A platform for research: civil engineering, architecture and urbanism
MILLING TOOLS FROM NEW WURTZITE BORON NITRIDE (W-BN) SUPERHARD MATERIAL
Systems and methods include a computer-implemented method can be used to make milling tools from new wurtzite boron nitride (w-BN) superhard material. An ultra-high-pressure, high-temperature operation is performed on pure w-BN powder to synthesize w-BN and cubic boron nitride (c-BN) compact having a first size greater than particles of the pure w-BN powder. The ultra-high-pressure, high-temperature operation includes pressurizing the w-BN powder to a pressure of approximately 20 Gigapascal, heating the w-BN powder at a heating rate of 100° C/minute and cooling the w-BN powder at a cooling rate of 50° C/minute. The compact is cut to a second size smaller than the first size using laser cutting tools. The cut compact is turbulently mixed with additives in a mixer under vacuum. The cut compact mixed with the additives is thermally sprayed onto a tool substrate to form the tool.
La présente invention concerne des systèmes et des procédés qui comprennent un procédé mis en œuvre par ordinateur qui peut être utilisé pour fabriquer des outils de broyage à partir d'un nouveau matériau extradur de nitrure de bore wurtzite (w-BN). Une opération à ultra-haute pression et à haute température est effectuée sur de la poudre de w-BN pur pour synthétiser un comprimé de w-BN et de nitrure de bore cubique (c-BN) présentant une première taille supérieure à celle des particules de la poudre de w-BN pur. L'opération à ultra-haute pression et à haute température consiste à mettre sous pression la poudre de w-BN à une pression d'environ 20 Gigapascals, à chauffer la poudre de w-BN à une vitesse de chauffage de 100 °C/minute et à refroidir la poudre de w-BN à une vitesse de refroidissement de 50 °C/minute. Le comprimé est découpé à une seconde taille plus petite que la première taille à l'aide d'outils de découpe au laser. Le comprimé découpé est mélangé de manière turbulente à des additifs dans un mélangeur sous vide. Le comprimé découpé mélangé aux additifs est projeté thermiquement sur un substrat d'outil pour former l'outil.
MILLING TOOLS FROM NEW WURTZITE BORON NITRIDE (W-BN) SUPERHARD MATERIAL
Systems and methods include a computer-implemented method can be used to make milling tools from new wurtzite boron nitride (w-BN) superhard material. An ultra-high-pressure, high-temperature operation is performed on pure w-BN powder to synthesize w-BN and cubic boron nitride (c-BN) compact having a first size greater than particles of the pure w-BN powder. The ultra-high-pressure, high-temperature operation includes pressurizing the w-BN powder to a pressure of approximately 20 Gigapascal, heating the w-BN powder at a heating rate of 100° C/minute and cooling the w-BN powder at a cooling rate of 50° C/minute. The compact is cut to a second size smaller than the first size using laser cutting tools. The cut compact is turbulently mixed with additives in a mixer under vacuum. The cut compact mixed with the additives is thermally sprayed onto a tool substrate to form the tool.
La présente invention concerne des systèmes et des procédés qui comprennent un procédé mis en œuvre par ordinateur qui peut être utilisé pour fabriquer des outils de broyage à partir d'un nouveau matériau extradur de nitrure de bore wurtzite (w-BN). Une opération à ultra-haute pression et à haute température est effectuée sur de la poudre de w-BN pur pour synthétiser un comprimé de w-BN et de nitrure de bore cubique (c-BN) présentant une première taille supérieure à celle des particules de la poudre de w-BN pur. L'opération à ultra-haute pression et à haute température consiste à mettre sous pression la poudre de w-BN à une pression d'environ 20 Gigapascals, à chauffer la poudre de w-BN à une vitesse de chauffage de 100 °C/minute et à refroidir la poudre de w-BN à une vitesse de refroidissement de 50 °C/minute. Le comprimé est découpé à une seconde taille plus petite que la première taille à l'aide d'outils de découpe au laser. Le comprimé découpé est mélangé de manière turbulente à des additifs dans un mélangeur sous vide. Le comprimé découpé mélangé aux additifs est projeté thermiquement sur un substrat d'outil pour former l'outil.
MILLING TOOLS FROM NEW WURTZITE BORON NITRIDE (W-BN) SUPERHARD MATERIAL
OUTILS DE BROYAGE À PARTIR D'UN NOUVEAU MATÉRIAU EXTRADUR DE NITRURE DE BORE WURTZITE (W-BN)
HE DUANWEI (author) / ZHAN GUODONG (author) / BADRAN MOHAMMED (author) / MOELLENDICK TIMOTHY E (author)
2021-02-04
Patent
Electronic Resource
English
MILLING TOOLS FROM NEW WURTZITE BORON NITRIDE (W-BN) SUPERHARD MATERIAL
European Patent Office | 2021
|BINDERS FOR MILLING TOOLS USING WURTZITE BORON NITRIDE (W-BN) SUPERHARD MATERIAL
European Patent Office | 2021
|European Patent Office | 2022
|