CEMENT CLINKER, CEMENT COMPOSITION, AND CEMENT CLINKER PRODUCTION METHOD
Provided are a cement clinker and a cement composition which can be reduced in heat of hydration and are excellent in short term strength development. A cement clinker in which the proportion of C3S determined by Bogue calculation is 50-75% by mass, the proportion of C2S determined by Bogue calculation is 5-25% by mass, and the total proportion of C3A and C4AF determined by Bogue calculation is 15-22% by mass, and which contains MgO, TiO2, MnO and ZnO, and satisfies the following formula (1). (1): CMg-C3A×CTi-C3A×CMn-C3A×CZn-C3A≤0.0010 (in the formula (1), CMg-C3A represents the MgO content (% by mass) in C3A, CTi-C3A represents the TiO2 content (% by mass) in C3A, CMn-C3A represents the MnO content (% by mass) in C3A, and CZn-C3A represents the ZnO content (% by mass) in C3A).
L'invention concerne une scorie de ciment et une composition de ciment qui peuvent être réduites en termes de chaleur d'hydratation et qui sont excellents en termes de développement de résistance à court terme. L'invention concerne une scorie de ciment dans laquelle la proportion de C3S déterminée par le calcul de Bogue est de 50 à 75 % en masse, la proportion de C2S déterminée par le calcul de Bogue est de 5 à 25 % en masse, et la proportion totale de C3A et C4AF déterminée par le calcul de Bogue est de 15 à 22 % en masse, et qui contient des MgO, TiO2, MnO et ZnO, et satisfait à la formule (1) suivante. (1) : CMg-C3A×CTi-C3A×CMn-C3A×CZn-C3A ≤ 0,0010 (dans la formule (1), CMg-C3A représente la teneur en MgO (% en masse) dans C3A, CTi-C3A représente la teneur en TiO2 (% en masse) dans C3A, CMn-C3A représente la teneur en MnO (% en masse) dans C3A, et CZn-C3A représente la teneur en ZnO (% en masse) dans C3A).
水和熱を低減させることができるとともに、短期強度発現性に優れるセメントクリンカ及びセメント組成物を提供する。ボーグ式で算出されたC3Sの割合が50~75質量%であり、ボーグ式で算出されたC2Sの割合が5~25質量%であり、ボーグ式で算出されたC3A及びC4AFの合計の割合が15~22質量%であり、MgO、TiO2、MnO及びZnOを含み、下記式(1)を満たす、セメントクリンカ。 CMg-C3A×CTi-C3A×CMn-C3A×CZn-C3A≦0.0010 ・・・(1) 式(1)中、 CMg-C3Aは、C3A中のMgOの含有率(質量%)を表し、 CTi-C3Aは、C3A中のTiO2の含有率(質量%)を表し、 CMn-C3Aは、C3A中のMnOの含有率(質量%)を表し、 CZn-C3Aは、C3A中のZnOの含有率(質量%)を表す。
CEMENT CLINKER, CEMENT COMPOSITION, AND CEMENT CLINKER PRODUCTION METHOD
Provided are a cement clinker and a cement composition which can be reduced in heat of hydration and are excellent in short term strength development. A cement clinker in which the proportion of C3S determined by Bogue calculation is 50-75% by mass, the proportion of C2S determined by Bogue calculation is 5-25% by mass, and the total proportion of C3A and C4AF determined by Bogue calculation is 15-22% by mass, and which contains MgO, TiO2, MnO and ZnO, and satisfies the following formula (1). (1): CMg-C3A×CTi-C3A×CMn-C3A×CZn-C3A≤0.0010 (in the formula (1), CMg-C3A represents the MgO content (% by mass) in C3A, CTi-C3A represents the TiO2 content (% by mass) in C3A, CMn-C3A represents the MnO content (% by mass) in C3A, and CZn-C3A represents the ZnO content (% by mass) in C3A).
L'invention concerne une scorie de ciment et une composition de ciment qui peuvent être réduites en termes de chaleur d'hydratation et qui sont excellents en termes de développement de résistance à court terme. L'invention concerne une scorie de ciment dans laquelle la proportion de C3S déterminée par le calcul de Bogue est de 50 à 75 % en masse, la proportion de C2S déterminée par le calcul de Bogue est de 5 à 25 % en masse, et la proportion totale de C3A et C4AF déterminée par le calcul de Bogue est de 15 à 22 % en masse, et qui contient des MgO, TiO2, MnO et ZnO, et satisfait à la formule (1) suivante. (1) : CMg-C3A×CTi-C3A×CMn-C3A×CZn-C3A ≤ 0,0010 (dans la formule (1), CMg-C3A représente la teneur en MgO (% en masse) dans C3A, CTi-C3A représente la teneur en TiO2 (% en masse) dans C3A, CMn-C3A représente la teneur en MnO (% en masse) dans C3A, et CZn-C3A représente la teneur en ZnO (% en masse) dans C3A).
水和熱を低減させることができるとともに、短期強度発現性に優れるセメントクリンカ及びセメント組成物を提供する。ボーグ式で算出されたC3Sの割合が50~75質量%であり、ボーグ式で算出されたC2Sの割合が5~25質量%であり、ボーグ式で算出されたC3A及びC4AFの合計の割合が15~22質量%であり、MgO、TiO2、MnO及びZnOを含み、下記式(1)を満たす、セメントクリンカ。 CMg-C3A×CTi-C3A×CMn-C3A×CZn-C3A≦0.0010 ・・・(1) 式(1)中、 CMg-C3Aは、C3A中のMgOの含有率(質量%)を表し、 CTi-C3Aは、C3A中のTiO2の含有率(質量%)を表し、 CMn-C3Aは、C3A中のMnOの含有率(質量%)を表し、 CZn-C3Aは、C3A中のZnOの含有率(質量%)を表す。
CEMENT CLINKER, CEMENT COMPOSITION, AND CEMENT CLINKER PRODUCTION METHOD
SCORIE DE CIMENT, COMPOSITION DE CIMENT, ET PROCÉDÉ DE PRODUCTION DE SCORIE DE CIMENT
セメントクリンカ及びセメント組成物、並びにセメントクリンカの製造方法
SHIMIZU JUN (author) / YAMADA YOH (author) / YAMAGATA KYOSUKE (author) / SATO TOMOKI (author) / NASU HIDEYUKI (author)
2021-09-30
Patent
Electronic Resource
Japanese
IPC:
C04B
Kalk
,
LIME
Cement clinker, cement composition, and cement clinker production method
European Patent Office | 2022
|CEMENT CLINKER, METHOD OF PRODUCING CEMENT CLINKER, AND CEMENT COMPOSITION
European Patent Office | 2023
|PORTLAND CEMENT CLINKER, CEMENT COMPOSITION AND METHOD FOR PRODUCING PORTLAND CEMENT CLINKER
European Patent Office | 2024
|CEMENT CLINKER PRODUCTION SYSTEM AND CEMENT CLINKER PRODUCTION METHOD
European Patent Office | 2024
|