A platform for research: civil engineering, architecture and urbanism
LOW-TEMPERATURE CO-FIRED CERAMIC POWDER, PREPARATION METHOD THEREFOR AND APPLICATION THEREOF
A low-temperature co-fired ceramic powder, a preparation method therefor and an application thereof. The components of the raw materials of the low-temperature co-fired ceramic powder comprise: xRO-yM2O3-zXO2, wherein R is at least one of Mg, Ca, Ba, Zn, Cu, and Pb, M is at least one of B, Al, Co, In, Bi, Nd, Sm, and La, X is at least one of Si, Ge, Sn, Ti, Zr, and Hf, 0≤x≤85 wt%, 15 wt%≤y≦90 wt%, 10 wt%≤z≤85 wt%, and x+y+z=1. The low-temperature co-fired ceramic powder is obtained by performing high-temperature melting, quenching treatment, and recrystallization treatment. The high-temperature melting temperature is 1200-1600°C, and the recrystallization temperature is 500-900°C.
Une poudre de céramique co-cuite à basse température, son procédé de préparation et son application. Les constituants des matières premières de la poudre de céramique co-cuite à basse température comprennent : xRO-yM2O3-zXO2, R étant au moins l'un de Mg, Ca, Ba, Zn, Cu, et Pb, M étant au moins l'un de B, Al, Co, In, Bi, Nd, Sm, et La, X étant au moins l'un de Si, Ge, Sn, Ti, Zr, et Hf, 0 ≤ x ≤ 85 % en pds, 15 % en pds ≤ y ≦ 90 % en pds, 10 % en pds ≤ z ≤ 85 % en pds, et x + y + z = 1. La poudre de céramique co-cuite à basse température est obtenue en effectuant une fusion à haute température, un traitement de trempe, et un traitement de recristallisation. La température de fusion à haute température est de 1 200 à 1 600 °C, et la température de recristallisation est de 500 à 900 °C.
一种低温共烧陶瓷粉体及其制备方法和应用,所述低温共烧陶瓷粉体的原料组成为xRO-yM 2O 3-zXO 2;其中,R为Mg、Ca、Ba、Zn、Cu、Pb中的至少一种,M为B、Al、Co、In、Bi、Nd、Sm、La中的至少一种,X为Si、Ge、Sn、Ti、Zr、Hf中的至少一种,0≤x≤85wt%,15wt%≤y≤90wt%,10wt%≤z≤85wt%,且x+y+z=1;所述低温共烧陶瓷粉体是经过高温熔融、淬火处理和再析晶处理得到,所述高温熔融的温度为1200℃~1600℃,所述再析晶处理的温度为500~900℃。
LOW-TEMPERATURE CO-FIRED CERAMIC POWDER, PREPARATION METHOD THEREFOR AND APPLICATION THEREOF
A low-temperature co-fired ceramic powder, a preparation method therefor and an application thereof. The components of the raw materials of the low-temperature co-fired ceramic powder comprise: xRO-yM2O3-zXO2, wherein R is at least one of Mg, Ca, Ba, Zn, Cu, and Pb, M is at least one of B, Al, Co, In, Bi, Nd, Sm, and La, X is at least one of Si, Ge, Sn, Ti, Zr, and Hf, 0≤x≤85 wt%, 15 wt%≤y≦90 wt%, 10 wt%≤z≤85 wt%, and x+y+z=1. The low-temperature co-fired ceramic powder is obtained by performing high-temperature melting, quenching treatment, and recrystallization treatment. The high-temperature melting temperature is 1200-1600°C, and the recrystallization temperature is 500-900°C.
Une poudre de céramique co-cuite à basse température, son procédé de préparation et son application. Les constituants des matières premières de la poudre de céramique co-cuite à basse température comprennent : xRO-yM2O3-zXO2, R étant au moins l'un de Mg, Ca, Ba, Zn, Cu, et Pb, M étant au moins l'un de B, Al, Co, In, Bi, Nd, Sm, et La, X étant au moins l'un de Si, Ge, Sn, Ti, Zr, et Hf, 0 ≤ x ≤ 85 % en pds, 15 % en pds ≤ y ≦ 90 % en pds, 10 % en pds ≤ z ≤ 85 % en pds, et x + y + z = 1. La poudre de céramique co-cuite à basse température est obtenue en effectuant une fusion à haute température, un traitement de trempe, et un traitement de recristallisation. La température de fusion à haute température est de 1 200 à 1 600 °C, et la température de recristallisation est de 500 à 900 °C.
一种低温共烧陶瓷粉体及其制备方法和应用,所述低温共烧陶瓷粉体的原料组成为xRO-yM 2O 3-zXO 2;其中,R为Mg、Ca、Ba、Zn、Cu、Pb中的至少一种,M为B、Al、Co、In、Bi、Nd、Sm、La中的至少一种,X为Si、Ge、Sn、Ti、Zr、Hf中的至少一种,0≤x≤85wt%,15wt%≤y≤90wt%,10wt%≤z≤85wt%,且x+y+z=1;所述低温共烧陶瓷粉体是经过高温熔融、淬火处理和再析晶处理得到,所述高温熔融的温度为1200℃~1600℃,所述再析晶处理的温度为500~900℃。
LOW-TEMPERATURE CO-FIRED CERAMIC POWDER, PREPARATION METHOD THEREFOR AND APPLICATION THEREOF
POUDRE DE CÉRAMIQUE CO-CUITE À BASSE TEMPÉRATURE, SON PROCÉDÉ DE PRÉPARATION ET SON APPLICATION
一种低温共烧陶瓷粉体及其制备方法和应用
LIU FENG (author) / LIANG YONGYUAN (author) / LV TAN (author) / JIN HANGFENG (author)
2023-03-23
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
LOW-TEMPERATURE CO-FIRED CERAMIC POWDER, PREPARATION METHOD THEREFOR AND APPLICATION THEREOF
European Patent Office | 2024
|LOW-TEMPERATURE CO-FIRED CERAMIC POWDER AND PREPARATION METHOD AND APPLICATION THEREOF
European Patent Office | 2024
|LOW-TEMPERATURE CO-FIRED CERAMIC POWDER AND PREPARATION METHOD AND APPLICATION THEREOF
European Patent Office | 2024
|European Patent Office | 2021
|LOW TEMPERATURE CO-FIRED CERAMIC MATERIAL AND PREPARATION METHOD THEREFOR
European Patent Office | 2016
|