Disclosed in the present invention are a carbon fiber gain ceramic atomization core and a preparation method therefor. The carbon fiber gain ceramic atomization core comprises the following raw materials in parts by weight: 30-70 parts of ceramic powder, 1-10 parts of carbon fiber, 10-50 parts of sintering aid, and 0-30 parts of pore-forming agent. According to the carbon fiber gain ceramic atomization core, a carbon fiber is added, such that the atomization core has columnar pore channels which are similar to straight pore channels where cotton core fibers are accumulated, the oil guiding and locking capacity of the atomization core is improved, and the atomization effect and taste of the atomization core are improved; and the carbon fiber can also form bridging around the pore channels, such that a toughening effect is achieved, and the strength of the atomization core is improved.
Sont divulgués dans la présente invention un noyau d'atomisation en céramique à gain en fibre de carbone et son procédé de préparation. Le noyau d'atomisation en céramique à gain en fibre de carbone comprend les matières premières suivantes en parties en poids : 30 à 70 parties de poudre céramique, 1 à 10 parties de fibre de carbone, 10 à 50 parties d'adjuvant de frittage et 0 à 30 parties d'agent porogène. Selon le noyau d'atomisation en céramique à gain en fibre de carbone, une fibre de carbone est ajoutée, de telle sorte que le noyau d'atomisation présente des canaux à pores en colonnes qui sont similaires à des canaux à pores droits où des fibres de noyau de coton sont accumulées, la capacité de guidage et de verrouillage d'huile du noyau d'atomisation est améliorée, et l'effet d'atomisation et le goût du noyau d'atomisation sont améliorés ; et la fibre de carbone peut également former un pont autour des canaux à pores, de telle sorte qu'un effet de renforcement est obtenu et que la résistance du noyau d'atomisation est améliorée.
本发明公开了一种碳纤维增益陶瓷雾化芯及其制备方法,碳纤维增益陶瓷雾化芯包括原料及其质量份数如下:陶瓷粉体30-70份、碳纤维1-10份、助烧剂10-50份以及造孔剂0-30份。本发明的碳纤维增益陶瓷雾化芯,通过碳纤维的加入,使雾化芯具有柱状孔道,类似于棉芯纤维堆积的直通式孔道,提高雾化芯的导油和锁油能力,提高雾化芯的雾化效果及口感;碳纤维还可在孔道周围形成架接,具有增韧作用,提高雾化芯的强度。
Disclosed in the present invention are a carbon fiber gain ceramic atomization core and a preparation method therefor. The carbon fiber gain ceramic atomization core comprises the following raw materials in parts by weight: 30-70 parts of ceramic powder, 1-10 parts of carbon fiber, 10-50 parts of sintering aid, and 0-30 parts of pore-forming agent. According to the carbon fiber gain ceramic atomization core, a carbon fiber is added, such that the atomization core has columnar pore channels which are similar to straight pore channels where cotton core fibers are accumulated, the oil guiding and locking capacity of the atomization core is improved, and the atomization effect and taste of the atomization core are improved; and the carbon fiber can also form bridging around the pore channels, such that a toughening effect is achieved, and the strength of the atomization core is improved.
Sont divulgués dans la présente invention un noyau d'atomisation en céramique à gain en fibre de carbone et son procédé de préparation. Le noyau d'atomisation en céramique à gain en fibre de carbone comprend les matières premières suivantes en parties en poids : 30 à 70 parties de poudre céramique, 1 à 10 parties de fibre de carbone, 10 à 50 parties d'adjuvant de frittage et 0 à 30 parties d'agent porogène. Selon le noyau d'atomisation en céramique à gain en fibre de carbone, une fibre de carbone est ajoutée, de telle sorte que le noyau d'atomisation présente des canaux à pores en colonnes qui sont similaires à des canaux à pores droits où des fibres de noyau de coton sont accumulées, la capacité de guidage et de verrouillage d'huile du noyau d'atomisation est améliorée, et l'effet d'atomisation et le goût du noyau d'atomisation sont améliorés ; et la fibre de carbone peut également former un pont autour des canaux à pores, de telle sorte qu'un effet de renforcement est obtenu et que la résistance du noyau d'atomisation est améliorée.
本发明公开了一种碳纤维增益陶瓷雾化芯及其制备方法,碳纤维增益陶瓷雾化芯包括原料及其质量份数如下:陶瓷粉体30-70份、碳纤维1-10份、助烧剂10-50份以及造孔剂0-30份。本发明的碳纤维增益陶瓷雾化芯,通过碳纤维的加入,使雾化芯具有柱状孔道,类似于棉芯纤维堆积的直通式孔道,提高雾化芯的导油和锁油能力,提高雾化芯的雾化效果及口感;碳纤维还可在孔道周围形成架接,具有增韧作用,提高雾化芯的强度。
CARBON FIBER GAIN CERAMIC ATOMIZATION CORE AND PREPARATION METHOD THEREFOR
NOYAU D'ATOMISATION EN CÉRAMIQUE À GAIN EN FIBRE DE CARBONE ET SON PROCÉDÉ DE PRÉPARATION
碳纤维增益陶瓷雾化芯及其制备方法
CHEN PING (author)
2023-03-02
Patent
Electronic Resource
Chinese
CARBON FIBER GAIN CERAMIC ATOMIZATION CORE AND PREPARATION METHOD THEREFOR
European Patent Office | 2023
|MICROPOROUS CERAMIC ATOMIZATION CORE AND PREPARATION METHOD THEREFOR
European Patent Office | 2024
|MICROPOROUS CERAMIC ATOMIZATION CORE AND PREPARATION METHOD THEREFOR
European Patent Office | 2023
|HUMIDITY-SENSITIVE POROUS CERAMIC, ATOMIZATION CORE AND PREPARATION METHOD THEREFOR
European Patent Office | 2022
|CERAMIC ATOMIZATION CORE, AND PREPARATION METHOD THEREFOR AND USE THEREOF
European Patent Office | 2023
|