PREPARATION METHOD FOR INTERCALATION MODIFIED C-S-H GEL NANODISPERSION
The present invention provides a low-cost preparation method for an intercalation modified calcium silicate hydrate (C-S-H) gel nanodispersion. The preparation method comprises: adding calcium hydroxide, superfine quartz sand powder, and water-soluble small molecules to a certain molar concentration of a sodium hydroxide solution; then adding the mixture to a ball mill for ball milling treatment for 90-240 min; and performing repeated pressure filtration treatment and dispersion treatment on the reaction solution to obtain an intercalation modified C-S-H gel nanodispersion. Beneficial effects of the present invention are mainly that: the mechanical force chemical effect during a ball milling process is fully utilized; sodium hydroxide is used as an intermediate component of the chemical reaction of quartz sand powder under a mechanical force chemical effect, so as to promote the chemical reaction of the low-cost quartz sand powder and calcium hydroxide under the mechanical force chemical effect, so that cheap and easily available quartz sand powder and calcium hydroxide can be used as raw materials to prepare intercalation modified C-S-H gel nanodispersion; the preparation process is low in cost; and the sodium hydroxide and pressure filtration water can be recycled.
La présente invention concerne une méthode de préparation à faible coût d'une nanodispersion de gel d'hydrate de silicate de calcium (C-S-H) modifié par intercalation. La méthode de préparation comprend : l'ajout d'hydroxyde de calcium, de poudre de sable de quartz super-fine et de petites molécules solubles dans l'eau à une certaine concentration molaire d'une solution d'hydroxyde de sodium ; puis l'ajout du mélange à un broyeur à boulets pour un traitement de broyage à boulets pendant 90 à 240 min ; et la réalisation d'un traitement de filtration sous pression répétée et d'un traitement de dispersion sur la solution de réaction pour obtenir une nanodispersion de gel de C-S-H modifié par intercalation. Les effets bénéfiques de la présente invention sont principalement : l'effet chimique de force mécanique pendant un procédé de broyage à boulets est complètement utilisé ; de l'hydroxyde de sodium est utilisé en tant que composant intermédiaire de la réaction chimique de poudre de sable de quartz sous un effet chimique de force mécanique, de manière à favoriser la réaction chimique de la poudre de sable de quartz à faible coût et de l'hydroxyde de calcium sous l'effet chimique de force mécanique, de telle sorte que de la poudre de sable de quartz et de l'hydroxyde de calcium bon marché et facilement disponibles peuvent être utilisés en tant que matières premières pour préparer une nanodispersion de gel de C-S-H modifié par intercalation ; le procédé de préparation est peu coûteux ; et l'hydroxyde de sodium et l'eau de filtration sous pression peuvent être recyclés.
本发明提供了一种插层改性C-S-H凝胶纳米分散液的低成本制备方法,所述制备方法为将氢氧化钙、超细石英砂粉和水溶性小分子加入一定摩尔浓度的氢氧化钠溶液中,然后将混合物加入球磨机进行球磨处理90-240min,反应液经反复压滤处理和分散处理后,即可制得所述插层改性C-S-H凝胶纳米分散液,本发明的有益效果主要体现在充分利用球磨过程中的机械力化学效应,采用氢氧化钠作为石英砂粉在机械力化学作用下发生化学反应的中间组分,促进低成本石英砂粉和氢氧化钙在机械力化学作用下的化学反应,从而可利用价廉易得的石英砂粉和氢氧化钙作为原材料,制备插层改性的水化硅酸钙凝胶纳米分散液,其制备过程成本低廉,氢氧化钠和压滤水可循环利用。
PREPARATION METHOD FOR INTERCALATION MODIFIED C-S-H GEL NANODISPERSION
The present invention provides a low-cost preparation method for an intercalation modified calcium silicate hydrate (C-S-H) gel nanodispersion. The preparation method comprises: adding calcium hydroxide, superfine quartz sand powder, and water-soluble small molecules to a certain molar concentration of a sodium hydroxide solution; then adding the mixture to a ball mill for ball milling treatment for 90-240 min; and performing repeated pressure filtration treatment and dispersion treatment on the reaction solution to obtain an intercalation modified C-S-H gel nanodispersion. Beneficial effects of the present invention are mainly that: the mechanical force chemical effect during a ball milling process is fully utilized; sodium hydroxide is used as an intermediate component of the chemical reaction of quartz sand powder under a mechanical force chemical effect, so as to promote the chemical reaction of the low-cost quartz sand powder and calcium hydroxide under the mechanical force chemical effect, so that cheap and easily available quartz sand powder and calcium hydroxide can be used as raw materials to prepare intercalation modified C-S-H gel nanodispersion; the preparation process is low in cost; and the sodium hydroxide and pressure filtration water can be recycled.
La présente invention concerne une méthode de préparation à faible coût d'une nanodispersion de gel d'hydrate de silicate de calcium (C-S-H) modifié par intercalation. La méthode de préparation comprend : l'ajout d'hydroxyde de calcium, de poudre de sable de quartz super-fine et de petites molécules solubles dans l'eau à une certaine concentration molaire d'une solution d'hydroxyde de sodium ; puis l'ajout du mélange à un broyeur à boulets pour un traitement de broyage à boulets pendant 90 à 240 min ; et la réalisation d'un traitement de filtration sous pression répétée et d'un traitement de dispersion sur la solution de réaction pour obtenir une nanodispersion de gel de C-S-H modifié par intercalation. Les effets bénéfiques de la présente invention sont principalement : l'effet chimique de force mécanique pendant un procédé de broyage à boulets est complètement utilisé ; de l'hydroxyde de sodium est utilisé en tant que composant intermédiaire de la réaction chimique de poudre de sable de quartz sous un effet chimique de force mécanique, de manière à favoriser la réaction chimique de la poudre de sable de quartz à faible coût et de l'hydroxyde de calcium sous l'effet chimique de force mécanique, de telle sorte que de la poudre de sable de quartz et de l'hydroxyde de calcium bon marché et facilement disponibles peuvent être utilisés en tant que matières premières pour préparer une nanodispersion de gel de C-S-H modifié par intercalation ; le procédé de préparation est peu coûteux ; et l'hydroxyde de sodium et l'eau de filtration sous pression peuvent être recyclés.
本发明提供了一种插层改性C-S-H凝胶纳米分散液的低成本制备方法,所述制备方法为将氢氧化钙、超细石英砂粉和水溶性小分子加入一定摩尔浓度的氢氧化钠溶液中,然后将混合物加入球磨机进行球磨处理90-240min,反应液经反复压滤处理和分散处理后,即可制得所述插层改性C-S-H凝胶纳米分散液,本发明的有益效果主要体现在充分利用球磨过程中的机械力化学效应,采用氢氧化钠作为石英砂粉在机械力化学作用下发生化学反应的中间组分,促进低成本石英砂粉和氢氧化钙在机械力化学作用下的化学反应,从而可利用价廉易得的石英砂粉和氢氧化钙作为原材料,制备插层改性的水化硅酸钙凝胶纳米分散液,其制备过程成本低廉,氢氧化钠和压滤水可循环利用。
PREPARATION METHOD FOR INTERCALATION MODIFIED C-S-H GEL NANODISPERSION
MÉTHODE DE PRÉPARATION D'UNE NANODISPERSION DE GEL DE C-S-H MODIFIÉ PAR INTERCALATION
一种插层改性C-S-H凝胶纳米分散液的制备方法
KONG DEYU (author) / SHENG JIANSONG (author) / YANG HUI (author)
2023-03-30
Patent
Electronic Resource
Chinese
Processing and nanodispersion: A quantitative approach for polylactide nanocomposite
British Library Online Contents | 2008
|DOAJ | 2018
|Thermosensitive PLA based nanodispersion for targeting brain tumor via intranasal route
British Library Online Contents | 2016
|Modeling of the Process of Drying and Coalescing Nanodispersion Spreading
British Library Conference Proceedings | 2021
|