LOW-STRESS-SENSITIVITY HIGH-FREQUENCY MANGANESE-ZINC FERRITE MATERIAL, AND PREPARATION METHOD THEREFOR
The present text discloses a low-stress-sensitivity high-frequency manganese-zinc ferrite material and a preparation method therefor. The low-stress-sensitivity high-frequency manganese-zinc ferrite material comprises: main components and additives; the main components comprise Fe2O3, ZnO and MnO; and the additives comprise Co2O3, CaCO3, Nb2O5 and TiO2. In the present application, the suitable main formula ratios reduce the magnetostriction coefficient of the material, reducing the stress sensitivity characteristics of the material; the suitable additive combination and addition amounts reduce material loss and improve material temperature properties; and a combination of low-temperature sintering and a special cooling curve reduce the grain size of the material, reduce the stress sensitivity and high-frequency loss of the material, and result in a high-frequency manganese-zinc ferrite material having low stress sensitivity and low loss.
Le présent texte divulgue un matériau de ferrite de manganèse-zinc haute fréquence à faible sensibilité à la contrainte et un procédé de préparation associé. Le matériau de ferrite de manganèse-zinc haute fréquence à faible sensibilité à la contrainte comprend : des composants principaux et des additifs, les composants principaux comprenant Fe2O3, ZnO et MnO, les additifs comprenant Co2O3, CaCO3, Nb2O5 et TiO2. Dans la présente demande, les rapports de formule principaux appropriés réduisent le coefficient de magnétostriction du matériau, réduisant les caractéristiques de sensibilité à la contrainte du matériau ; la combinaison d'additifs appropriée et les quantités d'ajout réduisent la perte de matériau et améliorent les propriétés de température de matériau ; et une combinaison de frittage à basse température et d'une courbe de refroidissement spéciale réduit la taille de grain du matériau, réduit la sensibilité à la contrainte et la perte haute fréquence du matériau, et permet d'obtenir un matériau de ferrite de manganèse-zinc haute fréquence présentant une faible sensibilité à la contrainte et une faible perte.
本文公布了一种低应力敏感的高频锰锌铁氧体材料及其制备方法,所述低应力敏感的高频锰锌铁氧体材料包括主成分和添加剂;所述主成分包括Fe2O3、ZnO和MnO;所述添加剂包括Co2O3、CaCO3、Nb2O5以及TiO2。本申请通过合适的主配方比例降低材料本身的磁致伸缩系数,减小材料本身的应力敏感性能;通过合适的添加剂组合、添加量降低材料损耗和改善材料温度特性;并通过低温烧结工艺和特殊的降温曲线配合减小材料晶粒尺寸,减小材料应力敏感性和高频损耗,制备出低应力敏感、低损耗的高频锰锌铁氧体材料。
LOW-STRESS-SENSITIVITY HIGH-FREQUENCY MANGANESE-ZINC FERRITE MATERIAL, AND PREPARATION METHOD THEREFOR
The present text discloses a low-stress-sensitivity high-frequency manganese-zinc ferrite material and a preparation method therefor. The low-stress-sensitivity high-frequency manganese-zinc ferrite material comprises: main components and additives; the main components comprise Fe2O3, ZnO and MnO; and the additives comprise Co2O3, CaCO3, Nb2O5 and TiO2. In the present application, the suitable main formula ratios reduce the magnetostriction coefficient of the material, reducing the stress sensitivity characteristics of the material; the suitable additive combination and addition amounts reduce material loss and improve material temperature properties; and a combination of low-temperature sintering and a special cooling curve reduce the grain size of the material, reduce the stress sensitivity and high-frequency loss of the material, and result in a high-frequency manganese-zinc ferrite material having low stress sensitivity and low loss.
Le présent texte divulgue un matériau de ferrite de manganèse-zinc haute fréquence à faible sensibilité à la contrainte et un procédé de préparation associé. Le matériau de ferrite de manganèse-zinc haute fréquence à faible sensibilité à la contrainte comprend : des composants principaux et des additifs, les composants principaux comprenant Fe2O3, ZnO et MnO, les additifs comprenant Co2O3, CaCO3, Nb2O5 et TiO2. Dans la présente demande, les rapports de formule principaux appropriés réduisent le coefficient de magnétostriction du matériau, réduisant les caractéristiques de sensibilité à la contrainte du matériau ; la combinaison d'additifs appropriée et les quantités d'ajout réduisent la perte de matériau et améliorent les propriétés de température de matériau ; et une combinaison de frittage à basse température et d'une courbe de refroidissement spéciale réduit la taille de grain du matériau, réduit la sensibilité à la contrainte et la perte haute fréquence du matériau, et permet d'obtenir un matériau de ferrite de manganèse-zinc haute fréquence présentant une faible sensibilité à la contrainte et une faible perte.
本文公布了一种低应力敏感的高频锰锌铁氧体材料及其制备方法,所述低应力敏感的高频锰锌铁氧体材料包括主成分和添加剂;所述主成分包括Fe2O3、ZnO和MnO;所述添加剂包括Co2O3、CaCO3、Nb2O5以及TiO2。本申请通过合适的主配方比例降低材料本身的磁致伸缩系数,减小材料本身的应力敏感性能;通过合适的添加剂组合、添加量降低材料损耗和改善材料温度特性;并通过低温烧结工艺和特殊的降温曲线配合减小材料晶粒尺寸,减小材料应力敏感性和高频损耗,制备出低应力敏感、低损耗的高频锰锌铁氧体材料。
LOW-STRESS-SENSITIVITY HIGH-FREQUENCY MANGANESE-ZINC FERRITE MATERIAL, AND PREPARATION METHOD THEREFOR
MATÉRIAU DE FERRITE DE MANGANÈSE-ZINC HAUTE FRÉQUENCE À FAIBLE SENSIBILITÉ À LA CONTRAINTE, ET PROCÉDÉ DE PRÉPARATION ASSOCIÉ
一种低应力敏感的高频锰锌铁氧体材料及其制备方法
HU XINYUE (author) / XU XIAOJIA (author) / ZHU YONG (author)
2024-02-15
Patent
Electronic Resource
Chinese
MANGANESE-ZINC FERRITE MATERIAL AND PREPARATION METHOD THEREFOR
European Patent Office | 2024
|HIGH-FREQUENCY AND HIGH-IMPEDANCE MANGANESE-ZINC FERRITE MATERIAL AND PREPARATION METHOD THEREFOR
European Patent Office | 2022
|High-frequency manganese zinc ferrite material and preparation method thereof
European Patent Office | 2024
|High-frequency manganese-zinc ferrite material and preparation method thereof
European Patent Office | 2020
|Preparation method and equipment of high-frequency manganese zinc ferrite material
European Patent Office | 2022
|