POWER FERRITE MATERIAL, PREPARATION METHOD THEREFOR, AND USE THEREOF
Disclosed are a power ferrite material, a preparation method therefor, and a use thereof. The power ferrite material is composed of main components and auxiliary components; the main components comprise, in percentage by mole, 52.7-53 mol% of Fe2O3, 10-12 mol% of ZnO, and 35-37.3 mol% of MnO. On the basis of the total mass percentage of the main components, the auxiliary components comprise 0.08-0.1 wt% of CaCO3, 0.02-0.04 wt% of Nb2O5, and 0.4-0.42 wt% of Co2O3. According to the present application, by matching reasonable content proportioning of the main components and the auxiliary components, the prepared power ferrite material has the characteristics of keeping low loss in a wide temperature range, and can meet the requirement of serving as a power ferrite of an automobile electronic product.
La présente invention concerne un matériau ferrite de puissance, son procédé de préparation et son utilisation. Le matériau de ferrite de puissance est composé d'éléments principaux et d'éléments subsidiaires ; les éléments principaux comprennent, en pourcentage molaire, 52,7 à 53 % de Fe2O3, 10 à 12 % de ZnO et 35 à 37,3 % de MnO. Sur la base du pourcentage de masse total des composants principaux, les composants auxiliaires comprenent 0,08 à 0,1 % en poids de CaCO3, 0,02 à 0,04 % en poids de Nb2O5 et 0,4 à 0,42 % en poids de Co2O3. Selon la présente invention, grâce à un dosage raisonnable des composants principaux et des composants subsidiaires, la ferrite de puissance préparée présente les caractéristiques suivantes : faible perte dans une large plage de température et peut répondre aux exigences d'un produit électronique automobile en tant que ferrite de puissance.
本文公布一种功率铁氧体材料及其制备方法与应用,所述功率铁氧体材料由主成分与辅助成分组成;以摩尔百分数计,所述主成分包括:Fe2O3 52.7-53mol%;ZnO 10-12mol%;MnO 35-37.3mol%;以所述主成分的总质量百分数计,所述辅助成分包括:CaCO3 0.08-0.1wt%;Nb2O5 0.02-0.04wt%;Co2O3 0.4-0.42wt%。本申请通过搭配合理的主成分以及辅助成分的含量配比,制得的功率铁氧体材料具有宽温低损耗的特性,能够满足作为汽车电子产品功率铁氧体的要求。
POWER FERRITE MATERIAL, PREPARATION METHOD THEREFOR, AND USE THEREOF
Disclosed are a power ferrite material, a preparation method therefor, and a use thereof. The power ferrite material is composed of main components and auxiliary components; the main components comprise, in percentage by mole, 52.7-53 mol% of Fe2O3, 10-12 mol% of ZnO, and 35-37.3 mol% of MnO. On the basis of the total mass percentage of the main components, the auxiliary components comprise 0.08-0.1 wt% of CaCO3, 0.02-0.04 wt% of Nb2O5, and 0.4-0.42 wt% of Co2O3. According to the present application, by matching reasonable content proportioning of the main components and the auxiliary components, the prepared power ferrite material has the characteristics of keeping low loss in a wide temperature range, and can meet the requirement of serving as a power ferrite of an automobile electronic product.
La présente invention concerne un matériau ferrite de puissance, son procédé de préparation et son utilisation. Le matériau de ferrite de puissance est composé d'éléments principaux et d'éléments subsidiaires ; les éléments principaux comprennent, en pourcentage molaire, 52,7 à 53 % de Fe2O3, 10 à 12 % de ZnO et 35 à 37,3 % de MnO. Sur la base du pourcentage de masse total des composants principaux, les composants auxiliaires comprenent 0,08 à 0,1 % en poids de CaCO3, 0,02 à 0,04 % en poids de Nb2O5 et 0,4 à 0,42 % en poids de Co2O3. Selon la présente invention, grâce à un dosage raisonnable des composants principaux et des composants subsidiaires, la ferrite de puissance préparée présente les caractéristiques suivantes : faible perte dans une large plage de température et peut répondre aux exigences d'un produit électronique automobile en tant que ferrite de puissance.
本文公布一种功率铁氧体材料及其制备方法与应用,所述功率铁氧体材料由主成分与辅助成分组成;以摩尔百分数计,所述主成分包括:Fe2O3 52.7-53mol%;ZnO 10-12mol%;MnO 35-37.3mol%;以所述主成分的总质量百分数计,所述辅助成分包括:CaCO3 0.08-0.1wt%;Nb2O5 0.02-0.04wt%;Co2O3 0.4-0.42wt%。本申请通过搭配合理的主成分以及辅助成分的含量配比,制得的功率铁氧体材料具有宽温低损耗的特性,能够满足作为汽车电子产品功率铁氧体的要求。
POWER FERRITE MATERIAL, PREPARATION METHOD THEREFOR, AND USE THEREOF
POWER FERRITE MATERIAL, PREPARATION METHOD THEREFOR, AND USE THEREOF
一种功率铁氧体材料及其制备方法与应用
ZHANG LIKANG (author) / LV DONGHUA (author)
2024-05-23
Patent
Electronic Resource
Chinese
FERRITE MATERIAL, PREPARATION METHOD THEREFOR AND USE THEREOF
European Patent Office | 2022
|FERRITE MATERIAL, PREPARATION METHOD THEREFOR AND USE THEREOF
European Patent Office | 2024
|MICROWAVE FERRITE MATERIAL, PREPARATION METHOD THEREFOR AND APPLICATION THEREOF
European Patent Office | 2025
|NICUZN FERRITE MATERIAL, AND PREPARATION METHOD THEREFOR AND USE THEREOF
European Patent Office | 2023
|NICUZN FERRITE MATERIAL, AND PREPARATION METHOD THEREFOR AND USE THEREOF
European Patent Office | 2024
|