BÉTON À FAIBLE DOSAGE EN CIMENT
The present invention relates to a fresh concrete composition comprising at least: i) a hydraulic binder comprising: - from 20% to 40% by weight of Portland cement clinker based on the total weight of said binder, - from 45% to 75% by weight of filler based on the total weight of said binder, and - from 5% to 15% by weight of material of ultrafine particle size based on the total weight of said binder, selected from hydraulic additives, pozzolanic additives, ultrafine cements and mixtures thereof, ii) at least one superplasticiser or plasticiser, iii) water, and iv) aggregates.
La présente invention concerne une composition de béton frais comprenant au moins : i) un liant hydraulique comprenant : - de 20% à 40% en poids de clinker Portland par rapport au poids total dudit liant, - de 45% à 75% en poids en filler par rapport au poids total dudit liant, et - de 5% à 15% en poids en matériau de granulométrie ultrafine par rapport au poids total dudit liant, étant choisi parmi les additions hydrauliques, les additions pouzzolaniques, les ciments ultrafins et leurs mélanges, ii) au moins un superplastifiant ou plastifiant, iii) de l'eau, et iv) des granulats.
BÉTON À FAIBLE DOSAGE EN CIMENT
The present invention relates to a fresh concrete composition comprising at least: i) a hydraulic binder comprising: - from 20% to 40% by weight of Portland cement clinker based on the total weight of said binder, - from 45% to 75% by weight of filler based on the total weight of said binder, and - from 5% to 15% by weight of material of ultrafine particle size based on the total weight of said binder, selected from hydraulic additives, pozzolanic additives, ultrafine cements and mixtures thereof, ii) at least one superplasticiser or plasticiser, iii) water, and iv) aggregates.
La présente invention concerne une composition de béton frais comprenant au moins : i) un liant hydraulique comprenant : - de 20% à 40% en poids de clinker Portland par rapport au poids total dudit liant, - de 45% à 75% en poids en filler par rapport au poids total dudit liant, et - de 5% à 15% en poids en matériau de granulométrie ultrafine par rapport au poids total dudit liant, étant choisi parmi les additions hydrauliques, les additions pouzzolaniques, les ciments ultrafins et leurs mélanges, ii) au moins un superplastifiant ou plastifiant, iii) de l'eau, et iv) des granulats.
BÉTON À FAIBLE DOSAGE EN CIMENT
CONCRETE HAVING A LOW CEMENT CONTENT