ENVIRONMENTALLY FRIENDLY MORTAR COMPOSITIONS
A mortar composition comprises: a) 15 – 50 wt.-% of a mineral binder, whereby: - with respect to 100 parts by weight of the mineral binder, the mineral binder comprises 40 – 70 parts by weight of cement and 30 –60 parts by weight of a cement substitute based on clay, limestone and gypsum; - and whereby, with respect to 100 parts by weight of the cement substitute, the cement substitute comprises: 35 – 65 parts by weight of clay, especially calcined clay, 1 – 20 parts by weight of gypsum, and rest to 100 parts by weight of limestone; b) 50 – 80 wt.-%, especially 62 – 65 wt.-%, of aggregates, especially sand; c) 0 – 10 wt.-%, especially 0 – 6 wt.-% of one or more additives; whereby all of the wt.-% are with respect to the dry weight of the mortar composition.
Composition de mortier comprenant : a) 15 à 50 % en poids d'un liant minéral, dans laquelle : - par rapport à 100 parties en poids du liant minéral, le liant minéral comprend de 40 à 70 parties en poids de ciment et de 30 à 60 parties en poids d'un substitut de ciment à base d'argile, de calcaire et de gypse ; - et dans lequel, par rapport à 100 parties en poids du substitut de ciment, le substitut de ciment comprend : de 35 à 65 parties en poids d'argile, en particulier d'argile calcinée, de 1 à 20 parties en poids de gypse, et du reste à 100 parties en poids de calcaire ; b) 50 à 80 % en poids, en particulier 62 à 65 % en poids, d'agrégats, en particulier de sable ; c) 0 à 10 % en poids, en particulier 0 à 6 % en poids d'un ou de plusieurs additifs ; tous les % en poids se rapportent au poids sec de la composition de mortier.
ENVIRONMENTALLY FRIENDLY MORTAR COMPOSITIONS
A mortar composition comprises: a) 15 – 50 wt.-% of a mineral binder, whereby: - with respect to 100 parts by weight of the mineral binder, the mineral binder comprises 40 – 70 parts by weight of cement and 30 –60 parts by weight of a cement substitute based on clay, limestone and gypsum; - and whereby, with respect to 100 parts by weight of the cement substitute, the cement substitute comprises: 35 – 65 parts by weight of clay, especially calcined clay, 1 – 20 parts by weight of gypsum, and rest to 100 parts by weight of limestone; b) 50 – 80 wt.-%, especially 62 – 65 wt.-%, of aggregates, especially sand; c) 0 – 10 wt.-%, especially 0 – 6 wt.-% of one or more additives; whereby all of the wt.-% are with respect to the dry weight of the mortar composition.
Composition de mortier comprenant : a) 15 à 50 % en poids d'un liant minéral, dans laquelle : - par rapport à 100 parties en poids du liant minéral, le liant minéral comprend de 40 à 70 parties en poids de ciment et de 30 à 60 parties en poids d'un substitut de ciment à base d'argile, de calcaire et de gypse ; - et dans lequel, par rapport à 100 parties en poids du substitut de ciment, le substitut de ciment comprend : de 35 à 65 parties en poids d'argile, en particulier d'argile calcinée, de 1 à 20 parties en poids de gypse, et du reste à 100 parties en poids de calcaire ; b) 50 à 80 % en poids, en particulier 62 à 65 % en poids, d'agrégats, en particulier de sable ; c) 0 à 10 % en poids, en particulier 0 à 6 % en poids d'un ou de plusieurs additifs ; tous les % en poids se rapportent au poids sec de la composition de mortier.
ENVIRONMENTALLY FRIENDLY MORTAR COMPOSITIONS
COMPOSITIONS DE MORTIER RESPECTUEUSES DE L'ENVIRONNEMENT
HESSELBARTH DANIELA (author) / GALLUCCI EMMANUEL (author) / JUILLAND PATRICK (author) / FRUNZ LUKAS (author)
2024-01-04
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Special mortar for antibiotic and environmentally-friendly aerated bricks
European Patent Office | 2016
|Environmentally friendly heat-insulation fireproof mortar and preparation method thereof
European Patent Office | 2016
|