is 0.5–70 μm.
L'invention concerne une poudre qui satisfait l'exigence 1 et l'exigence 2. Exigence 1 : À au moins une température T1 dans la plage de -200°C à 1 200°C, |dA(T)/dT| est d'au moins 10 ppm/°C, A étant (constante de réseau de l'axe a (axe court) des cristaux de la poudre)/(constante de réseau de l'axe c (axe long) des cristaux de la poudre), les constantes de réseau étant obtenues par mesure de diffraction des rayons X de la poudre. Exigence 2 : Le diamètre de particule D50 auquel la fréquence cumulative est de 50 %, le diamètre de particule D10 auquel la fréquence cumulative est de 10 %, et le diamètre de particule D90 auquel la fréquence cumulative est de 90 % sur une courbe de distribution de diamètre de particule cumulatif basée sur le volume obtenue par diffraction/diffusion laser satisfont des conditions (I) et (II). (I) D10/D50 est de 0,05 à 0,45. (II) D90 est de 0,5 à 70 μm.
粉体は、要件1及び要件2を満たす。 要件1:-200℃~1200℃における少なくとも一つの温度T1で|dA(T)/dT|が10ppm/℃以上を満たす。 Aは(粉体中の結晶のa軸(短軸)の格子定数)/(粉体中の結晶のc軸(長軸)の格子定数)であり、各格子定数は前記粉体のX線回折測定から得られる。 要件2:レーザー回折散乱法により得られる体積基準累積粒子径分布曲線における、累積頻度が50%となる粒子径D50、累積頻度が10%となる粒子径D10、及び累積頻度が90%となる粒子径D90が、条件(I)及び(II)を満たす。 (I)D10/D50が0.05以上0.45以下である。 (II)D90が0.5μm以上70μm以下である。
POWDER AND SOLID COMPOSITION
POUDRE ET COMPOSITION SOLIDE
粉体及び固体組成物
DOI ATSUNORI (author) / SHIMANO SATOSHI (author)
2021-01-21
Patent
Electronic Resource
Japanese
TITANIUM OXIDE, POWDER, POWDER COMPOSITION, SOLID COMPOSITION, LIQUID COMPOSITION, AND MOLDED BODY
European Patent Office | 2021
|TITANIUM OXIDE, POWDER, POWDER COMPOSITION, SOLID COMPOSITION, LIQUID COMPOSITION, AND MOLDED BODY
European Patent Office | 2021
|PARTICLE GROUP, POWDER COMPOSITION, SOLID COMPOSITION, LIQUID COMPOSITION, AND COMPACT
European Patent Office | 2023
|